Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!

Soy Ink Research Promises New Printing Applications

May 31, 2002
Soybean oil-based printing inks have come a long way since being introduced more than a decade ago by the newspaper industry. Soy ink's U.S. market share has quadrupled, from less than 5% in 1989 to 25% today.

With continued support from the soybean checkoff and the United Soybean Board, several soy ink research projects under way promise new printing applications targeted at a variety of end users. Once commercialized, these new applications promise to revolutionize the printing industry for another decade.

Ballpoint Pens

Researchers at Southwest Texas State University's Institute for Environmental and Industrial Science Coatings Center are studying ways to use the "green" products found in soybean oil for ballpoint pen ink formulations. Studies indicate that incorporation of soybean oil phosphate ester polyol into water- and solventborne inks could replace gel ink in inexpensive ballpoint pens.

Researchers indicate that the soy products are economical replacements for petroleum inks, and could lower production costs by 20-50% and maintain comparable quality. Collaborators have transfered the technology to an industry partner for commercial testing and application in mid-March.

Toner Cartridges

A soy-based toner for use in office copiers and laser printers is under development by Battelle, the world's largest independent science and technology institute headquartered in Columbus, OH. Researchers anticipate that the "tofu toner" will be easier to de-ink during the paper recycling process, resulting in better fiber recovery and a cleaner, brighter pulp. Less energy is required for de-inking, which could also result in lower paper prices.

Several soy-based toner compositions have been formulated and tested in a commercial copier with good copy quality results. Work is in progress to further improve copy quality, conduct extensive de-inking studies, make patent filings and perform field tests by potential industry partners prior to commercialization in 3-5 years.

UV Inks

Lehigh University researchers in Bethlehem, PA, are evaluating the use of soybean oil in UV-curable printing inks. Research indicates that treated soybean oil can replace at least 25% of the most commonly used acrylates in UV-curable lithographic printing inks.

Researchers have confirmed that with up to 20% soybean oil, the ink's printability and curability are maintained and even improved. Replacing a portion of the more expensive acrylate oligomer resins would also decrease the amount of VOCs released during curing. Users would realize enhanced pigment wetting, decreased odor, favorable paper-recycling properties and improved biodegradability of printed products. Radcure Division of USB Chemical Corp. is preparing the product for commercialization, which is expected to be made available to major suppliers soon.

Textile Printing

Soybean alkyds may become the next binder in the pigment printing technique employed in textile printing. Kansas State University researchers have discovered that soy alkyd resins are an environmentally friendly alternative to petroleum-produced acrylic binders. Soy alkyds produce bright, crisp prints on fabric with depth of shade values similar to acrylic binder. Researchers are working with BASF and hope to commercialize the product for applications in the apparel, home furnishings and industrial markets.

Fast-Drying Oil

Iowa State University scientists are refining conjugated soybean oil to determine its potential as a fast-drying oil. With a drying speed between the popular linseed and tung oils, conjugated soybean oil could replace the more expensive, imported drying oils and be used in printing inks and surface coatings. Conjugated oil has a low odor, and also appears to produce a harder ink film. Researchers are now looking at ways to optimize the process, and have involved a number of industrial partners, including Flint Ink, in defining the market for this promising product.

Baby Prints

Newborn baby feet may be stamped using soy ink kits someday soon, replacing the traditional petroleum-based ink kits. Dr. Sevim Erhan, leader of the oil chemical research unit at the USDA's National Center for Agricultural Utilization Research in Peoria, IL, has developed an ink formulation for stamping baby footprints onto birth certificates. Petroleum-based mineral oil and resin are replaced with soybean oil-based products, except for the pigment where a food-grade black is being tested to replace carbon black, making cleanup much easier with just soap and water. Erhan is working with Hollister Inc., which market ink kits to hospitals.

The United Soybean Board is composed of 62 U.S. soybean farmers appointed by the Secretary of Agriculture to invest soybean checkoff funds. The soybean checkoff is a farmer-supported marketing and research fund collected on each bushel of U.S. soybeans sold. USB invests these funds on behalf of the 600,000 U.S. soybean farmers in activities specifically designed to increase the global utilization of U.S. soybeans and to reduce production costs. Checkoff-funded investment areas include human and animal health and nutrition, research and development of new uses, and research to improve soybean composition and production efficiencies.

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • pci1022-Kinaltek-Lead-1170.jpg

    A Novel Pigment Production Technology

    Following an extensive R&D program that demonstrated...
    Paint and Coating Pigments
    By: Jawad Haidar and Nitin Soni
  • pci global top 10

    2025 Global Top 10: Top Paint and Coatings Companies

    The following is PCI’s annual ranking of the top 10...
    Paint and Coating Market Reports
    By: Courtney Bassett
  • 2025 pci 25

    2025 PCI 25: Top Paint and Coatings Companies

    PCI's annual ranking of the top 25 North American paint...
    Paint and Coating Market Reports
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

Popular Stories

Akzo, SW, Nippon Logos

AkzoNobel Rejects Cash Offer From Nippon Paint, Sherwin-Williams

BASF SE Logo

BASF Announces Strategic Business Sale

AkzoSWNipponEndTalks

Nippon Paint, Sherwin-Williams End AkzoNobel Pursuit

POB-Point-and-Shoot

PCI Buyers Guide

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

Find Suppliers

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

September 15, 2026

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Automotive Paints and Coatings, 2nd Edition

Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

See More Products
Inside the AI Shift in Coatings - See the article now

Related Articles

  • NDSU Bio-Research Promises Game-Changing Technology

    See More
  • NDSU Bio-Research Promises Game-Changing Technology

    See More
  • SWeNT Introduces New Printing Ink Technology

    See More

Related Products

See More Products
  • polymer coatings.jpg

    Polymer Coatings: Technologies and Applications

  • thin film.jpg

    Thin Film Coatings Properties, Deposition, and Applications

  • smart coatings.jpg

    Smart Coatings Fundamentals, Developments, and Applications

See More Products

Related Directories

  • Orion Technical Service Applications Lab

×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing