Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!

Adapting Industrial Maintenance Coatings to Accommodate an Ever-Changing World

By Jerry M. Mitchell
September 1, 2006


As we all know, change is just a part of life. No one knows this better than paint formulators who have dealt with many changes in their market for the last few years. In the past, formulators focused on making sure their customers were satisfied by providing coatings that had consistent performance, durability, proper application viscosity, long-lasting substrate protection, and were aesthetically pleasing. Consumers want all of that, as well as low prices.

Now, in addition to performance requirements, there are various government regulations that have an impact. Environmental concerns have required formulators to remove certain additives that are considered harmful to the eco system and/or are suspected of having adverse health effects. As a result, the paint is reformulated to meet government regulations and customer needs.



Table 1. Click image for larger view.

Long-Term Performance

One of the important additives for Industrial Maintenance (IM) coatings is plasticizers. Plasticizers help to maintain film flexibility throughout the many thermal cycles that a coating experiences during its service life. Without the plasticizer the coating would become brittle and crack as the substrate expanded and contracted during hot and cold cycles of the seasons. The paint must withstand not only direct sunlight and the blistering summer heat, but also freezing rain and cold of the winter seasons. If the coating cracks, then the substrate is no longer protected from the outside elements. The substrate will then begin to deteriorate at the point where the film cracked, leading to delaminating of the coating which, in turn, leads to further deterioration of the substrate. This cycle leads to expensive repairs of the structure that the coating was developed to protect.

In a perfect world the coating would never fail, but the environment to which a coating is subjected day after day is anything but perfect. The paint formulator must determine which additive will perform the best while producing a coating that will meet both the customer needs and regulatory requirements.



Table 2. Click image for larger view.
Two of the most popular plasticizers in coatings are butyl benzyl phthalate (BBP) and dibutyl phthalate (DBP). These two plasticizers are used in many different markets such as caulks, sealants and adhesives, along with various coatings applications. They have become the plasticizers of choice for many different reasons. A primary reason is that they can be used in both waterborne and solventborne systems. These very efficient plasticizers have a high boiling point, which enables them to stay in the coating for a long time so that the film will remain flexible throughout the life of the coating. Because of these properties, these versatile products are certainly considered very "formulator friendly".

In recent years, however, ortho-phthalate plasticizers such as BBP and DBP have become targets of consumer groups that have demanded the removal of these additives in products that range from toys to coatings. On December 2, 2005, the California Office of Environmental Health Hazard Assessment (OEHHA) added BBP and DBP, along with di-n-hexyl phthalate (DnHP) to the Proposition 65 list of chemicals as being "known to the state to cause reproductive toxicity," prompting manufacturers to seek alternative products.



Table 3. Click image for larger view.
As a result, more formulators are looking for non-ortho-phthalate alternatives for their coatings. Because the two industry standards, BBP and DBP, are so versatile this can prove to be quite challenging. While there are several plasticizers on the market that are compatible with solventborne systems, there are very few that are compatible with both solvent- and waterborne systems. Fewer still have a boiling point over 300 °C to ensure that the plasticizer will remain in the film over an extended period to maintain film flexibility.



Table 4. Click image for larger view.

New Product Development

Raw material suppliers are developing new products every day to help paint formulators meet both performance and regulatory demands. As an example, one recently introduced material, Optifilm Enhancer 400, offers the best of both worlds. It is a nonphthalate alternative with a similar boiling point (Table 1) that is compatible with both solvent- and waterborne systems. In addition, it can help formulators meet a number of environmental regulations (Table 2).

Another benefit of this type of additive is that it not only keeps the films flexible but it also aids in film formation of latex systems (Table 3). This is an important benefit to formulators who are under constant pressure to reduce the VOC in their coatings. Additives such as co-solvents, thickeners, preservatives and lower-boiling plasticizers can add to the VOC level of the coating. As a coalescent, Optifilm Enhancer 400 efficiently decreases the minimum film formation temperature (MFFT) of a variety of latexes while making very little contribution to the VOC of the coating. High-boiling plasticizers like DBP and BBP will also reduce the MFFT of the latexes but with varying efficiency.



Table 5. Click image for larger view.

Formulating with Optifilm 400

Naturally, it is important that an alternative product allows the formulator to maintain the overall physical properties of the coating, and care must be exercised not only in selection but also in the amount of the product used in the paint. For example, in a solventborne lacquer formula the films were softer when Optifilm Enhancer 400 was used at equivalent levels to the ortho-phthalate plasticizers, suggesting that it is more efficient. Subsequent testing of two more coatings formulated with reduced levels of Optifilm Enhancer 400 showed that the hardness value increased with reduced levels of Optifilm Enhancer 400 while the flexibility remained constant (Table 4).

The Optifilm Enhancer 400 and the ortho-phthalate plasticizers were also evaluated for flexibility and hardness in a waterborne system. The results were similar for all three systems (Table 5). The waterborne paints were also submitted for Prohesion testing for corrosion resistance. Under the severe conditions of this test, all of the paints exhibited the same amount of blisters and rust on the surface after 500 hours exposure.

Having a choice of solutions is important for paint formulators when it comes to selecting the raw materials in their paint. Government regulations and consumer concerns have forced the formulator to become more selective in his/her choice of paint additives. Optifilm Enhancer 400 allows paint chemists to continue meeting the needs of their customers and the requirements of regulatory agencies.

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Jerry M. Mitchell, Coatings Technologist | Eastman Chemical Company, Kingsport, TN

Jerry M. Mitchell has been with Eastman Chemical Company for the last 13 years. He is currently a Coatings Technologist with the Technical Service Department of Eastman's Coatings Technology Division, serving as the technical contact for Eastman's coalescing aids and plasticizers for coatings with a focus on water-based architectural paints.

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • pci1022-Kinaltek-Lead-1170.jpg

    A Novel Pigment Production Technology

    Following an extensive R&D program that demonstrated...
    Paint and Coating Pigments
    By: Jawad Haidar and Nitin Soni
  • pci global top 10

    2025 Global Top 10: Top Paint and Coatings Companies

    The following is PCI’s annual ranking of the top 10...
    Paint and Coating Market Reports
    By: Courtney Bassett
  • 2025 pci 25

    2025 PCI 25: Top Paint and Coatings Companies

    PCI's annual ranking of the top 25 North American paint...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

Popular Stories

Akzo, SW, Nippon Logos

AkzoNobel Rejects Cash Offer From Nippon Paint, Sherwin-Williams

BASF SE Logo

BASF Announces Strategic Business Sale

AkzoSWNipponEndTalks

Nippon Paint, Sherwin-Williams End AkzoNobel Pursuit

POB-Point-and-Shoot

PCI Buyers Guide

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

Find Suppliers

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

September 15, 2026

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Automotive Paints and Coatings, 2nd Edition

Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

See More Products
Inside the AI Shift in Coatings - See the article now

Related Articles

  • First WCS Keynote Speaker to Discuss the Ever-Changing World of Architectural Coatings

    See More
  • SSPC Publishes Study Of Industrial Maintenance Coatings Market in U.S.

    See More
  • Lower VOC Limits Expected for Architectural and Industrial Maintenance Coatings

    See More
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing