Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!
FT Archives

Boosting Appliance Appeal

By Charles Baldwin, Jim Gavlenski
June 1, 2008
Copper Evolution™, a metallic-look porcelain enamel coating, provides a durable, cost-effective finish on a grill.


Appliance designers face a difficult task. The cost of stainless steel and other materials continues to increase, yet prices must be kept low to drive consumer purchases without compromising style or performance. How can these seemingly opposing goals be achieved? Ceramic finishes offer a solution. New porcelain enamel-derived coatings are taking today’s stylish home and industrial finishes to a higher level, with performance that maintains beauty to build long-term brand popularity.

Figure 1. Stainless-Style Evolution™ on a range (photo courtesy of Whirlpool® Corp.).

Durable Metallic Finishes

Metallic surfaces, special effect colors and reflective finishes increasingly have found their way into product design. The metallic trend shows no sign of slowing, but the growing demand for stainless steel appliances, outdoor grills, fire bowls and decorative items has dramatically boosted base metal prices. For example, 304 stainless steel typically used for appliances contains 8 to 10.5% nickel. According to USGS Minerals Information, about two-thirds of all nickel production was earmarked for stainless steel in 2005. Cost data from the London Metals Exchange shows a steep price jump, with nickel prices nearly quadrupling from $5.40/lb in December 2005 to $22.78/lb in 2007 before falling back slightly in 2008.1 Copper, chrome and other metal prices have risen sharply as well.

Appliance designers have taken these sharp cost increases on the chin. Fortunately, new developments in porcelain enamels are presenting a more cost-effective alternative. These engineered coatings give trendy metallic looks with a substantially lower price.

Using these new coatings, designers can fabricate a range or another appliance from 24-gauge enameling steel instead of 300 series stainless. The coating would be applied as a 0.002 in. (2 mil) ground coat and a 0.004 in. (4 mil) cover coat. Using general market prices, the metallic-look porcelain enamel could reduce costs by nearly 50% compared to stainless steel. The porcelain coating also withstands scratches that typically damage a significant percentage of stainless steel parts during fabrication, turning them into scrap. Porcelain enamel- coated parts also lend themselves to the superior forming characteristics of carbon steel versus the more difficult to form stainless steel.

Coating colors developed to date include several shades of stainless, mirror finishes and copper. Figure 1 shows a stainless-style porcelain enamel-coated range.

The coating is applied and fired like conventional porcelain enamel. It provides the benefits of enamels such as:
  • Sanitary qualities
  • Easy cleaning
  • Superior scratch and abrasion resistance
  • Superior chemical and corrosion resistance
  • Flame resistance
  • Color stability
  • A low environmental impact with zero solvents
Additionally, prior studies have shown porcelain enamels to be significantly more durable than 304 austenitic stainless steel.2 Since austenitic stainless is more corrosion resistant than the ferritic stainless, one can conclude that the porcelain enamel coating would be more durable than the ferritics as well. The coating colors are suitable for appliances, barbecue grills, housewares, architectural components, automotive parts and general industrial applications. The coatings also could be used to develop accent pieces with stainless or to create durable cabinetry.

Figure 2a. After soaking test panels soiled with baked-on strawberry jam in soapy water for 15 minutes, the AquaRealEase™ panel (above) wiped completely clean, but the pyrolytic panel (below) retained significant soil.

Steam-Cleanable Surfaces

Oven cleaning technology consists of three types: self-cleaning pyrolytic ground coats, non-self-cleaning ground coats or catalytic continuous-clean enamels. The first reduces foodstuffs to ash with exposure to temperatures between 900 and 1,000°F (482 and 538°C), while the second requires harsh alkaline cleaners to remove soils. The third, which largely has fallen out of use, relies on porous enamels to catalyze the reduction of soils to ash at normal cooking temperatures.

Innovations in porcelain enamel technology are providing a new alternative. These coatings allow baked-on food residues to be released with exposure to moisture (either as water or steam), thereby offering a more environmentally friendly and energy-efficient option to cleaning ovens without the use of harsh chemicals, high temperatures and the resulting fumes in the kitchen. Additionally, interlocks and extra insulation are not required, freeing oven manufacturers to add other features such as advanced electronics or integration into a home network to the previously old-fashioned range.

These advanced coatings can be applied in a single coat over existing oven finishes. They have the mechanical durability and superior thermal resistance of traditional enamel, can be applied to steel in a single fire, and fire out between 1470 and 1570°F (799 and 854°C).

Figure 2 shows the comparative cleaning results of test panels coated with traditional pyrolytic enamel and the new porcelain enamel technology. Strawberry jam was baked on both panels at 450°F (232°C) for one hour, then the soiled panels were soaked in soapy water for 15 minutes. The porcelain enamel panel wiped completely clean, while the pyrolytic panel retained significant soil.

Figure 2b. The strawberry jam-coated pyrolytic panel.

Although cleaning cycles might vary for various range manufacturers, the advanced coating sheds baked-on soils in service with exposure to steam. The steam can be generated with closed vents by using only the lower heating element to heat 1 qt of water in a pan on the lower rack to 190°F (88°C) for at least 30 minutes. Then, the oven is turned off and allowed to cool for 30 minutes. The sides of the cavity are wiped with the soft side of the sponge to allow water to run down the sides. After 20 minutes, the soils can be wiped out of the range. Because of the use of steam for the cleaning cycle, the advanced porcelain enamel coating holds promise for steam cooking ranges emerging on the market. It is currently in use on a commercially produced range.3

Figure 3. A toaster oven coated with the nonstick RealEase® ceramic composite finish.

Nonstick Solutions

New ceramic composites combine the cleanability of organic nonstick coatings, such as polytetrafluoroethylene (PTFE), with the hardness and durability of a ceramic coating. Some of the benefits of the coating include:4
  • Cleanability equal to PTFE coatings and superior to stainless steel
  • A pencil hardness of 8H
  • Superior heat resistance compared to PTFE coatings
  • Conformability to U.S. Food and Drug Administration (FDA) requirements
  • A low environmental impact with zero solvents
While significant concerns about the chemical components of PTFE-based nonstick coatings continue to exist,5 the new composites provide a vitreous ceramic finish that meets EPA 2010 guidelines. Additionally, because of the scratch resistance of the material and a lower tendency to discolor on exposure to heat, the original appearance can be maintained longer than PTFE.

The coatings can be applied to a variety of substrates, including aluminum, stainless steel, aluminized steel, cast iron, enameling steel and ceramic. For aluminum and stainless steel, roughening with blasting is required, while aluminized steel only needs an alkaline degrease. For cast iron and steel, the light application of a proprietary primer is necessary. Additionally, for facilities with enameling capabilities, several vitreous primers called hard bases are available, which have been used as base coats on ceramics.

The coatings can be used to create a wipe-clean surface usable up to 500°F (260°C). For domestic uses, these include cookware and bakeware (aluminum, aluminized steel, stainless steel, or ceramic), small appliances, toaster and microwave ovens, simmer plates, and outdoor/backyard grills/griddles. Because the coatings are certified as safe for use in restaurant kitchens, they are also suitable for commercial kitchenware, cookware, bakeware, and appliances.

Figure 3 shows a commercially available toaster oven with the ceramic composite coating on the oven cavity. The coating also could offer the same tough, nonstick properties on free-standing or built-in ranges.

New Options for Appliances

Metallic-colored porcelain enamel coatings provide durable, attractive metallic finishes that are suitable for high-end products. Water-cleanable coatings offer an oven-cleaning technology that eliminates the need for high heat, fumes or caustic cleaners. And nonstick coatings have a firing temperature and cleanability similar to PTFE coatings but with superior scratch and thermal resistance. These new technologies are providing cost-effective options for enhancing the style and performance of modern appliances and cookware.


For more information, call 216.750.2310 or visit www.ferro.com.

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Charles Baldwin is technical manager at Ferro Corp., Cleveland, OH, supplier of the Evolution™ (metallic), AquaRealEase™ (steam-cleanable) and RealEase® (nonstick) porcelain enamel technologies.
Jim Gavlenski is responsible for new product sales at Ferro Corp.

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • pci1022-Kinaltek-Lead-1170.jpg

    A Novel Pigment Production Technology

    Following an extensive R&D program that demonstrated...
    Paint and Coating Pigments
    By: Jawad Haidar and Nitin Soni
  • pci global top 10

    2025 Global Top 10: Top Paint and Coatings Companies

    The following is PCI’s annual ranking of the top 10...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • 2025 pci 25

    2025 PCI 25: Top Paint and Coatings Companies

    PCI's annual ranking of the top 25 North American paint...
    Paint and Coating Market Reports
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

Popular Stories

Akzo, SW, Nippon Logos

AkzoNobel Rejects Cash Offer From Nippon Paint, Sherwin-Williams

BASF SE Logo

BASF Announces Strategic Business Sale

AkzoSWNipponEndTalks

Nippon Paint, Sherwin-Williams End AkzoNobel Pursuit

POB-Point-and-Shoot

PCI Buyers Guide

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

Find Suppliers

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

September 15, 2026

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Automotive Paints and Coatings, 2nd Edition

Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

See More Products
Inside the AI Shift in Coatings - See the article now

Related Articles

  • Flood Co. Announces Additional Move Aimed at Boosting Overseas Business

    See More
  • MATERIALS: Metallic-Look Appliance Coatings

    See More
  • Appliance Manufacturer Benefits from New Pretreatment Process - Posted 11/14/07

    See More

Related Products

See More Products
  • thin film.jpg

    Thin Film Coatings Properties, Deposition, and Applications

  • April 18, 2024

  • October 24, 2024

See More Products

Events

View AllSubmit An Event
  • September 24, 2025

    Boosting Margins in Paint, Coatings & Sealant Manufacturing

    On Demand Attend this webinar to hear real examples of margin growth through accurate data visibility, eliminating estimations.
View AllSubmit An Event

Related Directories

  • X-Rite Pantone

    X-Rite delivers advanced color measurement and management solutions for the paints and coatings industry. Its instruments and software support precise color formulation, quality control, and consistency across production. X-Rite empowers manufacturers to achieve accurate, repeatable color, reduce waste, and enhance product appeal in decorative, industrial, and automotive coatings.
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing