Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!
FT Archives

Eco-Friendly Stripping

July 1, 2008
An eco-friendly chemical stripping solution has allowed Filtech, Inc., a manufacturer/finisher of automotive oil and air filters based in Findlay, OH, to improve rack stripping and powder coating rework.

Racks at Filtech are immersed in an eco-friendly chemical solution at 180 to 200°F and are then rinsed, dried and ready to be placed back on the powder coating line. The entire process takes just 60 to 90 minutes.


Filtech, Inc., a manufacturer/finisher of automotive oil and air filters based in Findlay, OH, uses automated electrostatic powder coating equipment from Nordson Corp. to apply a quality powder coating to its products. Unfortunately, the powder coating also builds up on the racks used to carry parts through the finishing operation.

The company originally cleaned its racks in burn-off ovens, but as production requirements grew and energy costs increased, this process became too labor-, energy- and time-intensive. Filtech investigated allowing the same racks to pass through the powder coating process up to six times and then replacing them with new racks, but this option presented a cost concern. To remain competitive, the company needed to find another way to remove powder coating from its paint line racks and occasional powder coating rework in-house.

Stripping in-house allows racks to be stripped and returned to service the same day, versus three to five days for outsourcing.

An Eco-Friendly Solution

After evaluating a number of different options, Gary Burns, project engineer at Filtech, selected Miles Chemical Solutions based in Rochester Hills, MI, to fabricate custom stripping equipment and provide eco-friendly chemical stripping solutions. Miles Chemical Solutions’ founder, Samuel L. Miles, first patented methods in April 1999 and October 2001 to strip paint and remove coatings from aluminum and galvanized substrates with a soap-based stripper that is 99% free of volatile organic compounds (VOCs). More recently, the company has developed environmentally friendly, low-VOC paint strippers that also save energy by operating at lower temperatures (<205°F/96°C), as well as proprietary technologies and methods to salvage and recycle paint rework, thus avoiding parts disposal.

Burns was impressed with the company’s capabilities. After receiving the initial stripping equipment layouts from Miles Chemical Solutions, Burns provided a few of his own engineering improvements that were incorporated into the Filtech stripping equipment design. The equipment was installed in spring 2008.

The stripping process at Filtech is operated daily on two production shifts. The powder coating racks are allowed to pass through the paint line only twice prior to stripping and cleaning. This restriction maintains a cured powder coating film build of no greater than 5 to 6 mils for optimum chemical stripping index times of 60 to 90 minutes. The racks are immersed in the chemical solution at 180 to 200°F (82 to 93°C) and are then rinsed, dried and ready to be placed back on the powder coating line. The plant uses three sets of parts racks; while one set is in production, the second set of racks is in the stripping solution and the third set is clean and ready to replace coated production racks.

Powder coating rework is subjected to the same process. The technology restores substrate surfaces to like-new condition with the original surface quality, allowing the company to achieve “zero-tolerance” paint quality without having to reprocess sanded and paint-repaired parts.

Filtech’s stripping equipment was customized to meet the needs of the plant.

Improved Stripping

According to Burns, the in-house powder coating rack stripping process presents a number of advantages compared to other stripping methods. Stripping in-house allows the racks to be stripped and returned to service the same day, versus three to five days for outsourcing, and it provides greater control over the quality of the powder coating racks. It minimizes rack replacement and is a more operator-friendly process compared to corrosive or higher-heat methods of paint removal. Additionally the undercutting and lifting action of the stripping chemistry creates powder coating “skins,” which are easier to remove from the stripping solution process tank compared to dissolving chemistries. As a result, the technology has an increased stripping solution bath life for a more cost-effective operation.

For Filtech, the technology has provided the stripping solution the plant needed to optimize production while minimizing its labor and energy costs and reducing its environmental impact.


For more details about Filtech, Inc., call 419.424.9713, e-mail gburns@filtechusa.com or visit www.filtechusa.com. For more information about Miles Chemical Solutions, call 248.765.9946, e-mail sam@mileschemicalsolutions.com or visit www.mileschemicalsolutions.com.

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • pci1022-Kinaltek-Lead-1170.jpg

    A Novel Pigment Production Technology

    Following an extensive R&D program that demonstrated...
    Paint and Coating Pigments
    By: Jawad Haidar and Nitin Soni
  • pci global top 10

    2025 Global Top 10: Top Paint and Coatings Companies

    The following is PCI’s annual ranking of the top 10...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • 2025 pci 25

    2025 PCI 25: Top Paint and Coatings Companies

    PCI's annual ranking of the top 25 North American paint...
    Paint and Coating Market Reports
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

Popular Stories

Akzo, SW, Nippon Logos

AkzoNobel Rejects Cash Offer From Nippon Paint, Sherwin-Williams

BASF SE Logo

BASF Announces Strategic Business Sale

AkzoSWNipponEndTalks

Nippon Paint, Sherwin-Williams End AkzoNobel Pursuit

POB-Point-and-Shoot

PCI Buyers Guide

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

Find Suppliers

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

September 15, 2026

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Automotive Paints and Coatings, 2nd Edition

Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

See More Products
Inside the AI Shift in Coatings - See the article now

Related Articles

  • SUPPLIES: Drum Stripping Kit Offers Enviro-Friendly Alternative - Posted 2/6/08

    See More
  • Rhodia Focuses on Eco-Friendly Paint Additives and Solvents

    See More
  • Innovation Spotlight: Eco-Friendly Corrosion Protection

    See More

Related Products

See More Products
  • Principles and Applications of Emulsion Polymerization

  • Powder Coatings Processing (Virtual Course - 6/25/26)

  • July 25, 2024

See More Products
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing