Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!

Cost-Effective Ways to Increase Productivity

March 10, 2006
Q: We have an old alkyd and polyester resin manufacturing plant and want to increase productivity. Can you suggest some cost-effective ways to do it?

A: Productivity, when measured as the annual production of a given plant, is a key factor in assessing manufacturing costs. It is not surprising that many alkyd and polyester resin manufacturers under competitive pressures want to improve the productivity of their existing equipment at minimum cost.

The first area to look at is batch time. In modern plants, typical batch times are 16-19 hours for alkyds, 14-16 hours for saturated polyesters (with phthalic anhydride feed) and 18-25 hours for saturated polyesters (with isophthalic acid feed), respectively. Of course, batch times vary somewhat from one plant to another, due to different formulations and types of operations. Generally speaking, batch times are 20% to 50% longer in older plants. This leaves a lot of room for management to spend a few dollars and justify a return on investment.

Shorter batch times mean higher production rates using the same equipment. Consequently, one must look for the obvious bottlenecks in the process, such as those noted below.

  • The raw material loading and/or product unloading steps may take too long. This can easily be fixed by retrofitting larger equipment with proper automation.
  • The heating and cooling transfer rates may be too slow. This is a more difficult task to tackle, since they are limited mainly by the design of the reactor and the agitator. Assuming that replacing the reactor is not a solution due to its prohibitive cost, we are left with the following alternatives.
    1. Retrofitting a new agitator that can provide gentle but more efficient horizontal and vertical mixing.
    2. Modifying the existing heating/ cooling system to provide better control of the heating/cooling rates, thus minimizing potential fouling or degradation of the product and accelerating the energy transfer.
  • The distillation and decantation systems may be improperly designed or undersized. Revamping the existing equipment, adding more controls or operating the distillation column under vacuum may be the answer.
  • The next area to look at is process controls. It is important to examine the state of the existing instrumentation. Modern resin manufacturing plants use Programmable Logic Control (PLC)-based control systems with Human Machine Interface (HMI) as a minimum; the more sophisticated systems also have recipe management software. When touring an older plant, one of the most striking points is the lack of reliable instrumentation. Adding computers and basic instruments, such as mass flow meters, load cells, temperature transmitters etc., is a relatively inexpensive solution to the problem.

    Monitoring product viscosity and acid/hydroxyl numbers is paramount to good quality control in alkyd and polyester resin manufacturing processes. Most plants use the old-fashioned method, which consists of taking a sample from the reactor and testing it in the lab. During this procedure, valuable time (typically 30 minutes) is lost, the chemical reaction continues and the reaction end point always remains a guess.

    The net result is an approximate chemical composition of the final product. To overcome this problem, some plants have installed reactor-mounted viscometers, but without much success. The state-of-the-art solution is to retrofit continuous in-line viscosity and acid/hydroxyl number measurement systems. Such systems are proven, reliable and give instantaneous measurements of these key parameters. The operator knows the state of the reaction and the product characteristics at any given time during the batch process. The signals sent by the instruments can be integrated to the existing process control system. The benefits are numerous: consistent, on-spec product; shorter batch time; less labor involvement and a safer procedure.

    Each plant is different, and only a complete technical audit of the existing equipment and a thorough review of the operating procedures by experts will determine which of these cost-effective solutions is the best to improve productivity.

    For more information, e-mail Bernard Seguy, RHE America, at info@rhe-america.com.

    Share This Story

    Looking for a reprint of this article?
    From high-res PDFs to custom plaques, order your copy today!

    Recommended Content

    JOIN TODAY
    to unlock your recommendations.

    Already have an account? Sign In

    • pci1022-Kinaltek-Lead-1170.jpg

      A Novel Pigment Production Technology

      Following an extensive R&D program that demonstrated...
      Paint and Coating Pigments
      By: Jawad Haidar and Nitin Soni
    • pci global top 10

      2025 Global Top 10: Top Paint and Coatings Companies

      The following is PCI’s annual ranking of the top 10...
      Global Top 10 and PCI 25
      By: Courtney Bassett
    • 2025 pci 25

      2025 PCI 25: Top Paint and Coatings Companies

      PCI's annual ranking of the top 25 North American paint...
      Paint and Coating Market Reports
      By: Courtney Bassett
    You must login or register in order to post a comment.

    Report Abusive Comment

    Manage My Account
    • eMagazine
    • Newsletters
    • Online Registration
    • Subscription Customer Service

    More Videos

    Sponsored Content

    Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

    close
    • wooden kitchen set and shelving
      Sponsored bySirca North America

      Leveraging Coatings to Meet ESG Goals in Manufacturing

    • man woodworking in workshop
      Sponsored byGemini Industries, Inc.

      Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

    Popular Stories

    Akzo, SW, Nippon Logos

    AkzoNobel Rejects Cash Offer From Nippon Paint, Sherwin-Williams

    BASF SE Logo

    BASF Announces Strategic Business Sale

    AkzoSWNipponEndTalks

    Nippon Paint, Sherwin-Williams End AkzoNobel Pursuit

    POB-Point-and-Shoot

    PCI Buyers Guide

    Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

    Start your RFP

    Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

    Find Suppliers

    Events

    September 4, 2025

    N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

    ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

    September 15, 2026

    Coatings Trends & Technologies Summit

    The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

    View All Submit An Event

    Poll

    Longest-running laboratory experiment

    What is the longest-running laboratory experiment?
    View Results Poll Archive

    Products

    Automotive Paints and Coatings, 2nd Edition

    Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

    See More Products
    Inside the AI Shift in Coatings - See the article now

    Related Articles

    • A Ultimate Guide to the Safest Ways to Strip Paint

      An Ultimate Guide to the Safest Ways to Strip Paint

      See More
    • Coatings R&D Notebook: Increasing Productivity at Resin Making Plant

      See More
    • Custom-Designed Powder Coat Line to Increase Efficiency at OMT-Veyhl USA

      See More

    Related Directories

    • Eagle Specialty Products

      Serving industrial paint and coatings manufacturers since 1959, we specialize in creating advanced color pigment dispersions for water, solvent-based, and 100%-solids applications. We also offer opportunities for customization. As an ISO 9001:2015-certified company, our research and development team is equipped to create custom colorants and even toll manufacture product. Whether it's Conventional, Low-VOC, or Solvent-Free formulation, we can outfit you with the perfect solution.
    ×

    Keep the info flowing with our eNewsletters!

    Get the latest industry updates tailored your way.

    JOIN TODAY!
    • RESOURCES
      • Advertise
      • Contact Us
      • Directories
      • Store
      • Want More
      • Manufacturing Division
    • SIGN UP TODAY
      • Create Account
      • eMagazine
      • Newsletters
      • Customer Service
      • Manage Preferences
    • SERVICES
      • Marketing Services
      • Reprints
      • Market Research
      • List Rental
      • Survey & Sample
    • STAY CONNECTED
      • LinkedIn
      • Facebook
      • Youtube
      • X (Twitter)
    • PRIVACY
      • PRIVACY POLICY
      • TERMS & CONDITIONS
      • DO NOT SELL MY PERSONAL INFORMATION
      • PRIVACY REQUEST
      • ACCESSIBILITY

    Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

    Design, CMS, Hosting & Web Development :: ePublishing