Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!
Architectural CoatingsIndustrial Coatings

Anti-Pollution Paint Targets Urban Air Quality in Bangladesh

By Sk Emadul Bari, Researcher, Berger Paints Bangladesh Ltd
Dhaka, Bangladesh
Credit: Meinzahn / iStock via Getty Images Plus
December 19, 2025
  • Air pollution remains a critical environmental and public health challenge in rapidly urbanizing cities such as Dhaka, Bangladesh.
  • Rising carbon dioxide emissions from industrial activity, transportation and construction contribute to both outdoor and indoor air quality concerns.
  • Indoor environments are especially important, as people spend most of their time inside homes, schools, hospitals and workplaces.
  • Air-purifying coatings are being explored as one strategy to reduce exposure to greenhouse gases and airborne pollutants.
  • Recent product developments incorporate hybrid technologies designed to interact with carbon dioxide and other harmful gases.
  • Independent testing and validation play a key role in assessing pollutant-reduction performance under controlled conditions.

Dhaka is a rapidly growing megacity where residents pursue economic opportunity while facing mounting environmental pressures. As one of the most densely populated cities in the world, Dhaka has a population that exceeds its infrastructure capacity by an estimated four to five times. Have we ever considered whether this city can bear the pressure of such a large population and still provide adequate civic amenities?

In recent years, Dhaka has experienced severe air quality degradation. The city frequently ranks among the most polluted globally. As pollution levels rise, both environmental and public health risks continue to intensify.

Figure 1. Average AQI in 2024. Source: Air Quality Index (AQI).


Figure 1Source: Air Quality Index (AQI) via Berger Paints.


An analysis of air pollution sources in Dhaka shows that carbon dioxide (CO₂) and other greenhouse gases are primary contributors. Emissions from power plants, construction debris, industrial activity and transportation have all contributed to the toxic air that residents breathe daily.

Figure 2. Yearly CO₂ emissions in Bangladesh. Source: IEA (International Energy Agency).

Figure 2Source: IEA (International Energy Agency) via Berger Paints.


Bangladesh’s CO₂ emissions increased from 59.81 million tonnes in 2010 to 106.87 million tonnes in 2021, reflecting an average annual growth rate of approximately 5.5%. If this trend continues, emissions are projected to reach more than 155.45 MT CO₂ by 2028. If carbon emissions cannot be controlled, the environment may face serious long-term consequences, raising concern for both present and future generations.

Indoor air quality presents an additional challenge. Studies indicate that people spend approximately 80%–90% of their time indoors, making interior environments a significant factor in overall pollutant exposure. Maintaining acceptable levels of carbon dioxide and limiting other airborne contaminants is especially important for vulnerable populations, including children and older adults.

Berger Paints (BD) Ltd. has taken an initiative by launching Eco Coat, described as Bangladesh’s first anti-pollution paint, developed to address air pollution challenges. Air Purifying Hybrid (APH) technology, developed by Berger R&D researchers, is used to neutralize harmful airborne pollutants. According to the company, this paint is designed to absorb greenhouse gases including carbon dioxide (CO₂) and methane (CH₄), as well as toxic gases such as carbon monoxide (CO), hydrogen sulfide (H₂S), sulfur oxides (SOx), nitrogen oxides (NOx) and formaldehyde (HCHO) present in the air.

Figure 3. Berger Eco Coat: CO₂ absorption efficacy (%) and CO₂ absorption in ppm. Source: BUET test report.

Berger Paints Figure 3Source: BUET test report via Berger Paints 


The graphical data show that the CO₂ concentration in a demonstration room prior to application was measured at 4515 ppm. Three hours after application of the product, CO₂ levels reportedly decreased to 273 ppm, corresponding to a measured reduction efficiency of approximately 94%. Based on available test results, the coating demonstrated a capacity to reduce indoor air pollutants by up to 90% under specific conditions.

The coating is intended for both interior and exterior applications, including residential buildings, schools, hospitals and other enclosed environments where ventilation may be limited. The product has been tested and validated by SGS Bangladesh, Rudolf (Germany) and the Bangladesh University of Engineering and Technology (BUET).

Figure 4. Summary of air pollutant removal efficiency for Berger Eco Coat.

Figure 4Credit: Berger Paints


Berger Paints states that its products are formulated to be lead-free and free of other heavy metals, as well as low-VOC and APEO-free. In the context of growing concern around carbon footprints, Eco Coat represents one approach aimed at supporting more sustainable building practices. According to Md. Mohsin Habib Chowdhury, chief operating officer of Berger Paints Bangladesh Limited and president of the Bangladesh Paint Manufacturer’s Association (BPMA), “We recognize industry challenges and actively invest in climate-specific solutions.” The focus on environmental sustainability continues to grow worldwide, contributing to rising interest in eco-friendly paint technologies.

Berger Paints Bangladesh won the SDG Brand Champion Award this year in the Industry, Innovation and Infrastructure category. The company said this marks the first time a product from Bangladesh’s paint industry has received the award. Dr. A.S.M. Obaidullah Mahmud, chief research and development officer of Berger Paints Bangladesh and the developer of Berger EcoCoat, has focused his research on coatings intended to support healthier living and environmental responsibility. The company said his work has contributed to the development of paints that are free of harmful heavy metals, low in volatile organic compounds (VOCs) and formulated without alkylphenol ethoxylates (APEO) and nonylphenol ethoxylates (NPEO). The company said these efforts support eco-friendly paint solutions and aim to reduce greenhouse gas emissions, with Berger EcoCoat positioned as part of that approach.

Advances in sustainable coatings continue to shape how manufacturers address environmental performance and regulatory pressures across global markets.

KEYWORDS: air quality chemical-resistant coatings environmental health and safety manufacturing raw material raw materials raw materials for coatings sustainability Sustainability in Coatings VOCs

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Sk Emadul Bari, Researcher, Berger Paints Bangladesh Ltd

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • pci1022-Kinaltek-Lead-1170.jpg

    A Novel Pigment Production Technology

    Following an extensive R&D program that demonstrated...
    Paint and Coating Pigments
    By: Jawad Haidar and Nitin Soni
  • pci global top 10

    2025 Global Top 10: Top Paint and Coatings Companies

    The following is PCI’s annual ranking of the top 10...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • 2025 pci 25

    2025 PCI 25: Top Paint and Coatings Companies

    PCI's annual ranking of the top 25 North American paint...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

  • colorful building exterior
    Sponsored byDow

    Insights into Exterior Architectural Coating Degradation: Bridging Accelerated and Natural Weathering

Popular Stories

Supply chain question and cargo piles up and piling shipping containers question concept

Energy Disruptions Begin to Hit Coatings Supply Chain

basf

BASF Coatings Names Incoming CEO Ahead of Separation

PPG announced the installation of a state-of-the-art pilot finishing line that features IPG’s PhotoniCURE™ laser curing system at its powder manufacturing and technical facility in Strongsville, Ohio.

PPG Tests Laser Curing for Powder Coatings

POB-Point-and-Shoot

PCI Buyers Guide

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

Find Suppliers

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

March 31, 2026

Durability by Design: Waterborne Concrete Coatings that Protect, Beautify, and Extend Service Life

Attend this webinar to understand how protecting concrete enables lifespan extension and reduction of the CO₂ emissions associated with premature repair or replacement.
View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Automotive Paints and Coatings, 2nd Edition

Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

See More Products
Register for webinar: Next-Gen Dispersion Technology in Paint Production

Related Articles

  • Express Painting Service by Female

    Bangladesh’s Paint Industry Sees Rise of Female Painters

    See More
  • Clean energy, eco-friendly, sustainable solutions in industry. 3D green molecular illustration

    VOCs in Paint and Coatings: Sources, Risks and Benchmarks

    See More
  • Sunscreen coating system

    Radiative “Sunscreen” Coating Targets Urban Cooling

    See More

Related Products

See More Products
  • durability.jpg

    Increasing the Durability of Paint and Varnish Coatings in Building Products and Construction 1st Edition

See More Products

Events

View AllSubmit An Event
  • April 28, 2026

    Next Gen Dispersion Technology in Paint Production: Driving Higher Quality at Lower Costs

    Join this webinar to see how manufacturers reduce costs, energy use, raw materials, labor, and floor space while improving quality.
View AllSubmit An Event
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing