Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!

Higher-Quality, Consistent Drawdown Charts Improve QC Test Results

By Sherry Walter
August 1, 2006
Quality testing of coatings, inks and raw materials is required to ensure consistent production. Drawdown charts have been used for many years for checking color, gloss, opacity, hiding power, adhesion and many other physical properties that are important to the manufacturer of coatings as well as the end-user.



Figure 1. Click image for larger view.
What happens when you discover that the new shipment of drawdown charts that you are using is different from the previous supply that you had been using? Can changes in the color of the paper stock that was used to produce the drawdown chart affect your results? What about changes in the color of the coated white or black sections of the chart? How can changes in the gloss properties affect your testing?

Any of these physical changes in the drawdown chart can negatively influence your testing results and the reliability of your standards. For example, hiding power or coating opacity is measured by the lightness (L*) differences of the coating on the white and black areas of a drawdown chart. With a new batch of charts two possibilities can happen if the L* of the white and black areas are not kept consistent.



Figure 2. Click image for larger view.
Case 1: If the black has a higher L* value than usual, the difference between black and white is smaller. Less hiding pigments are needed in the paint to make this difference disappear; however when this paint is used on the wall to hide stains, the stains show through. The contractor has to apply a second paint layer, leading to increased material and labor cost.

Case 2: If the black has a lower L* value, the difference between black and white is larger. The QC lab then orders production to add more pigment to make the difference disappear. Pigment is wasted, and the hiding power of the paint does not improve when the paint is applied on the wall.

Inconsistent charts can lead to unnecessary costs, production adjustments and re-testing, only to discover that the problems detected were due to variances in the chart itself and NOT in the product being tested.

To illustrate the magnitude of the problem, consistency tests were conducted on different production lots of a leading brand of drawdown charts as well as our own byko-charts® over a period of 54 months.



Figures 3-4. Click image for larger view.

White Area Tests

Figures 1-3 show the variation of CIE L*a* b* color values for the white-coated portion of the competitive drawdown charts used in the tests. The variance in color values for the white-coated section of the competitive test chart was found to be:

L* (Min. 91.13 to Max. 92.94) = Range 1.51 units

a* (Min. -1.28 to Max. -0.12) = Range 1.16 units

b* (Min. 2.61 to Max 4.93) = Range 2.32 units



Figures 5-6. Click image for larger view.

Black Area Tests

Significantly greater color variance was found for the black sections of the competitive charts tested in this study (Figures 4-6). The variance in color values for the black coated section of the competitive test charts was found to be:

L* (Min. 3.64 to Max. 8.16) = Range 4.52 units

a* (Min. -0.23 to Max. 1.80) = Range 2.03 units

b* (Min. -0.58 to Max. 3.44) = Range 4.02 units

BYK-Gardner goes to great lengths to assure the quality of all the charts before, during and after the productions process. A quality technician is on site testing the charts as lots are being produced. Prior to a lot being released for sale to customers, random samples are collected across the entire chart run and subjected to extensive testing in the BYK-Gardner laboratory.



Figures 7-8. Click image for larger view.

Storage

Drawdown chart storage has also been found to be a serious problem when less than "ideal" storage conditions are used. For instance, in the hot, humid days of summer, boxes of drawdown charts that are stacked in a warehouse or a delivery truck can quickly deteriorate, making them totally unusable. Charts can stick together, causing the coatings to be pulled off when attempts are made to separate the charts.

ASTM D 4946 is a procedure to test for blocking (resistance of surfaces to stick together). BYK-Gardner had an independent laboratory conduct a test on our charts and the competitive drawdown charts using the ASTM D 4926 method. The byko-charts passed the test and the competitive charts failed. To prevent blocking, BYK-Gardner wraps each box of byko-charts with a protective film that guards against humidity in the warehouse and during shipment.

BYK-Gardner has solved all these serious problems with our byko-chart family of charts. Our charts set high standards for the most desirable features in drawdown charts:

  • most consistent color and gloss values in the industry;
  • superior blocking resistance;
  • industry best moisture resistance during storage; and
  • environmentally friendly topcoat.


Figures 9-12. Click image for larger view.
All the familiar drawdown charts are available in the byko-chart family (Figures 7-12).

1. Opacity Charts - comprised of simple combinations of black and white areas with ample space for reflectance measurement to test hiding power.

2. Penopac Charts - Penetration and opacity testing combined in one simple chart.

3. Spreading Rate Charts - Designed for visually comparing hiding power and calculating coating spreading rate.

4. Sag and Leveling Test Charts - Designed for use with anti-sag meters.

5. Display Charts - Bold diagonally striped black patterns visually emphasize variations in opacity.

6. Plain White Charts - Plain white charts with the coating on one side with no text or label on top.

Now you can test your coatings or inks with the greatest degree of reliability in the industry. We also have private label charts available. Customize your charts with your own logo and custom header.

For further information or a sample pack of charts, contact BYK-Gardner USA at 1-800-343-7721.

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Marketing Manager | BYK-Gardner USA, Columbia, MD

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • pci1022-Kinaltek-Lead-1170.jpg

    A Novel Pigment Production Technology

    Following an extensive R&D program that demonstrated...
    Paint and Coating Pigments
    By: Jawad Haidar and Nitin Soni
  • pci global top 10

    2025 Global Top 10: Top Paint and Coatings Companies

    The following is PCI’s annual ranking of the top 10...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • 2025 pci 25

    2025 PCI 25: Top Paint and Coatings Companies

    PCI's annual ranking of the top 25 North American paint...
    Paint and Coating Market Reports
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

Popular Stories

Akzo, SW, Nippon Logos

AkzoNobel Rejects Cash Offer From Nippon Paint, Sherwin-Williams

BASF SE Logo

BASF Announces Strategic Business Sale

AkzoSWNipponEndTalks

Nippon Paint, Sherwin-Williams End AkzoNobel Pursuit

POB-Point-and-Shoot

PCI Buyers Guide

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

Find Suppliers

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

September 15, 2026

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Automotive Paints and Coatings, 2nd Edition

Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

See More Products
Inside the AI Shift in Coatings - See the article now

Related Articles

  • Texture Training Helps Improve QC Analysis

    See More
  • Nalco Weighs in on Dispersant Test Results

    See More
  • A Must to Ensure Consistent Quality

    See More

Related Products

See More Products
  • Powder Coatings Processing (Virtual Course - 6/25/26)

  • corrosion of linings.jpg

    Corrosion of Linings & Coatings: Cathodic and Inhibitor Protection and Corrosion Monitoring

  • durability.jpg

    Increasing the Durability of Paint and Varnish Coatings in Building Products and Construction 1st Edition

See More Products

Events

View AllSubmit An Event
  • April 28, 2026

    Next Gen Dispersion Technology in Paint Production: Driving Higher Quality at Lower Costs

    On Demand Join this webinar to see how manufacturers reduce costs, energy use, raw materials, labor, and floor space while improving quality.
View AllSubmit An Event
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing