Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!
FT Archives

Rolls-Royce Acquires Innovative Coating for Jet Engines - Posted 6/12/07

June 12, 2007

Rolls-Royce Corp. has acquired exclusive rights to use a coating invented by Iowa State University researchers that helps turbines stand up to the heat in jet engines. The innovative bond coating will be applied to engine turbine blades made of nickel-based superalloys. Those superalloys are designed for strength but need help withstanding metal temperatures approaching 2,100°F inside the hot section of a jet engine, said Brian Gleeson, Iowa State's Alan and Julie Renken professor in materials science and engineering, a scientist with the U.S. Department of Energy's Ames Laboratory on the Iowa State campus and a co-inventor of the coating.

The bond coating improves the durability and reliability of a ceramic thermal barrier that's applied over the bond coat, said Daniel Sordelet, a senior scientist and group leader for the Ames Laboratory and a co-inventor of the technology.

"This coating composition is very good in terms of performance," Gleeson said. "It offers significant advantages over existing coating technologies."

Dr. William J. Brindley, the chief technologist for Rolls-Royce Corp., said, "This new coating offers excellent oxidation resistance. It's a new concept in coatings and a real step forward in understanding how and why coatings work. The technology also represents a remarkably quick transition from fundamental science to practical application."

Gleeson said the coating is based on a composition comprising platinum, nickel, aluminum and hafnium. It was invented by Gleeson, Sordelet and Wen Wang, a former Iowa State postdoctoral student. Gleeson, Sordelet, Brindley and Bingtao Li, a former Iowa State doctoral student and postdoctoral researcher, also developed a cost-effective method for applying the coating to engine parts.

The coating won a prestigious R&D 100 Award in 2005. The annual awards have been called the "Oscars of applied science" by the Chicago Tribune.

Nita Lovejoy, the associate director of the Iowa State University Research Foundation, Inc., said Rolls-Royce will have an exclusive license to commercialize the inventions. She said patents are pending for the inventions and the term of the license agreement is for the life of any patents. She also said the license has the potential to be an important source of revenue for the research foundation.

Sordelet said the coating compositions grew out of basic research that began about seven years ago and was supported by the Office of Naval Research. He said a key advantage to this technology is that it is mechanically compatible with the superalloys it covers and protects. It reacts to the heat and stress of an engine about the same way the superalloy does. And that gives the coating composition -- and therefore the engine parts -- better performance and a longer life.

The Iowa State researchers continue to work on the coating composition project. Sordelet said they're hoping to develop a better and cheaper way to produce the coating. They're also looking for new coating compositions and new ways to deposit them on materials.

For more information, contact Brian Gleeson, Materials Science and Engineering, at 515.294.5606 or bgleeson@iastate.edu.

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • pci1022-Kinaltek-Lead-1170.jpg

    A Novel Pigment Production Technology

    Following an extensive R&D program that demonstrated...
    Paint and Coating Pigments
    By: Jawad Haidar and Nitin Soni
  • pci global top 10

    2025 Global Top 10: Top Paint and Coatings Companies

    The following is PCI’s annual ranking of the top 10...
    Paint and Coating Market Reports
    By: Courtney Bassett
  • 2025 pci 25

    2025 PCI 25: Top Paint and Coatings Companies

    PCI's annual ranking of the top 25 North American paint...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

Popular Stories

Akzo, SW, Nippon Logos

AkzoNobel Rejects Cash Offer From Nippon Paint, Sherwin-Williams

BASF SE Logo

BASF Announces Strategic Business Sale

AkzoSWNipponEndTalks

Nippon Paint, Sherwin-Williams End AkzoNobel Pursuit

POB-Point-and-Shoot

PCI Buyers Guide

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

Find Suppliers

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

September 15, 2026

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Automotive Paints and Coatings, 2nd Edition

Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

See More Products
Inside the AI Shift in Coatings - See the article now

Related Articles

  • "Renewable" Ceramic Coating Holds Promise for Jet Engines - Posted 3/19/08

    See More
  • SOFTWARE: Coil Coating CD - Posted 6/12/07

    See More
  • Wolfe Hired as Senior Research Chemist for Prime Coatings - Posted 6/12/07

    See More

Related Products

See More Products
  • Hansen Solubility Parameters – A Scientific Approach for Coating Formulators (Virtual Course - 8/20/26)

See More Products
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing