MUTTENZ, Switzerland - Clariant is reorganizing the sales and distribution of its aluminum finishing activities in Europe. Effective April 1, 2007, the Swiss Omya group will be the exclusive distributor of the aluminum finishing products of Clariant’s Pigments & Additives Division. The goal of this measure is to reduce logistic complexity and offer improved customer service in all of Europe from one source.