Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!
Breaking News

PPG Reports Strong Second-Quarter Results

July 25, 2010
PPG Industries has reported second-quarter sales of $3.5 billion, an increase of 11 percent versus the prior year’s second quarter. Second-quarter reported net income was $272 million, or $1.63 per share.

PITTSBURGH – PPG Industries has reported second-quarter sales of $3.5 billion, an increase of 11 percent versus the prior year’s second quarter. Second-quarter reported net income was $272 million, or $1.63 per share. Second-quarter 2009 sales were $3.1 billion, and reported net income was $146 million, or 89 cents per share.

“PPG’s strong results this quarter benefited largely from a 10-percent increase in volumes,” said Charles E. Bunch, PPG Chairman and Chief Executive Officer. “The breadth of geographies and end-use markets that we serve is enabling us to leverage continuing positive momentum in global industrial demand. The performance of our portfolio is being elevated by this higher industrial activity and strong demand across the Asia-Pacific and Latin America regions. This is more than offsetting weak construction markets in North America and Europe,” he said.

“Our earnings this quarter were aided by an improved sales mix from some of our top-performing businesses, such as aerospace, auto refinish and our optical and specialty materials segment,” Bunch said. He added that commodity chemicals segment earnings have rebounded significantly versus the first quarter, and that the company’s Glass segment benefited from substantially improved performance in the fiberglass business.

“Our financial performance this quarter, despite demand levels that are more than 10 percent below 2008 pre-recession levels, clearly demonstrates that our global portfolio and our efforts to restructure our businesses to reduce structural costs have positioned PPG to capitalize on what we anticipate to be a continued, gradual, global economic recovery,” Bunch said. “We are beginning to utilize our strong balance sheet to accelerate growth and, in fact, are in the process of reviewing several potential small- to mid-size acquisitions.” He also stated that PPG had repurchased 1.6 million shares of stock during the quarter, and that the company has more than 4.5 million shares remaining under its existing share repurchase authorizations.

Performance Coatings segment sales in the second quarter 2010 increased $45 million, or 4 percent, versus last year’s second quarter, as a result of higher selling prices and favorable currency conversion. Volumes were flat, with modest declines in the North American architectural coatings business, offset by solid growth in automotive refinish and aerospace, two of PPG’s top-performing businesses, along with continued growth in the Asia-Pacific region. Segment earnings grew $32 million, or 20 percent, to a new quarterly record of $190 million.

Industrial Coatings segment sales for the quarter rose $198 million, or 27 percent, due to substantial volume growth of more than 25 percent, including higher year-over-year volumes in all businesses and in all regions. Segment earnings for the quarter were $112 million, an increase of $84 million from the prior year’s second quarter.

Sales for the Architectural Coatings – Europe, Middle East and Africa (EMEA) segment decreased $27 million, or 5 percent, due primarily to mid-single-digit percentage volume declines. The negative impact of currency conversion was offset by pricing gains and the impact of several small acquisitions. Segment earnings declined $5 million to $50 million, with about one half of the decline associated with currency conversion.

Optical and Specialty Materials segment sales for the quarter increased $46 million, or 18 percent, as a result of double-digit percentage volume growth in both businesses. Segment earnings improved $25 million to $86 million, establishing a quarterly record as a result of the higher sales volumes and a lower cost structure, countered slightly by increased advertising costs to support the sales growth.

Commodity Chemicals segment sales for the quarter increased $41 million, or 13 percent, due to increased volumes that were slightly offset by lower year-over-year selling prices. Segment earnings increased $11 million due to improved volumes and lower manufacturing costs, partially offset by lower prices. Results improved significantly over the first quarter 2010, with earnings up $50 million during the quarter on higher volumes, improving pricing and lower natural gas costs.

Glass segment sales increased $40 million, or 19 percent, compared with the prior year as a result of improved fiberglass volumes. Segment income was $16 million, an improvement of $23 million.

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • pci1022-Kinaltek-Lead-1170.jpg

    A Novel Pigment Production Technology

    Following an extensive R&D program that demonstrated...
    Paint and Coating Pigments
    By: Jawad Haidar and Nitin Soni
  • pci global top 10

    2025 Global Top 10: Top Paint and Coatings Companies

    The following is PCI’s annual ranking of the top 10...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • 2025 pci 25

    2025 PCI 25: Top Paint and Coatings Companies

    PCI's annual ranking of the top 25 North American paint...
    Paint and Coating Market Reports
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

Popular Stories

Akzo, SW, Nippon Logos

AkzoNobel Rejects Cash Offer From Nippon Paint, Sherwin-Williams

BASF SE Logo

BASF Announces Strategic Business Sale

AkzoSWNipponEndTalks

Nippon Paint, Sherwin-Williams End AkzoNobel Pursuit

POB-Point-and-Shoot

PCI Buyers Guide

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

Find Suppliers

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

September 15, 2026

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Automotive Paints and Coatings, 2nd Edition

Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

See More Products
Inside the AI Shift in Coatings - See the article now

Related Articles

  • DuPont Delivers Strong Second-Quarter Results

    See More
  • PPG Extends Partnership with the National Hockey League

    PPG Reports Record Second Quarter Financial Results

    See More
  • Market Reports 2.jpg

    PPG Reports Strong Performance and Strategic Growth in Q3 2024

    See More

Related Products

See More Products
  • Automotive Paints and Coatings, 2nd Edition

  • organic coatings.jpg

    Organic Coatings: Science and Technology, 4th Edition

  • marketsandmarketslogo.jpg

    Protective Coatings Market by Resin Type...

See More Products
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing