Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!
Breaking News

Carbon-Nanotube Coating Renders a 3D Object Flat

December 4, 2011

ANN ARBOR, MI — A carbon-nanotube coating developed at the University of Michigan acts as a "magic black cloth" that conceals an object's three-dimensional geometry and makes it look like a flat black sheet.

The 70-micron coating, or carbon-nanotube carpet, is about half the thickness of a sheet of paper. It absorbs 99.9 percent of the light that hits it, researchers say.

“You could use it to completely hide any 3D attributes of an object,” said Jay Guo, a professor in the Department of Electrical Engineering and Computer Science and principal investigator.

"It's not cloaking, as the object can still cast a shadow. But if you put an object on a black background, then with this coating, it could really become invisible."

A paper on the research is newly published online in Applied Physics Letters.

To demonstrate this concept, the researchers made a raised, microscopic tank shape on a piece of silicon. They then grew the carbon-nanotube carpet on top of the entire silicon chip. In photos taken through an optical microscope, they show that the tank is imperceptible. As a control, they did this again, carving out a rectangle that was not coated with carbon nanotubes. The rectangle is visible on this chip, but the tank remains hidden.

Here's how the new coating works: Human eyes perceive an object based on how it reflects or scatters light. The "refractive index" of this new coating is similar to that of air, meaning light traveling through air doesn't scatter or reflect when it hits the coating.

It's well known that carbon nanotubes are capable of absorbing light, but the researchers were able to push it to such a high percentage by spacing them just right.

The "perfect black" material Guo's team created for this coating has a host of varied applications. It could possibly be used in display screens for ultra-high contrast and a crisper picture. It holds promise as solar heating device. The National Institute of Standards and Technology is using a similar material to absorb infrared light and measure the amount of heat it can generate.

The coating could inspire a new type of camouflaging paint for stealth aircraft. Today's stealth planes use shape to scatter electromagnetic waves and avoid detection, and this scheme could actually absorb the waves.

"The carbon-nanotube forest can absorb very wide range of electromagnetic wave from ultraviolet up to terahertz," Guo said. "And in principle, it can be applied to an arbitrary-sized object."

Just how large an object? Guo suggested an intriguing possibility: perhaps entire planets or even stars.

"Since deep space itself is a perfect dark background, if a planet or star were surrounded by a thick, sooty atmosphere of light-absorbing carbon nanomaterial gases, it would become invisible due to the same principle," Guo said. "It would become totally dark to our instruments that rely on the detection of electromagnetic waves. Could this explain some of the missing matter in the universe?"

X-rays or gamma rays would be able to penetrate through the hypothetical "dark veil" Guo proposes. Or, objects behind such veils would cast a shadow by distant stars behind them.

The paper is called "Low density carbon nanotube forest as an index-matched and near perfect absorption coating." Other co-authors are electrical engineering post-doc Haofei Shi and Ph.D. student Hyoung Won Baac and mechanical engineering Ph.D. student Jong Ok. The university is pursuing patent protection for the intellectual property, and is seeking commercialization partners to help bring the technology to market. 

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • pci1022-Kinaltek-Lead-1170.jpg

    A Novel Pigment Production Technology

    Following an extensive R&D program that demonstrated...
    Paint and Coating Pigments
    By: Jawad Haidar and Nitin Soni
  • pci global top 10

    2025 Global Top 10: Top Paint and Coatings Companies

    The following is PCI’s annual ranking of the top 10...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • 2025 pci 25

    2025 PCI 25: Top Paint and Coatings Companies

    PCI's annual ranking of the top 25 North American paint...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

Popular Stories

Akzo, SW, Nippon Logos

AkzoNobel Rejects Cash Offer From Nippon Paint, Sherwin-Williams

BASF SE Logo

BASF Announces Strategic Business Sale

AkzoSWNipponEndTalks

Nippon Paint, Sherwin-Williams End AkzoNobel Pursuit

POB-Point-and-Shoot

PCI Buyers Guide

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

Find Suppliers

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

September 15, 2026

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Automotive Paints and Coatings, 2nd Edition

Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

See More Products
Inside the AI Shift in Coatings - See the article now

Related Articles

  • Carbon-Nanotube Coating Renders a 3D Object Flat

    See More
  • Brewer Science Commercializes First Microelectronics-Grade Carbon Nanotube Coating - Posted 7/25/07

    See More
  • Study Reveals Process to Make High-Performance Carbon Nanotube "Inks"

    See More

Related Products

See More Products
  • Hansen Solubility Parameters – A Scientific Approach for Coating Formulators (Virtual Course - 8/20/26)

  • coatings.jpg

    Advanced Coating Materials

See More Products
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing