Additives Consumption Study Released

ELMWOOD PARK, NJ – According to Global Coating & Ink Additives, a new study by the consulting firm Kusumgar, Nerlfi & Growney, consumption of the five leading additives for coatings and inks was 1.72 billion pounds, worth $3.47 billion, in 2009. Volume was down 10 percent compared to 2008, with North American and European usage down the most. Additive consumption in the Asia-Pacific region was off a more modest three percent, as growth in China and India partially offset the declines in Japan and South Korea. A five percent annual rate of growth is forecast for global additive consumption through 2014.

Rheology modifiers are the leading additive type with 39 percent of the 2009 dollars. Cellulosics, water-based synthetics, fumed silicas and organoclays are the leading rheology modifiers. Foam-control additives edged out dispersants for second in value in 2009 with the bulk used in water-based paints. Dispersants were 17 percent of the dollars and range from highly specialized polymeric types to higher-volume polyacrylic acid varieties for architectural paints.

Slip-and-rub additives were fourth in value and are comprised of wax products and silicones. Wetting agents were 11 percent of the volume and 12 percent of the value in 2009.

You must register or login in order to post comments.

Multimedia

Videos

Image Galleries

American Coating Show 2012

The American Coatings Show and Conference, held every two years, took place May 7-10 at the Indiana Convention Center in Indianapolis, IN, in the heart of the Manufacturing Belt, the oldest and largest concentration of industrial companies in the Midwest.

Podcasts

PCI Top 5 - January 12, 2012
PCI's Podcast series on the five most e-mailed/shared articles and stories for the week.

More Podcasts

THE MAGAZINE

PCI Magazine

PCI may 2012 cover

2012 May

Check out PCI's May issue!!

TABLE OF CONTENTS SUBSCRIBE

2012 Sales Growth

What is your projected sales growth for 2012?
See Poll Results Poll Archive

THE PCI STORE

PCI-June-2011-Coversmall.gif
PCI Additives Handbook

Encyclopedia of information on the properties and uses of coatings additives.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

Virtual Brochures

PageCollageClick on the Virtual Brochures page to view multiple categories that list downloadable product literature from leading industry suppliers.

STAY CONNECTED

Facebook Twitter  LinkedIn YouTube