Soy-Based Wood Stain Takes Environmental Approach to Preserve Wood and Concrete

Finding a staining agent worthy of handling industrial projects can be a daunting task. If you avoid selecting a quality wood stain, you may be setting yourself up for a host of problems. New Century Coatings (NCC), through funding from the soybean checkoff, is researching a solution to most staining dilemmas. The manufacturer has developed AgriStain, an environmentally friendly, soy methyl ester wood and concrete stain that increases the quality of stained products through enhanced penetration and colorization.

Many coating agents simply glaze the top layer of wood and wear away over a brief period of time. According to NCC President Tom Rauls, "AgriStain penetrates the growth cells of the wood, which adds two important features: preservation and colorization. Penetration into soft woods has been observed in multiple growth rings."

"Once the growth ring is saturated with the soy-based solvent, it continues to spread throughout the wood, regardless of the season," says Rauls. "The soybean base in AgriStain aids in actually tricking the wood into believing that summer never ends, which, in effect, causes the continual spreading and sealing of the stain in the product year-round."

Rauls notes that the final result is "a wood product that displays a reduction in splintering, contains a softer texture, expands the life of the wood, shows signs of resistance to mildew and a reduction in discoloration."



Test sites in four areas of the country were started last year. Decks in Florida, Georgia, Michigan and Arizona were each stained and treated with AgriStain to see how the product withstands different weather conditions. While these tests are still being carried out, no technical information is being released. Results are expected to be available for public release within the next six months. So far preliminary results are favorable.

"The decks have held the stain amazingly well," said Rauls. "We check in on the test sites every few months and most look like they were just stained. There is very little discoloration or fading."

In addition to wood staining, AgriStain also effectively stains concrete and cement siding. "AgriStain takes the same approach in staining brick walls, cement buildings and concrete floors as it does with wood," says Rauls. "It's fairly common that painted fiber cement hides the wood pattern; however, when penetrated with AgriStain, fiber cement structures exhibit the look of real wood."

AgriStain can be used to create designs on concrete floors, revitalize brick buildings, colorize concrete landscapes and pool ornaments as well as artistically stain porous stone. It is easily applicable with conventional methods such as paint rollers, brushes, pump sprayers and airless spray or HVLP spray guns.



Rauls states that AgriStain has proved to be superior to conventional stain counterparts in terms of lapping, drip mark repair and dry time. Significant time should pass between applying coats. Wiping the surface and then reapplying AgriStain can repair the wood stain. Research is currently under way regarding a biobased topcoat for stain projects. Until the evaluation is complete and a bio-based topcoat enters the market, Rauls suggests using a waterborne acrylic or acrylic-urethane as a topcoat.

According to New Century Coatings, AgriStain goes beyond what conventional coating agents do for wood products. Besides being odorless and nonflammable, biodegradable, containing no irritants and providing easy cleanup, AgriStain contains low VOCs, making it user friendly during application and providing a safe working environment.

For more information on AgriStain, contact New Century Coatings at 602/625.8925 or e-mail ncc@cox.net.

To learn more about soy-based products, visit the United Soybean Board at www.unitedsoybean.org/newuses.

You must register or login in order to post comments.

Multimedia

Videos

Image Galleries

Podcasts

PCI Top 5 - January 12, 2012
PCI's Podcast series on the five most e-mailed/shared articles and stories for the week.

More Podcasts

THE MAGAZINE

PCI Magazine

February 2012 cover

2012 February

PCI's new issue is now available. Check it out!

TABLE OF CONTENTS SUBSCRIBE

Coating Technology

What resources do you refer to when learning about coatings technology?
See Poll Results Poll Archive

THE PCI STORE

Power Coatings
CD Verison: Powder Coatings - Foundation for the Novice Formulator by Kevin Biller for $29.95 plus shipping
ON CD - Powder Coatings have been the fastest growing finishing technology for the past 30 years. In spite of this tremendous growth and the technology advances that come with it, very few technical tools have been provided for the formulator.
More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

Virtual Brochures

PageCollageClick to the Virtual Brochures page to view multiple catagories that list downloadable product literature from leading industry suppliers.

STAY CONNECTED

Facebook Twitter  LinkedIn