Spin-Off to Market Green Technology Using Waste Paint

A new venture, formed by a special licensing agreement signed with Rutgers University, has been launched to commercialize and market a green technology being developed by Rutgers’ Center for Advanced Materials via Immiscible Polymer Processing (AMIPP).

EAST BRUNSWICK, N.J. - A new venture, formed by a special licensing agreement signed with Rutgers University, has been launched to commercialize and market a green technology being developed by Rutgers’ Center for Advanced Materials via Immiscible Polymer Processing (AMIPP). The technology uses waste latex paint and recycled plastics as raw materials to:
  • create new blended polymers used in manufacturing,
  • increase the volume of available plastics to meet demand and
  • reduce the burden of leftover paint dumped in landfills.
The new green company, Re-Manufacturing Technologies, Inc. (RMT), is a spin-off of the National Council on Paint Disposition, Inc. (NCPD), a New Jersey-based national environmental organization, founded in 2002, with the mission to develop and implement a comprehensive approach to reducing the cost and environmental impact of waste paint products.

Re-Manufacturing Technologies will market Rutgers’ new technology as an environmentally preferred solution for dealing with this country’s costly waste latex paint problem, as well as the increasing demand for plastics, according to NCPD President Marv Goodman, who also serves as president of RMT.

For more information about RMT or NCPD, call 732/309.2022 or visit www.paintrecycling.org.

You must register or login in order to post comments.

Multimedia

Videos

Image Galleries

Podcasts

PCI Top 5 - January 12, 2012
PCI's Podcast series on the five most e-mailed/shared articles and stories for the week.

More Podcasts

THE MAGAZINE

PCI Magazine

February 2012 cover

2012 February

PCI's new issue is now available. Check it out!

TABLE OF CONTENTS SUBSCRIBE

Coating Technology

What resources do you refer to when learning about coatings technology?
See Poll Results Poll Archive

THE PCI STORE

Power Coatings
CD Verison: Powder Coatings - Foundation for the Novice Formulator by Kevin Biller for $29.95 plus shipping
ON CD - Powder Coatings have been the fastest growing finishing technology for the past 30 years. In spite of this tremendous growth and the technology advances that come with it, very few technical tools have been provided for the formulator.
More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

Virtual Brochures

PageCollageClick to the Virtual Brochures page to view multiple catagories that list downloadable product literature from leading industry suppliers.

STAY CONNECTED

Facebook Twitter  LinkedIn