Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!

New High-Performance Alkyl Phenol-Free Surfactants

By Ana Maria Fernandez, Loubna Jebbanema
October 1, 2009


This paper introduces a new generation of alkyl phenol-free nonionic surfactants. The new surfactants are environmentally compatible, exhibiting effective performance during polymerization and post-polymerization stabilization. These liquid surfactants meet demanding physicochemical properties, regulatory compliance and performance requirements. They exhibit low freezing temperatures, excellent water miscibility, minimum gel phase formation and low viscosity at high solids content. The new surfactants are clear, high-solid liquids at room temperature and are easy to handle and very effective during polymerization, providing overall latex stability. This paper focuses on their chemical and physical properties as well as on their performance in model acrylic formulations for architectural coatings.

Introduction

Earlier generations of nonionic surfactants (Disponil® As and Disponil AFXs) as well as the new surfactants introduced in this paper, were developed in response to increasing global environmental protection regulations and recommendations to phase out the use of Alkyl Phenol Ethoxylates (APEs). The two new high-HLB nonionic surfactants introduced in this paper, Disponil AFX 4061 and Disponil AFX 4070, have been designed to meet environmental requirements while providing effective performance in emulsion polymerization. Also, they are very effective as post-polymerization latex stabilizers or surfactant additives for coating and adhesive formulations. Similar to previous generations, the introduction of these new emulsifiers responds to the emulsion polymerization and coatings industry demands for ecologically acceptable and effective non-ionic emulsifiers.

Surfactant Composition and Properties

Table 1 shows the composition and properties of the two new nonionic surfactants: Disponil AFX 4061 and Disponil AFX 4070. Selected Disponil As and AFXs have also been included for comparison purposes. The hydrophobes in all the surfactants listed are aliphatic. This portion of the molecules is based on C12-14 natural fatty or synthetic alcohols and primary and secondary isomeric alcohols.

Some of the most important features of the Disponil AFX 4061 and Disponil AFX 4070 can be listed as follows:
  • alkyl phenol free (AP-free);

  • biodegradable;

  • easier handling at low temperatures;

  • high solid content of 60% and 70%;

  • minimum gel phase formation;

  • low freezing point range of -5 ºC to -9 ºC at 60% and 70%;

  • clear, high-solid liquids at sub zero and room temperatures;

  • excellent water miscibility; and

  • low viscosity.


Performance in Emulsion Polymerization

The mechanism of emulsion polymerization, as well as the role of surfactants has been discussed in a number of publications.1-4 Extensive surfactant screening in model formulations has shown that the new emulsifiers are very effective in acrylic formulations. Table 2 shows the physical properties of thermal acrylic latexes made combining one nonionic emulsifier at a time with Disponil FES 32 an anionic alkyl ether sodium sulfate, used for particle size control. The results demonstrate the role of an effective surfactant combination in particle size control, coagulum content and overall stabilization. All latexes exhibited desirable small particle sizes, low coagulum, mechanical stability and freeze thaw stability.

The electrostatic stability was obtained by post adding a 0.25% of either Disponil AFX 4061 or Disponil AFX 4070. The model thermal acrylic latex formulation is shown in Table 3.

Although there is an increasing tendency to replace alkyl phenol-based (AP) with alkyl phenol-free  (AP-free) surfactants, octyl phenol-40  (OP-40) still is extensively used in many different coating applications in North America. Results listed in Table 2 show remarkable performance similarities between OP-40 and both Disponil AFX 4061 and Disponil AFX 4070. These results clearly show that both surfactants are suitable replacements for OP-40.

Latex Stability: Post Polymerization Stabilization

Emulsion polymer and coating producers are increasing their efforts to replace OP-40 and similar AP-based surfactants in a wide spectrum of latexes and coatings. Some of the most important drivers of these efforts are a new North American wave of environmental awareness and efforts to increase sustainability, Canadian regulatory pressures, older European regulations, and recommendations and trends to globalize formulations.

Surfactant post addition is often necessary to stabilize latex formulations with high inorganic filler content such as for architectural and traffic coatings, as well as paper and adhesive coatings. A fundamental property of the surfactant molecules is their ability to orient and adsorb at the interfaces. In latex systems, most of the surfactant is adsorbed at the interface between the particles and the water. This adsorption is a thermodynamic process favored by a decrease in the overall free energy of the system. The adsorbed layer of surfactant molecules is essential for the stabilization of latexes during polymerization and during post polymerization processes. It is well known that the colloidal stabilization depends on the interactions of attractive and repulsive forces between the particles. It is also accepted that electrostatic repulsion stabilization and steric or spatial stabilization are the two most important barriers to flocculation. The addition of inorganic fillers containing divalent metallic ions such as calcium, magnesium and zinc, produces rapid flocculation by disrupting the electrical double layer surrounding the polymer particles.   This reduces the electrostatic repulsions between the adsorbed anionic surfactant molecules typically used during the emulsion polymerization process.

A pragmatic remedy to restore stability is the addition of high-HLB surfactants, specifically polyethoxylated nonionic emulsifiers. The hydrophilic polyethoxylated chain provides steric stabilization by orienting and extending towards the water phase. This prevents the particles from entry into the effective space of mutual attraction. Also, it has been proposed that the effectiveness of this type of stabilization is due to the hydrogen bond interactions and high-localized viscosity of the hydrated polyethoxylated chain, which acts as a protective shield preventing flocculation.5-10

High-HLB nonionic surfactants are characterized by a low amount of surfactant molecules adsorbed at the interfaces and high cross-sectional areas at the interfaces. These properties make them ideal as post polymerization stabilizers. Disponil AFX 4061, Disponil AFX 4070 and OP-40 were evaluated as post polymerization stabilizers. In this discussion, the latex stability to divalent cations and hence the electrostatic stability of the system, is measured by the stability of the latex to calcium chloride titration.

The results of the post polymerization stabilization study are shown in Table 4. The evaluation of the latex stability consisted in measuring the coagulum formed in model acrylic latexes after the addition of 0.25%, 0.50% and 1% nonionic surfactant added to acrylic latexes without electrostatic stability. The post addition of nonionic surfactants was followed by the addition of 5% calcium chloride solution. The model acrylic latexes were made with one primary anionic emulsifier, either SLS or alkyl ether sodium sulfate surfactant. Table 4 shows post stabilization results. No coagulum was formed after the addition of only 0.25 % of non-ionic surfactant to the latexes. The excellent performance of Disponil  AFX 4061 and Disponil AFX 4070 compared to OP-40 is a clear indication that they can replace OP-40 in commercial applications.

In previous studies it has been observed that the efficiency and effectiveness of surfactants as post polymerization stabilizers is system dependent. It has been observed that certain latexes made with large quantities of anionic surfactants as the primary emulsifier, may require more than 1% nonionic surfactant addition to restore the electrostatic stability.

Summary

The experimental results presented in this paper illustrate the efficiency and effectiveness of the new Disponil AFX 4061 and Disponil AFX 4070. They can be used in a variety of applications, either to effectively improve adsorption at diverse surfaces and interfaces or to efficiently stabilize emulsion polymers. This new generation of nonionic surfactants is AP-free, biodegradable, low viscosity at high solid content, clear, and easy to handle at low temperatures. These characteristics make them environmentally acceptable and provide an opportunity for developing new AP-free formulations. The new Disponil emulsifiers have been shown to be effective during polymerization and as post-polymerization stabilizers replacing high EO-bearing APEs and synthetic sec-alcohol ethoxylates.

This paper was presented at The Waterborne Symposium sponsored by The University of Southern Mississippi School of Polymers and High Performance Materials and The Southern Society for Coatings Technology, 2009, New Orleans, LA.

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Cognis Corporation, Ambler, PA
Cognis Corporation, Ambler, PA

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • pci1022-Kinaltek-Lead-1170.jpg

    A Novel Pigment Production Technology

    Following an extensive R&D program that demonstrated...
    Paint and Coating Pigments
    By: Jawad Haidar and Nitin Soni
  • pci global top 10

    2025 Global Top 10: Top Paint and Coatings Companies

    The following is PCI’s annual ranking of the top 10...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • 2025 pci 25

    2025 PCI 25: Top Paint and Coatings Companies

    PCI's annual ranking of the top 25 North American paint...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

Popular Stories

Akzo, SW, Nippon Logos

AkzoNobel Rejects Cash Offer From Nippon Paint, Sherwin-Williams

BASF SE Logo

BASF Announces Strategic Business Sale

AkzoSWNipponEndTalks

Nippon Paint, Sherwin-Williams End AkzoNobel Pursuit

POB-Point-and-Shoot

PCI Buyers Guide

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

Find Suppliers

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

September 15, 2026

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Automotive Paints and Coatings, 2nd Edition

Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

See More Products
Inside the AI Shift in Coatings - See the article now

Related Articles

  • New Generation of Alkyl Phenol-Free Nonionic Surfactants for Emulsion Polymerization

    See More
  • image of scooters each a different color

    New High-Performance Dispersion Range From Penn Color

    See More
  • Open paint cans with colorful paint and brush

    A New High-Performance Alternative to Cobalt Driers

    See More

Related Directories

  • Innospec Performance Chemicals

    Innospec is a global supplier of specialty chemicals for many different markets, including construction, emulsion polymerization, paint and coatings, polymers and waxes. Our innovative and responsible solutions cover a strong portfolio of additives and technically advanced solutions: rheology modifiers, anionic emulsifiers, wetting agents and dispersants.
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing