Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!
FT Archives

Copper Coatings Hold Promise for Antimicrobial Surfaces - Posted 1/2/08

January 2, 2008
The Copper Development Association has been awarded congressionally appropriated funds to continue clinical trails determining the antimicrobial effectiveness of copper, brass and bronze. Of the two studies funded by these appropriations, one is focused on the ability of copper alloy surfaces to kill deadly pathogens and impede cross-contamination. The monies will be used to complete the pilot conversion of touch surfaces in healthcare facilities in New York City and Charleston, SC, where extensive clinical trials have begun.

The Copper Development Association has been awarded congressionally appropriated funds to continue clinical trails determining the antimicrobial effectiveness of copper, brass and bronze.

Of the two studies funded by these appropriations, one is focused on the ability of copper alloy surfaces to kill deadly pathogens and impede cross-contamination. The monies will be used to complete the pilot conversion of touch surfaces in healthcare facilities in New York City and Charleston, SC, where extensive clinical trials have begun.

The other, which follows the same premise, is designed to demonstrate the effectiveness of copper components in heating, ventilating and air-conditioning (HVAC) systems in reducing the incidence of harmful microbes that spread throughout buildings and other indoor air environments.

According to Dr. Harold Michels, vice president of Technical and Information Services for CDA and the studies’ principal investigator, “This decision allows the trials to move into the next, critical phase of study. We fully expect our work will demonstrate that the utilization of antimicrobial copper alloy surfaces will be an effective weapon in the battle against hospital- and community-acquired infections and, when used in conjunction with good clinical hygiene, will help greatly to reduce the spread of certain virulent, antibiotic-resistant pathogens, such as methicillin-resistant Staphylococcus aureus (MRSA) and E. coli O157:H7.”

The clinical trials follow peer-reviewed research conducted at the University of Southampton in the U.K. proving that copper, brass and bronze can quickly and efficiently eradicate several different pathogens that are the source of many hospital-acquired infections. Estimates from the U.S. Centers for Disease Control and Prevention (CDC) state that infections acquired in U.S. hospitals affect some two million individuals every year, resulting in nearly 100,000 deaths annually and costing the healthcare industry some $30 billion. It is widely believed those numbers will grow, unless more effective measures are implemented.

The touch surfaces trials will determine how well natural copper, brass and bronze surfaces mitigate infectious microbes, decrease cross-contamination and ultimately help reduce the incidence of hospital-acquired infections in patients. Rates of infection are being measured using three indicator organisms: MRSA, vancomycin-resistant Enterococci (VRE) and Acinetobacter baumannii. The surfaces involved in the study are typically made of coated carbon steel, aluminum, stainless steel or plastic, which have little or no effect in controlling pathogens.

The studies are being conducted at Memorial Sloan-Kettering Cancer Center in New York City, the Medical University of South Carolina and the Ralph H. Johnson VA Medial Center, both in Charleston, SC. Previous studies were conducted by ATS Labs in Eagan, Minnesota, under test protocols established by the U.S. Environmental Protection Agency. They show solid copper alloys are more than 99.9% effective on five pathogens commonly found in healthcare facilities. The tests have been submitted to EPA as part of a registration process to secure approval for making human health claims for the copper metals.

For more information, visit www.copper.org.

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • pci1022-Kinaltek-Lead-1170.jpg

    A Novel Pigment Production Technology

    Following an extensive R&D program that demonstrated...
    Paint and Coating Pigments
    By: Jawad Haidar and Nitin Soni
  • pci global top 10

    2025 Global Top 10: Top Paint and Coatings Companies

    The following is PCI’s annual ranking of the top 10...
    Paint and Coating Market Reports
    By: Courtney Bassett
  • 2025 pci 25

    2025 PCI 25: Top Paint and Coatings Companies

    PCI's annual ranking of the top 25 North American paint...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

Popular Stories

Akzo, SW, Nippon Logos

AkzoNobel Rejects Cash Offer From Nippon Paint, Sherwin-Williams

BASF SE Logo

BASF Announces Strategic Business Sale

AkzoSWNipponEndTalks

Nippon Paint, Sherwin-Williams End AkzoNobel Pursuit

POB-Point-and-Shoot

PCI Buyers Guide

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

Find Suppliers

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

September 15, 2026

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Automotive Paints and Coatings, 2nd Edition

Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

See More Products
Inside the AI Shift in Coatings - See the article now

Related Articles

  • PPG Offers Seacoast Corrosion Warranty for DURANAR Coatings - Posted 1/2/08

    See More
  • RadTech Opens Online Registration for UV&EB Technology Expo - Posted 1/2/08

    See More
  • BASF Expands Waterborne Basecoat Production - Posted 1/2/08

    See More

Related Products

See More Products
  • Handbook of Adhesives and Sealants, Volume 1

See More Products

Related Directories

  • American Chemet Corp.

    American Chemet is a manufacturer and marketer of cuprous oxide for anti-fouling paint, preservatives and anti-microbial applications. Chemet is a leading producer of cupric oxide, copper-based powders, basic copper carbonate, copper catalyst, and market zinc oxide.
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing