Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!
Breaking NewsIndustry News

ECC ‘Coatings for Plastics' Program in Berlin Examines Adhesion Issues

May 1, 2004
Boasting 91 participants from 21 countries, the first European Coatings Conference (ECC) devoted to "Modern Coatings for Plastics Substrates", held on 24th and 25th November, 2003, was very much an international affair. The program of events, which was jointly organized by Vincentz Network and the German Research Association for Surface Treatment (Deutsche Forschungsgesellschaft für Oberflächenbehandlung, DFO), covered the entire chain of plastics coatings production.

A key issue in the coating of plastics is of course adhesion - and so it was no surprise that the first day of the conference was almost totally devoted to substrates and their pre-treatment. Adhesion, especially to thermoplastic polyolefins (TPOs), remains a substantial problem for waterborne coatings.

NCPOs for TPOs

Paul Swan (Eastman) presented new non-chlorinated polyolefin adhesion promoters (NCPOs) which, in primers, and especially when blended with traditional CPOs, lead to very good adhesion of the coatings to TPO substrates and impart excellent petrol resistance to coatings systems.

Kathrin Lehmann (Degussa/Tego Chemie Service) presented new Gemini surfactants that can perform the balancing act of serving as highly effective anti-foam agents for waterborne coating formulations and simultaneously enhancing wetting of substrates and adhesion of waterborne coatings.

Lasting Chemical Activation

Three speakers proposed direct chemical modification of the substrate surface: Dr. Jürgen Nagel (Institute for Polymer Research in Dresden) reported on research into functionalizing the surface of plastics by means of a reaction inside the injection mold as a way to make the surface more reactive. Rosanna Telesca (Ciba), on the other hand, presented a plasma activation by which substrates can be coated with a layer of photoinitiator molecules during activation that react according to their nature with UV coatings to afford very good adhesion. In a very similar vein, Dr. Pere Castell-Muixi (Technical University of Eindhoven) grafts benzophenone onto PP substrates to provide good adhesion for UV powder coatings. The advantage of all three techniques is that the substrate remains lastingly active, in contrast to the case for pure plasma methods and flame treatment.

3D Plasma Sources

The more physical surface-pretreatment regimes were addressed by Bernd Stedry (Henkel), who presented cleaning methods involving high-pressure water jets; by Dr. Hildegard Sung-Spitzl (Iplas), who demonstrated new plasma sources that are particularly notable for rapid plasma activation of 3D parts; and by Jörn Birkel (Clean-Lasersysteme), who showed that laser evaporation constitutes a sufficiently quick method of activating the substrate's surface.

Simulation Simplifies Process Development

José Gamero (Lactec) reported on highly efficient coating techniques that utilize "pigging" and are conducive to particularly fast, economical color changes. Ulrich Strohbeck (Fraunhofer IPA Stuttgart) demonstrated simulation techniques that can substantially simplify the development of methods for coating plastics. Among other things, given the correct approach, the conductivity of the still liquid coating can be exploited to dissipate electric charges, a fact that permits more effective electrostatic application, even to plastics that act as insulators.

Class A Surfaces With Coated Films

A highly interesting alternative method of coating substrates directly was presented by Dr. Winfried Kreis (BASF Coatings). A thin, chromophoric film is covered with a clearcoat, shaped and UV-cured. Only then is it back-molded with the plastic substrate. The advantage of this method is that Class A high-gloss surfaces can be achieved, and there is no problem with reproducibility or homogeneity of difficult hues, such as brilliant silver or emerald black.

Sol-gel coating systems for plastics were discussed by Dr. Stefan Gödicke (Nano-X). These coatings are notable for their extreme mar resistance. Karl-Heinz Fischer (Dr. Schoch AG) gave an account of coatings on PP that do not require any pre-treatment - however, after his paper, the audience was still trying to work out how this feat can be achieved chemically.

High-Throughput Adhesion Tests

Dr. Radislav Potyrailo (General Electric) reported on his research into the use of combinatorial high-throughput experiments (HTE) to develop new coatings systems featuring improved adhesion. Miniaturized, automated formulation and adhesion tests have been developed that are much, much faster than conventional methods. Many highly promising, new starting formulations have been found in this way.

Finally, three speakers presented new coatings raw materials: Stefan Smeets (Surface Specialties UCB) described efficient binders for UV coatings; Dirk Mestach (Akzo Nobel Resins) demonstrated novel, surfactant-free acrylic dispersions for aqueous formulations; and Frank Kother (BykChemie) showed how waxes may be used efficiently for matting and texturizing plastic coatings.

Plastics Substrates Developing Too Quickly?

A distinctive element of the ECC was again the group discussions on specific expert questions that had been submitted in advance, especially on the subject of coatings adhesion. For example, there was a discussion about how current test methods do not yield any information about the underlying mechanisms of adhesion, with the result that a good or bad performance provides no insight into the reasons for adhesion or non-adhesion.

There are fundamental studies that could provide such information but they suffer from the problem that "almost every year" the automotive sector alone introduces another substrate variant that often requires a complete review of coating systems - this is happening too quickly to enable important issues of industrially relevant substrates to be researched. A possible solution would be to make greater use of HTE, perhaps combined with simulations and followed by exact analyses of selected systems, both good ones and bad ones.

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • pci1022-Kinaltek-Lead-1170.jpg

    A Novel Pigment Production Technology

    Following an extensive R&D program that demonstrated...
    Paint and Coating Pigments
    By: Jawad Haidar and Nitin Soni
  • pci global top 10

    2025 Global Top 10: Top Paint and Coatings Companies

    The following is PCI’s annual ranking of the top 10...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • 2025 pci 25

    2025 PCI 25: Top Paint and Coatings Companies

    PCI's annual ranking of the top 25 North American paint...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

Popular Stories

Akzo, SW, Nippon Logos

AkzoNobel Rejects Cash Offer From Nippon Paint, Sherwin-Williams

BASF SE Logo

BASF Announces Strategic Business Sale

AkzoSWNipponEndTalks

Nippon Paint, Sherwin-Williams End AkzoNobel Pursuit

POB-Point-and-Shoot

PCI Buyers Guide

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

Find Suppliers

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

September 15, 2026

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Automotive Paints and Coatings, 2nd Edition

Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

See More Products
Inside the AI Shift in Coatings - See the article now

Related Articles

  • High-Performance Pigments Program Scheduled in Berlin

    See More
  • Coatings for Plastics Symposium Issues Call for Papers

    See More
  • Coatings For Plastics Symposium Issues Call For Papers

    See More

Related Products

See More Products
  • intelligent.jpg

    Intelligent Coatings for Corrosion Control 1st Edition

  • Kevin-Biller-PC-BOOK.jpg

    Powder Coatings - Foundation for the Novice Formulator (ebook)

  • laser tech.jpg

    Laser Technology: Applications in Adhesion and Related Areas

See More Products
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing