    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!
Paint and Coating PigmentsArchitectural CoatingsIndustrial CoatingsSustainable

Pigments in Modern-Day Coatings Formulations

By PCI Magazine
Pigments for coloring, in petri dishes
RHJ / iStock via Getty Images Plus
March 4, 2026

Market Momentum and Segment Shifts

Pigments continue to anchor coatings demand across architectural, industrial and specialty applications, with global consumption tracking broader construction and manufacturing activity. Public market analyses estimate the global pigments market at approximately $33 billion in 2024, with forecasts pointing to mid-single-digit annual growth through 2035, supported by replacement demand and continued use across paints and coatings, plastics and printing inks.¹

Within that broader market, organic pigments are gaining ground. Industry estimates place the organic pigments market at roughly $3.5–3.6 billion in 2024, with projected growth of about 6% CAGR through the early 2030s, outpacing many traditional inorganic pigment segments. Asia-Pacific accounts for the largest share of both production and consumption, reflecting the region’s concentration of coatings manufacturing capacity and downstream end-use demand.²


Functional Pigments in Coatings Performance

Functional pigments are routinely selected for roles tied to corrosion resistance, UV protection, reflectivity and thermal response, depending on application demands. Anticorrosive pigments support metal protection, pearlescent pigments contribute visual depth and specialty pigments enable safety or performance signaling through light or temperature response.³ As coatings applications become more specialized, pigment choice increasingly intersects with formulation strategy.


Pigment Research in Coatings Science

Research in coatings science continues to examine how pigment characteristics influence film performance at both the microscopic and macroscopic levels. Recent studies have focused on pigment–polymer interactions, dispersion behavior and surface modification strategies, with attention to how these factors affect optical properties, mechanical stability and weathering resistance.⁴


Pigment Research in Coatings Science

Carbon black remains one of the most widely used pigments in coatings, valued for its opacity, UV protection and conductivity. At the same time, producers are reassessing how this long-established material fits into changing sustainability expectations and performance requirements. Industry discussions point to growing interest in alternative feedstocks, process efficiency improvements and expanded functionality beyond traditional coloration.⁵ These themes are expected to shape discussions at Carbon Black World 2026.


References

¹ Transparency Market Research. Pigments Market—Global Industry Analysis, Size, Share, Growth, Trends and Forecast, 2025–2035.
https://www.transparencymarketresearch.com/pigments-market.html.

² Grand View Research. Organic Pigments Market Size, Share and Trends Analysis Report.
https://www.grandviewresearch.com/industry-analysis/organic-pigments-market.

³ SA Materials. The Functional Pigments Commonly Found in Coatings.
https://www.samaterials.com/content/the-functional-pigments-commonly-found-in-coatings.html.

⁴ Progress in Organic Coatings. Pigment–polymer interactions and their influence on coating performance. ScienceDirect.
https://www.sciencedirect.com/science/article/pii/S0300944025006629.

⁵ Carbon Black World. Interview with Greenergy One Company Limited.
https://www.carbonblackworld.com/carbon-black-world/speaker-interview/interview-with-greenergy-one-company-limited.

KEYWORDS: Carbon Black Organic Pigments

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • pci1022-Kinaltek-Lead-1170.jpg

    A Novel Pigment Production Technology

    Following an extensive R&D program that demonstrated...
    Paint and Coating Pigments
    By: Jawad Haidar and Nitin Soni
  • pci global top 10

    2025 Global Top 10: Top Paint and Coatings Companies

    The following is PCI’s annual ranking of the top 10...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • 2025 pci 25

    2025 PCI 25: Top Paint and Coatings Companies

    PCI's annual ranking of the top 25 North American paint...
    Paint and Coating Market Reports
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

  • colorful building exterior
    Sponsored byDow

    Insights into Exterior Architectural Coating Degradation: Bridging Accelerated and Natural Weathering

Popular Stories

Supply chain question and cargo piles up and piling shipping containers question concept

Energy Disruptions Begin to Hit Coatings Supply Chain

basf

BASF Coatings Names Incoming CEO Ahead of Separation

PPG announced the installation of a state-of-the-art pilot finishing line that features IPG’s PhotoniCURE™ laser curing system at its powder manufacturing and technical facility in Strongsville, Ohio.

PPG Tests Laser Curing for Powder Coatings

POB-Point-and-Shoot

PCI Buyers Guide

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

Find Suppliers

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

March 31, 2026

Durability by Design: Waterborne Concrete Coatings that Protect, Beautify, and Extend Service Life

Attend this webinar to understand how protecting concrete enables lifespan extension and reduction of the CO₂ emissions associated with premature repair or replacement.
View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Automotive Paints and Coatings, 2nd Edition

Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

See More Products
Register for webinar: Next-Gen Dispersion Technology in Paint Production

Related Articles

  • From the Heart of Africa to the Modern-Day Oil Patch, Paints Have Come a Long Way

    See More
  • Solvent Usage in Modern Coatings

    See More
  • LANXESS Inorganic Pigments Sample

    Pigments for Low-Carbon-Footprint Coating Formulations

    See More

Related Directories

  • Formulator Software LLC

    At Formulator Software, we understand the precision and complexity involved in perfecting formulations. Our software is designed specifically for chemists, lab technicians, researchers, and manufacturers, providing essential tools to streamline the entire formulation process. Formed in 2002, Formulator Software is trusted by thousands to manage their raw materials, formulations, QC, SDS, COA, costing and more!
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing