Measuring Effect Pigments

Color and appearance are key factors in the purchase of a product. Eye-catching finishes draw the customer's attention to the product and help give the impression of added value. Automotive manufacturers learned this lesson long ago and now use effect pigments (metallic-flake and interference pigments) in many of their coatings.

Coatings that contain effect pigments change appearance as the illuminating and viewing angles change. This phenomenon is called gonioappearance, and the changes in appearance can be very dramatic. While designers love the visual effects achieved by using these effect pigments, the very aspects that make these pigments so visually appealing also make them uniquely difficult to characterize and control. As the development time from concept color to finished product becomes shorter, the challenge to formulate, correct and evaluate gonioapparent pigments grows.

For years, the color of paint has been controlled using spectrophotometers. However, conventional spectrophotometers, using either integrating spheres or 45°/0° illuminating/viewing geometries, cannot measure or characterize samples containing gonioapparent materials. Goniospectrophotometers, which allow a colorist to change both the illuminating and viewing angles, have the capability of measuring effect pigments. While these instruments can completely characterize effect pigments, they are expensive, require a lot of training and are not generally suited to a production environment. During the 1980s, a new tool, the multiangle spectrophotometer, was introduced into commercial coatings applications as a tool for matching, correcting and evaluating coatings containing effect pigments. A multiangle spectrophotometer is an abridged version of a goniospectrophotometer. The first multiangle spectrophotometers had either one illuminating angle with multiple viewing angles, or multiple illuminating angles with one viewing angle. The second generation of multiangle spectrophotometers has multiple illuminating and viewing angles.

Metal-Flake Pigments

Automotive paint was the first industrial coating to use gonioapparent effect pigments. Initially, only metal-flake pigments were used. These pigments achieve their appearance characteristics by behaving like opaque mirrors, which are layered throughout the cured coating film. Formulations containing only metal-flake and conventional pigments vary most noticeably in lightness, as the viewing angle is changed. This change in lightness is called flop or travel, and the greater the lightness change, the more dramatic the visual effect. The most striking visual effects achieved with these pigments occur when the flakes are aligned parallel to the surface of the coating. The larger the flake, and the more consistent its alignment, the greater is the flop.

Researchers have found that the angle of illumination is not critical when measuring colors containing only metal-flake and conventional pigments. This has led to the specification of the "aspecular" angle for measuring coatings containing metal flakes. The aspecular angle is the difference between the viewing angle and the specular (mirror-like) reflection angle of the illuminator. Figure 1 illustrates the aspecular angle concept. The first generation of multiangle spectrophotometers was developed to accommodate this specification. Some of these instruments had a single illuminating angle (45°) and from three to five aspecular viewing angles. Others had from three to five illuminating angles with a single viewing angle (0°).

Two international standards have been adopted for measuring metal-flake pigments. Each includes the specification of aspecular angles for measuring and evaluating these materials. The angles in these standards are referred to as "metallic" angles.

In Germany, the Deutsches Institut für Normung e. V. published DIN 6175-2 Farbtoleranzen für Automobillackierungen - Teil 2: Effektlackierungen (Tolerances for automotive paints - Part 2: Goniochromatic paints). That standard specifies measurements at aspecular angles of 25°, 45°, 75° and 110°.

In the United States, ASTM International published E 2194 Standard Practice for Multiangle Color Measurement of Metal Flake Pigmented Materials. That practice recommends making measurements at aspecular angles of 15°, 45° and 110°, and provides the option for substituting two additional aspecular angles.

The DIN standard even includes a color difference equation with different specifications for manufacturers and users of automotive paints.

Interference Pigments

While conventional pigments produce color by absorbing selected wavelengths of light, metal-flake pigments generally reflect all wavelengths of light. The special visual effect achieved through their use is due to the layering of the pigments throughout the coating. This effect can be measured by changing only the aspecular angle. Since only the aspecular angles are important, a first-generation multiangle spectrophotometer having only one illuminating or viewing angle can adequately capture this effect. In contrast to conventional and metal-flake pigments, interference pigments selectively reflect light as the illuminating and viewing angles are changed. As a result, interference pigments vary most noticeably in hue and chroma. Adding interference pigments to a formula containing metal-flake pigments produces coatings that change not only in lightness, but also in hue and chroma.

The wavelengths of light reflected by the interference pigment depend upon the thickness of the pigment and the distance the light travels through the particle (pathlength). The reflected light is seen at, or very near to, the angle of the specular reflection. The thickness controls the range of hues that can be seen for a given particle. For a given interference pigment, as the illuminating angle increases, the pathlength decreases, and a range of colors is seen (see Figure 2). Two types of mica-based interference pigments have been developed for commercial applications. While the first generation of interference pigments produces subtle changes in the hue of the coating, the latest generation of these materials produces striking hue changes.

Unfortunately, multiangle instruments designed for the measurement of metal-flake coatings cannot properly measure or characterize interference pigments. Since they have only one illuminating angle and one near-aspecular viewing angle, they can only measure the color for single pathlength. Multiple illuminating and viewing angles are required to measure the color at multiple pathlengths and provide the essential information needed by the colorist for evaluating the color of these coatings.

Research done by several pigment suppliers has shown that three illuminating angles (q1 = 25°, 45° and 75°) and two near-aspecular viewing angles for each of the illuminating angles (Y = +15° and Y = -15°) are sufficient for the practical measurement of industrial coatings containing interference pigments. These are referred to as the "interference" angles. Each set of these angles measures a different pathlength of light through the pigment and thus a different color. Ideally, interference pigments are also oriented parallel to the coating's surface. If all of the pigment particles were perfectly aligned, only light reflected at, or very near to, the specular angle would be seen. However, since the ideal is rarely achieved, measurements made at medium and far-aspecular angles are indicative of the flake orientation.

Measuring Coatings Containing Interference Pigments

In order to accurately evaluate a coating containing interference pigments, data about the chromaticity (hue and chroma) of the coating is required.

Figure 3 is an a*,b* chromaticity diagram plotting the measurements made of a second-generation interference pigment. The solid line in Figure 3 connects the six sets of interference angles in the order in which they were measured. The data points move through all four quadrants of the plot as the illuminating and viewing angles change. This confirms the visual perception that the hue of this sample ranges from purple through green. The resulting horseshoe shape of the connected interference angles is a general characteristic of second-generation interference pigments.

The dotted line in Figure 3 connects the four sets of metallic angles specified in the DIN standard. The origin of the dotted line is the interference point having an illuminating angle of 45° and an aspecular viewing angle of +15°. This is one of the aspecular angles allowed in the ASTM standard. Since the interference reflection is only at, or very near to, the specular angle, the metallic angles are measuring flake orientation. For this particular sample, most of the flakes are parallel to the surface, and the metallic measurements spiral in towards the black color of the substrate. Table 1 contains the L*, a* and b* color coordinates of the points plotted in Figure 3. The table shows that the lightness also decreases rapidly as the metallic aspecular angle increases. If a coating containing only metal-flake and conventional pigments was plotted on an a*b* chromaticity diagram, the chromaticities measured at the interference angles would all cluster around the same a*, b* point.

Table 2 contains the L*, a* and b* color coordinates of a purple coating containing 60% aluminum flake. For five of the six interference angles, the coordinates are very close. The measurements at a 25° illuminating angle and a 170° viewing angle includes some gloss from the sample, which decreases the saturation. For the metallic angles, the lightness decreases rapidly as the aspecular angle increases.

Multiangle spectrophotometers are mostly used for quality-control applications, and the evaluations are typically color difference evaluations. However, the spectral data provided can be used as a tool for matching samples containing interference pigments. Figure 4 illustrates the measurement of two samples containing the same interference pigment. One curve shows the measurements made of the pigment manufacturer's color card, and the other curve shows the measurements of an opaque paint drawdown containing only that pigment. The differences between these curves can be used to quantitatively judge how to adjust a formula to match a standard. For this particular set of samples, the vehicle and solvent package are most likely different.

The key to spectral analysis is the type of multiangle spectrophotometer you use. It must provide information from multiple illuminating and multiple viewing angles. Consider, for example, that a customer submits a green sample for a match, which contains an interference pigment. The colorist makes a visual match. When measured on a multiangle spectrophotometer that offers only one illuminating angle and four aspecular viewing angles, the curves shown in Figure 5 are produced. From the curves, it looks like the formula should produce a good match. However, a visual examination of the standard and trial indicate that something is wrong with the formulation and that it can probably not be adjusted to match the standard. When the interference angles are included in the measurement (Figure 6), the reason for the poor visual agreement becomes obvious. The chromaticity diagram curve shapes of the two samples immediately shows that different pigments were used in making the samples. One of the samples contained Pearlgreen and the other sample contained a mixture of Pearlsilver and Pearlgold. With the data produced from multiple illumination and viewing angles, the colorist now has a much more accurate indicator of the pigments needed to match the sample.

Conclusion

Effect pigments will continue to be used in formulating coatings, and their use is expected to grow. Consumers and product designers demand the eye-catching effects that can be obtained with the use of these pigments. Coatings with only metal-flake and conventional pigments can be controlled with instruments having only one illuminating angle and several aspecular angles. However, to control coatings containing interference pigments, a multiangle spectrophotometer offering three illuminating angles with two near-aspecular angles at each of the illuminating angles, is necessary for evaluating and controlling interference pigments.
You must register or login in order to post comments.

Multimedia

Videos

Image Galleries

American Coating Show 2012

The American Coatings Show and Conference, held every two years, took place May 7-10 at the Indiana Convention Center in Indianapolis, IN, in the heart of the Manufacturing Belt, the oldest and largest concentration of industrial companies in the Midwest.

Podcasts

PCI Top 5 - January 12, 2012
PCI's Podcast series on the five most e-mailed/shared articles and stories for the week.

More Podcasts

THE MAGAZINE

PCI Magazine

PCI may 2012 cover

2012 May

Check out PCI's May issue!!

TABLE OF CONTENTS SUBSCRIBE

iPad

Do you own/use an iPad?
If yes, do you use your iPad for business or personal reasons?
Have you purchased a business app within the last 6 months?
See Poll Results Poll Archive

THE PCI STORE

PCI-June-2011-Coversmall.gif
PCI Additives Handbook

Encyclopedia of information on the properties and uses of coatings additives.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

Virtual Brochures

PageCollageClick on the Virtual Brochures page to view multiple categories that list downloadable product literature from leading industry suppliers.

STAY CONNECTED

Facebook Twitter  LinkedIn YouTube