DEARBORN, MI – BYK-Gardner hosted its sixth user meeting April 12-13 at the historical Henry Ford Museum in Dearborn, MI. Dr. Georg Schroeder, President, opened the meeting with an overview of BYK’s business structure and focus.
The focus of the meeting was on color and appearance harmony, with in-depth discussions on gloss, waviness, color match, effect and mottling. The meeting included presentations from General Motors, Boeing, Akzo Nobel Car Refinishes, Q-Lab, Wyle Integrated Science and Engineering Group, Eckart America, DuPont Performance Coatings, Office Color Science Co., BYK-Gardner and BYK-Chemie.
At the conclusion of the first day, the 140+ attendees were treated to a sit-down dinner in the heart of the Henry Ford Museum, followed by a private tour of the facility.