Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!
FT Archives

Roobol On Painting

January 20, 2004

Early Rusting on Powder Coated Fencing

We manufactured a fence system and had the panel powder coated. The panels are made of welder wire mesh, held in place with an angle iron with a leg out onto a flat plate that is on the other side of the mesh. The mesh was welded to the angle iron and then the plate and angle iron were welded together. We installed about 900 linear feet of this fence and all the panels have rusted.

What can be done to stop the rusting? What design changes can be made to the fence panels to stop the rusting? Should the powder coating have fully encapsulated the edge detail?

Yes, there is indeed a reason for this rust. A likely cause for corrosion at the locations you mentioned is called the Faraday Cage effect. Powder coatings are applied electrostatically, and the charged powder particles deposit on the nearest grounded surface. They do not penetrate much into recesses where the plate and wire mesh are welded together. The same lack of coverage tends to occur at points where wires cross in the mesh. Since the powder coating is thin or missing in those spots, early rusting will be seen, as you have discovered.

You can change the construction details or materials as one major redesign, or you can change the coating method to dipping, chemiphoretic coating or electrodeposition coating. Spraying non-electrostatically with liquid paint would lessen the problem, but again it will be tough to get paint into all the myriad recesses.

Cleaning Zinc Phosphate Buildup

How can I clean a stainless-steel pipe that has zinc phosphate buildup inside and outside?

It can be mechanically sanded or grit blasted off. Immersion in chromic acid will also remove phosphate coatings.

Waterborne Latex Not for Traffic

Recently my supervisor asked me to take over the yellow striping of the heavily traveled parking lot where I am the maintenance person for all types of work. I'm not familiar with the various types of paint products used to stripe the asphalt area. Also, I was not well informed by the person I purchased paint from for this purpose. Consequently, I used water-based latex paint and the stripes are wearing off after two days of use. The area is heavily used by large trucks and cranes, and the yellow lines are crucial to their safe operation. Please advise.

Why you were not advised to use paints made specifically for stripe marking is strange, unless the person was avaricious or not sufficiently kind to admit they didn't know enough to properly advise you.

Most traffic marking paint is acrylic latex or acrylic-vinyl acetate latex. These dry rapidly, a major advantage for obvious reasons. Your local commercial painting supply store will certainly handle them. Ask for "traffic marking paint" and they will likely have six or more different paints available. As an example, Sherwin-Williams alone makes at least eight different formulations of traffic marking coatings. You can also do a Web search using "traffic marking paint" for additional options.

Poor Cleaning Probable Culprit in Cratering

I am having a problem painting ABS components for a two-wheeler company. There are a lot of craters where even primers are getting stuck. We have tried many things, but all in vain. Can you help?

ABS (acrylonitrile-butadiene-styrene terpolymer) is one of the easiest plastics to paint and is seldom the root cause of the defect you are experiencing. It is abundantly clear that you have a contamination problem here, possibly from poorly cleaned parts that have residual hydrocarbon or silicone oil on them when being painted. Another source of these crater-causing materials may be your paint or the compressed air supply. From halfway around the globe I cannot be sure the ABS has not been inadvertently fouled by oil or silicone, but I suspect other sources are at fault.

Carefully clean several parts very thoroughly with acetone or similar solvent, and then paint them as you normally would. If no craters appear, then poor cleaning is the most probable cause of the defects. But if craters still are evident, the contamination may be either in the compressed air or in the bulk paint itself. Only if you are certain that parts are clean and that the compressed air and the coatings are not contaminated should you investigate the possibility of the ABS having been contaminated.

More on Friction-Reducing Coatings

I was forwarded a question about friction-reducing coatings asked by a naval architect in your column. Apparently these coatings are not familiar to these end users or to you. My company holds patents for such hydrophilic coatings, which are routinely used in the medical markets for ease of insertion and leaching of antimicrobials and drugs. In fact, we also supply the recreational boating market with a temporary "go fast" coating that is hydrophilic. We wondered if you would like some commentary on these coatings? Of particular interest were the thoughts put forward by the NPCA group that met in Virginia Beach with a large contingent of Navy and Coast Guard personnel about marine and offshore coatings. Please advise if we can help in this matter.

Thank you very much for your response with information on this topic. Many readers would certainly be interested in learning more about such coatings and hearing comments concerning their usage. I'm eager to find out the specifics of their performance.

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • pci1022-Kinaltek-Lead-1170.jpg

    A Novel Pigment Production Technology

    Following an extensive R&D program that demonstrated...
    Paint and Coating Pigments
    By: Jawad Haidar and Nitin Soni
  • pci global top 10

    2025 Global Top 10: Top Paint and Coatings Companies

    The following is PCI’s annual ranking of the top 10...
    Paint and Coating Market Reports
    By: Courtney Bassett
  • 2025 pci 25

    2025 PCI 25: Top Paint and Coatings Companies

    PCI's annual ranking of the top 25 North American paint...
    Paint and Coating Market Reports
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

Popular Stories

Akzo, SW, Nippon Logos

AkzoNobel Rejects Cash Offer From Nippon Paint, Sherwin-Williams

BASF SE Logo

BASF Announces Strategic Business Sale

AkzoSWNipponEndTalks

Nippon Paint, Sherwin-Williams End AkzoNobel Pursuit

POB-Point-and-Shoot

PCI Buyers Guide

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

Find Suppliers

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

September 15, 2026

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Automotive Paints and Coatings, 2nd Edition

Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

See More Products
Inside the AI Shift in Coatings - See the article now

Related Articles

  • Roobol on Painting

    See More
  • Roobol On Painting

    See More
  • Roobol on Painting

    See More

Related Products

See More Products
  • pci november

    PCI November 2019 Issue

  • pci may 2020

    PCI May 2020 Issue

See More Products

Related Directories

  • Titan

    As a leader in spraying technology, Titan manufactures and markets a full line of professional-grade paint sprayers for applying a variety of coatings.
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing