Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!

From Rocks to Nanos

By John Allen
March 1, 2008

Over many years the continuous development of wet grinding mills has resulted in finer and finer particle size reduction with lower process times. It is well established that small-diameter grinding media (beads) produce finer product particle sizes. Bead sizes down to 0.05 mm are now available. The inherent high-density ceramic material used results in smaller media with higher kinetic energy potential.

However, these can only be used under certain conditions. The bead mill mechanical specification has to be engineered correctly, with particular reference to the separator type (gap/screen) and other rotating/stationary element tolerances (seals, bead eliminators, grinding zone limits, etc.).

Product viscosity is also an important factor as small beads typically have less mass, which in turn can result in a fall in bead velocity under certain rheological conditions.

Most horizontal/vertical mill mechanical aspects within the grinding chamber are not suitable for maintaining constant bead velocity; the grinding zones are typically too far apart. Most horizontal mills are unable to accommodate very small beads for prolonged usage, as eventual mechanical break down (bead entry into separators, seal housing, etc.) and separator blockage will occur. In addition, most bead mills generate the necessary grinding action in a fairly random manner, and cylinders must be packed with a large volume of beads. Generally, horizontal mills give unstable grinding media control as there is a tendency for the media to move continually toward the separator/outlet. In the case of a vertical mill, there is an uneven bead packing density, heavier at the bottom and lighter at the top. In order to maximize the efficiency of these mills, a media charge of up to 70–90% is required. Of course, efficient separation of the product and grinding media is essential, and large volumes of media will result in high process temperatures and pressures, separator damage, and mill wear (cylinders and agitators).

The agitation, by either discs or pegs, imparts shear and attrition forces to the bead mass, which in turn transfers some of this energy into the grinding action. However, most of this energy is lost in frictional heat build-up and it is necessary to incorporate an efficient cooling system. Controlling and managing this otherwise random bead action becomes paramount in order to use the energy being consumed more efficiently.

Whilst most mills will produce, in time, a dispersion where the majority of particles fall into the sub-micron territory, there is usually a ‘big end’ of micron-sized material still in evidence. Further size reduction of these particles is difficult to achieve under the above conditions.

The Microtron™

Now consider the Microtron, which has been developed with the specific task of “sub-micron grinding” in order to produce better-quality products within the coating industry. It is a misconception that grinding finer is simply a function of time when we consider how to quickly obtain 100% nanometer particle size reduction.

First consider the effect of replacing a 1-millimeter diameter bead as a contact object with one thousand 0.1-millimeter diameter beads occupying the same volume.

The contact ratio increases many times and, therefore, the grinding ability of a given mass of beads improves dramatically.

In order to achieve consistent nanometer particle sizes it was essential to specify the milling mechanics accordingly.

· Particular attention to the effective bead mass control.

· The ability to effectively separate product from media.

· Utilizing the smallest available grinding media (down to 0.05mm).

· Media charge volumes of no more than 45%, which result in 100% nanometer particle sizes reduction at low temperatures.

To achieve consistent sub-micron particle sizes it is essential to ensure that the physical properties of the premixed slurry fall into a specific range. Particular attention should always be given to product viscosity and initial particle size. Initial pre-mixes of 50 microns can be reduced to 300 nanometres and below consistently in minimum pass operations. Effective and reliable separation of the product and grinding media is achieved away from the outlet of the mill.

Utilizing both the smallest grinding media size available, along with specific grinding media management control and effective separation within the milling operation, 100% sub-micron sized particles will result. The large particle size end is removed altogether.

The bead velocity is maximized by the design of the main agitator. High-velocity beads moving only short distances are continually recaptured, forming a double spiralling opposing helix in and around the periphery of the main agitator, precisely directing the movement of the bead charge. Separation is also achieved at this stage. Centrifugal force separation is maximized by specific design where the grinding media and product separate accordingly.

The media is held in a controlled and continually interactive double spiralling mass where the centrifugal milling intensity is at its greatest. The product is subject to a consistent and intensely packed bead mass. These conditions do not alter during the milling operation. The product can only escape from the mill via this intense grinding zone.

For more information, e-mail info@cdcmicrotron.com or call (44) 1925 575678.

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

John Allen is Manager Director at CDC Microtron Ltd., Warrington, Cheshire, U.K.

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • pci1022-Kinaltek-Lead-1170.jpg

    A Novel Pigment Production Technology

    Following an extensive R&D program that demonstrated...
    Paint and Coating Pigments
    By: Jawad Haidar and Nitin Soni
  • pci global top 10

    2025 Global Top 10: Top Paint and Coatings Companies

    The following is PCI’s annual ranking of the top 10...
    Paint and Coating Market Reports
    By: Courtney Bassett
  • 2025 pci 25

    2025 PCI 25: Top Paint and Coatings Companies

    PCI's annual ranking of the top 25 North American paint...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

Popular Stories

Akzo, SW, Nippon Logos

AkzoNobel Rejects Cash Offer From Nippon Paint, Sherwin-Williams

BASF SE Logo

BASF Announces Strategic Business Sale

AkzoSWNipponEndTalks

Nippon Paint, Sherwin-Williams End AkzoNobel Pursuit

POB-Point-and-Shoot

PCI Buyers Guide

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

Find Suppliers

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

September 15, 2026

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Automotive Paints and Coatings, 2nd Edition

Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

See More Products
Inside the AI Shift in Coatings - See the article now

Related Articles

  • Solvay Science Ambassadors Prove 'Chemistry Rocks'

    See More
  • Explosion Rocks BASF’s Ludwigshafen Site, Killing One and Injuring at Least Six

    See More
  • A Guide to Size Reduction Using Impact Machines - From Coarse to Fine

    See More

Related Products

See More Products
  • Optimizing Social Media from a B2B Perspective

See More Products

Events

View AllSubmit An Event
  • January 15, 2026

    From Data Silos to AI Success: Lessons from Collano’s Journey

    On Demand In this webinar, Raphael Schaller, CTO of Collano, shares how his team envisioned their data to make it usable for AI-driven materials discovery. He reflects on what he would do differently if starting over, and how adopting the Citrine Platform has accelerated learning, collaboration, and innovation across the organization.
View AllSubmit An Event
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing