Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!

Environmentally Friendly Corrosion-Protective Polyester Resins for Powder Coatings

By Eric Blokhuizen, Dana Ionescu, Marcel Schutte, Paul Vercoulen
March 3, 2009
DSM Uralac® Corres opens a new window of opportunity for corrosion-protective coatings.



Powder coatings are increasingly preferred over conventional solventborne and waterborne coatings. These types of coatings offer a high environmental advantage and, in addition, they are key to the economic benefit in the coating process. One of the reasons is that powder coatings are 100% solid, solvent-free materials that process with close to 100% utility. Even more important is their high technical performance.

Corrosion Protection

As the global market leader, DSM Powder Coating Resins specializes in the innovation, development and manufacture of polyester resins for powder coatings. Corrosion-protective powder coatings, based on environmentally friendly polyester, are a new DSM development in line with the company strategy on sustainability. Coatings are the primary solution to prevent corrosion of metal, and steel is the most commonly used metal. Depending on the environment where the product is in use, it needs protection from corrosion.

Uralac® Corres

Uralac® Corres is especially developed for corrosion protection on steel and can be used in many market segments. The main target segments range from thin, flat steel applications like metal furniture, shelving, heating/ventilation and domestic appliances to equipment, automotive parts and even heavy steel applications like ACE and construction beams. Corrosion protection is needed for every single application; depending on the expected lifetime and conditions of use it has its own specified requirements.

Industry Requirements



Direct Comparison Study

To support and prove the above claims, DSM ran a direct comparison with common powder coating systems. Uralac® P 7604 Corres was applied on R 46 Q-panels and compared after a 480 h natural salt spray test according to ISO 9227 with standard references like a pure epoxy, a 70/30 hybrid and a 95/ Primid system. Figure 2 clearly shows the good performance of Uralac® Corres P 7604 Corres against all three references.

In addition to passing the industry requirements, DSM used analytical tools to support its theory on the enhanced barrier properties.

Resistance Monitoring

To support the practical results on salt spray, the Dutch research and test institute TNO Science & Industry Den Helder monitored the resistance against corrosion with Electrochemical Impedance Spectroscopy (EIS). The EIS technique determines the anti-corrosive properties of a coating. This is done by measuring the resistance to an alternating current in an electrochemical cell system. The higher the measured coating resistance, the better the anti-corrosion performance.

Figure 3 shows that the anti-corrosive performance of Uralac® Corres remains good before and after the natural salt spray test, and is better than the tested reference systems. The high resistance values, also in comparison with TNO industry classification, support the theory on the high barrier against corrosion of the Uralac® Corres polyester. Due to the exceptionally good corrosion protection in metal coating, the Uralac® Corres technology offers the possibility to significantly reduce and sometimes completely eliminate chemical pre-treatment steps.



Figure 4 illustrates the reduction in process steps for a nine-stage iron phosphate pretreatment process compared to a simple cleaning process needed for Uralac® Corres.

In addition to the good technical performance, Uralac® Corres can save production space and reduce new investments especially for new lines.

Environmental Impact

Because Uralac® Corres significantly reduces or completely eliminates pretreatment steps it removes the usage of environmentally hazardous chemicals. Uralac® Corres fulfills all requirements up to 480 h NSS without any pretreatment. This is a 100% saving on hazardous phosphate chemicals, a significant risk reduction in handling and waste disposal related to the phosphate chemicals. It translates to a better work environment.

Conclusion

With high-performance corrosion protection and an ability to eliminate pretreatment steps and replace epoxy-based primers in the coating process, DSM Uralac® Corres opens a new window of opportunity for corrosion-protective coatings. DSM Powder Coating Resins continues to contribute with its cutting-edge innovation to the development of the coating industry.

For more information about the current and future portfolio of DSM Powder Coating Resins, visit www.dsmpowdercoatingresins.com, or contact your local account manager.

This article was first published in PPCJ, October 2008.

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

DSM Powder Coating Resins, The Netherlands
DSM Powder Coating Resins, The Netherlands
DSM Powder Coating Resins, The Netherlands
DSM Powder Coating Resins, The Netherlands

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • pci1022-Kinaltek-Lead-1170.jpg

    A Novel Pigment Production Technology

    Following an extensive R&D program that demonstrated...
    Paint and Coating Pigments
    By: Jawad Haidar and Nitin Soni
  • pci global top 10

    2025 Global Top 10: Top Paint and Coatings Companies

    The following is PCI’s annual ranking of the top 10...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • 2025 pci 25

    2025 PCI 25: Top Paint and Coatings Companies

    PCI's annual ranking of the top 25 North American paint...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

Popular Stories

Akzo, SW, Nippon Logos

AkzoNobel Rejects Cash Offer From Nippon Paint, Sherwin-Williams

BASF SE Logo

BASF Announces Strategic Business Sale

AkzoSWNipponEndTalks

Nippon Paint, Sherwin-Williams End AkzoNobel Pursuit

POB-Point-and-Shoot

PCI Buyers Guide

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

Find Suppliers

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

September 15, 2026

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Automotive Paints and Coatings, 2nd Edition

Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

See More Products
Inside the AI Shift in Coatings - See the article now

Related Articles

  • resins, powder coatings

    Crosslinker Resins for Powder Coatings

    See More
  • Resins for Powder Coatings from Arkema Inc.

    See More
  • Sustainable Polyesters for Powder Coatings

    See More

Related Products

See More Products
  • Kevin-Biller-PC-BOOK.jpg

    Powder Coatings - Foundation for the Novice Formulator (ebook)

  • Powder Coatings Processing (Virtual Course - 6/25/26)

  • marketsandmarketslogo.jpg

    Metallic Powder Coatings Market by Process Type (Bonding, Blending, Extrusion)...

See More Products

Related Directories

  • SUN POLYMERS International Inc.

    Sun Polymers manufactures and supplies specialty resins, curing agents, and additives for powder coatings. Sun Polymers provides polyester resins to powder coating manufacturers in a manner that is wide ranging, consistent in quality, and environmentally friendly. Sun Polymers also sells resins manufactured by our parent company, Chan Sieh Enterprises, including a wide range of acrylics, waterborne, and solvent borne resins.
  • SUN POLYMERS International Inc.

    Sun Polymers manufactures and supplies specialty resins, curing agents, and additives for powder coatings. Sun Polymers provides polyester resins to powder coating manufacturers in a manner that is wide ranging, consistent in quality, and environmentally friendly. Sun Polymers also sells resins manufactured by our parent company, Chan Sieh Enterprises, including a wide range of acrylics, waterborne, and solvent borne resins.
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing