Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!

New Topcoat Formulated with Polyaspartic Binders Sets New Standards in Corrosion Protection

April 1, 2010
The discus-shaped, translucent roof of the BayArena, with a diameter of 217 meters is a new and spectacular showpiece project for the application of Makrolon® high-tech sheeting.



After a complete overhaul, the BayArena, the home of Bundesliga soccer team Bayer 04 Leverkusen, re-opened its gates in time for the start of the new season, and now complies with the very latest international standards. Bayer MaterialScience played a significant role in this. The discus-shaped, translucent roof with a diameter of 217 meters is a new and spectacular showpiece project for the application of Makrolon® high-tech sheeting. To ensure durability, the steel support structure, weighing around 3,000 metric tons, has been provided with a special anti-corrosion coating based on polyaspartic raw materials that has both economic and ecological advantages. Both applications underline Bayer MaterialScience's many years of expertise in these fields and highlight the intensive cooperation with customers along the value chain.

The World's Largest Makrolon Frisbee

With a total area of 28,000 square meters, the roof spans the stadium's entire extended stand area. Its construction is based on the spoked wheel principle. The triple-wall sheets of Makrolon Multi UV 3X/25-25ES white S 146 were supplied by Bayer Sheet Europe GmbH, a subsidiary of Bayer MaterialScience that specializes in the development, production and marketing of high-quality polycarbonate and polyester sheet for a wide variety of applications. Polycarbonate is noted above all for its high break resistance, impact strength, high- and low-temperature resistance, and light weight. "This material is brilliant. I can't imagine anything better for designing a large roof like this without any additional supports," says Hans Dannenberg, who headed the stadium redevelopment project. "What we have here is the world's largest Makrolon Frisbee".

The design and subsequent assembly of the sheets presented a major challenge, because the roof’s circular external contours gradually change to a rectangular shape towards the inside. This means, simply because of the very large area involved, that enormous forces act on the roof. Another handicap was that very little time was available for actually putting up the roof. But Makrolon has two great advantages: its outstanding machinability and the very low weight of the individual plastic sheets. After preliminary assembly, the sheets were hoisted up by cranes to a height of 30 meters, where they were mounted on the unsupported steel cable structure by specially trained industrial climbers.

Makrolon sheets have, in fact, been doing an outstanding job in the BayArena since the 1990s. In the meantime, the product's properties have been further optimized: for example, the light transmission of the sheets is better suited to the requirements of a stadium. While they protect the spectators from too much sunshine, they also allow enough light through to encourage the grass to grow.

Decision makers in the building sector also value the versatility and attractiveness of polycarbonate, as is shown by other large-scale projects that are currently being planned, for example in China. "The models we have demonstrate once again how adaptable polycarbonate sheeting is in use," says Thomas Kastner, head of the semi-finished products segment. Other spectacular stadiums were also projected – for the next European Football Championship in Poland in 2012 and the Football World Cup in Brazil in 2014, for example. Says Kastner: "I am delighted with the continually increasing popularity of polycarbonate and the status it enjoys as the material of choice in modern architecture. We intend to continue expanding  our sheet business, both in horizontal and in vertical applications."

Economical, Ecologically Effective Corrosion Protection

With large structures such as bridges and power plants, a three-coat paint system is normally used to provide the corrosion protection needed to withstand the ravages of wind and weather. To protect the steel girders of the BayArena, however, a different concept was chosen. With the innovative topcoat used here, which is based on polyaspartic binders from Bayer MaterialScience, two coats were sufficient, because a much higher film thickness can be obtained with one application than is possible with conventional topcoats.

"It would never have been possible to keep to the tight schedule for the BayArena without this new topcoat," explains Karl-Heinz Birk, head of the coating shop at Max Bögl Bauservice GmbH & Co. KG, one of the two general contractors responsible for the rebuilding of the BayArena. "Thanks to its rapid drying, we were able to significantly increase the throughput in the workshop compared with the conventional system. Furthermore, we were able to reduce solvent emissions very considerably due to its low VOC content."

Whereas a normal three-coat system takes about 24 hours to apply and dry, the complete application of the new two-coat system takes only six to eight hours. This saves time and money and is also good for the environment. If the topcoat is based on raw materials from the Desmophen® NH and Desmodur® N ranges, it will contain some 40 percent less VOCs than a conventional three-coat system. An ultra-high-solids coating such as this more than meets the present statutory requirements. "A further bonus with this topcoat is its excellent adhesion to metal. I see enormous potential for one-coat application directly to such surfaces," says Dr. Markus Mechtel, a corrosion protection expert at Bayer MaterialScience.

For more information, visit http://www.bayermaterialscience.com and www.bayersheeteurope.com.

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • pci1022-Kinaltek-Lead-1170.jpg

    A Novel Pigment Production Technology

    Following an extensive R&D program that demonstrated...
    Paint and Coating Pigments
    By: Jawad Haidar and Nitin Soni
  • pci global top 10

    2025 Global Top 10: Top Paint and Coatings Companies

    The following is PCI’s annual ranking of the top 10...
    Paint and Coating Market Reports
    By: Courtney Bassett
  • 2025 pci 25

    2025 PCI 25: Top Paint and Coatings Companies

    PCI's annual ranking of the top 25 North American paint...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

Popular Stories

Akzo, SW, Nippon Logos

AkzoNobel Rejects Cash Offer From Nippon Paint, Sherwin-Williams

BASF SE Logo

BASF Announces Strategic Business Sale

AkzoSWNipponEndTalks

Nippon Paint, Sherwin-Williams End AkzoNobel Pursuit

POB-Point-and-Shoot

PCI Buyers Guide

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

Find Suppliers

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

September 15, 2026

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Automotive Paints and Coatings, 2nd Edition

Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

See More Products
Inside the AI Shift in Coatings - See the article now

Related Articles

  • Ultra-Short Pulsed Laser Deposition Sets New Standards for Diamond-Like Coatings

    See More
  • Hempel Avantguard 750 Pro.jpg

    New Avantguard 750 Pro Sets Standard for Corrosion Protection

    See More
  • Corrosion Protection with New Cost-Effective Coating

    See More

Related Products

See More Products
  • corrosion of linings.jpg

    Corrosion of Linings & Coatings: Cathodic and Inhibitor Protection and Corrosion Monitoring

  • pci march 2020

    PCI March 2020 Issue

  • corrosion.jpg

    Corrosion Control Through Organic Coatings 2nd Edition

See More Products
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing