Silicone-Based Coating Improves Peel and Tear Strength of Coated Fabrics

SOMERSET, NJ - NEI Corp., a provider of nanoscale materials, announced the demonstration of a novel silicone-based coating in prototype airbags. Commercially available coating formulations were modified with the addition of highly dispersed, functionalized nanoscale additives. Upon application and curing of the coating with the use of conventional processing techniques, these nanoscale additives form the necessary chemical bonds to become an integral part of the silicone network. Subsequent material characterization demonstrated improvements in mechanical, thermal and barrier properties, which enable high-performance coated fabrics to be engineered with reduced areal density, thereby allowing for significant reductions in system mass and volume.
 
The relevant mechanical properties of commercial silicone coatings, as well as those of the resulting coated fabrics, were substantially improved with the addition of small amounts of engineered nanostructured additives. Successful pilot scale up was achieved, culminating in the fabrication of prototype airbags that exhibited enhanced gas retention. The NASA-sponsored program was carried out in collaboration with ILC Dover, which is a leader in design and manufacturing of engineered soft goods, products that are flexible by nature.
 
High-performance coated fabrics of various types have already been used by NASA in a number of applications, including space suits and impact-attenuating airbag systems. The demand for such materials is expected to grow as research and development continues in the areas of inflatable habitats, sunshields, aerodynamic decelerators and other deployable space structures (e.g., antennas, trusses, solar arrays). Commercial applications for silicone-based nanocomposite coatings are numerous and varied. Inflatables, such as those used in safety restraint systems, can benefit from improvements in mechanical, thermal and barrier properties. Other applications that employ coated fabrics, such as hot-air balloons, cold-air inflatables, boat sails, paragliders and parachutes, also stand to benefit from the potential for greater durability with reduced weight and gas permeability.
 
The program began with the development of novel additives intended to alter the mechanical and physical properties of conventional two-part silicones, followed by a demonstration of the benefits when applied to different fabrics, such as woven fiberglass and VECTRAN®. The nanoadditive synthesis was then scaled up to prepare large batches of coating formulation that enabled production of coated fabrics at pilot scale. Test articles were manufactured in the form of 18” spherical prototype airbags. Leakage testing conducted at ILC Dover concluded that the nanocomposite-coated test articles exhibited a gas retention capability superior to that of the control airbags.
 
“The success of this project can be traced to our core competency in synthesizing and functionalizing nanoscale materials targeted at specific applications,” said Kenneth Eberts, Senior Product Development Engineer at NEI.
 
NEI welcomes the opportunity to partner with end users of silicone coatings to tailor the properties to the specific application needs. NEI will create a custom solution that meets the requirements and will work with the customer from initial R&D all the way through large-scale manufacturing.
You must register or login in order to post comments.

Multimedia

Videos

Image Galleries

American Coating Show 2012

The American Coatings Show and Conference, held every two years, took place May 7-10 at the Indiana Convention Center in Indianapolis, IN, in the heart of the Manufacturing Belt, the oldest and largest concentration of industrial companies in the Midwest.

Podcasts

PCI Top 5 - January 12, 2012
PCI's Podcast series on the five most e-mailed/shared articles and stories for the week.

More Podcasts

THE MAGAZINE

PCI Magazine

PCI may 2012 cover

2012 May

Check out PCI's May issue!!

TABLE OF CONTENTS SUBSCRIBE

iPad

Do you own/use an iPad?
If yes, do you use your iPad for business or personal reasons?
Have you purchased a business app within the last 6 months?
See Poll Results Poll Archive

THE PCI STORE

PCI-June-2011-Coversmall.gif
PCI Additives Handbook

Encyclopedia of information on the properties and uses of coatings additives.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

Virtual Brochures

PageCollageClick on the Virtual Brochures page to view multiple categories that list downloadable product literature from leading industry suppliers.

STAY CONNECTED

Facebook Twitter  LinkedIn YouTube