DuBois Chemicals, Cincinnati, OH, working with ACT Test Panel Technologies, Hillsdale, MI, has produced a new “standard” paint pretreatment and metal surface finishing test panel.
SHARONVILLE, OH – DuBois Chemicals, Cincinnati, OH, working with ACT Test Panel Technologies, Hillsdale, MI, has produced a new “standard” paint pretreatment and metal surface finishing test panel. The panels are coated with the new DuBois non-phosphate, low-temperature Zirconization paint pretreatment process. The DuraTEC process, which is zirconium based, is a high-performing alternative to traditional iron phosphate conversion coatings that can be applied via traditional spray washer, immersion or spray wand.
SHARONVILLE, OH – DuBois Chemicals, Cincinnati, OH, working with ACT Test Panel Technologies, Hillsdale, MI, has produced a new “standard” paint pretreatment and metal surface finishing test panel. The panels are coated with the new DuBois non-phosphate, low-temperature Zirconization paint pretreatment process. The DuraTEC process, which is zirconium based, is a high-performing alternative to traditional iron phosphate conversion coatings that can be applied via traditional spray washer, immersion or spray wand.


More

With access to over one million professionals and more than 60 industry-specific publications,