Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!

The Way We Color Our World

June 1, 2006


Is it film or is it paint? This is the question increasingly being asked in automotive, heavy truck, marine and other markets. Every major automotive OEM has major initiatives to identify, develop and use alternatives to paint. This is all good news for Soliant LLC, a global leader in exterior durable films. Soliant estimates that over 40 million exterior automotive components have been surfaced with dry paint film in the past five years, and expects to see explosive growth in the next three to five years. Applications will range from small trim components to fascias to roofing modules or body panels.



2006 Buick Lucerne. Soliant paint film rocker panels supplied by Durakon Industries.

A Change of Perspective - Paint Film Use Grows

Paint Film History
Paint films appeared in the market for the first time in a significant way in the late 1980s. These films were laminated to aluminum and stainless steel coil and then roll formed or stamped. The films proved to be very durable, and have shown excellent durability in exterior environments. The use of films began to move toward plastic in the late 1990s as more metal parts were converted to plastic.

Automotive OEMs Push for Films
The Japanese OEMs were the first to implement films in a large way on plastic beginning in the late '90s. The growth of the product was limited initially by the lack of infrastructure for using the film in part-manufacturing operations. Initially, there were only a small number of companies who possessed the thermoforming or other processing know-how to use films effectively. However, as the major OEMs placed a higher emphasis on paint alternatives, the infrastructure began to develop and has grown substantially over the past 24 months. As this infrastructure came on line, the use of film and number of applications exploded.



2006 Acura TL. Soliant paint film rocker panels supplied by The Green Tokai Company.

Good for More Than Automotive
The film products offered today are changing the way we think about decorative finishes, and not just from the automotive industry. Films are being incorporated into recreation vehicles such as personal watercraft or ATVs. Mobile phones and other handheld consumer electronics also are using films. The film technology offers the various industries flexibility, efficiency and economy. In addition, the environment benefits substantially because of reduced volatile organic compounds, reduced energy consumption and increased use of recycling when compared to traditional paint methods.



Great for the Environment
The positive environmental impact of paint film versus paint has been well documented. Independent studies show that paint film is 10 times more effective in reducing VOC emissions compared to a state-of-the-art paint system. The Soliant coating lines are designed for 100% capture of ALL fumes, and are far more effective and efficient than a paint system. As environmental regulations become more stringent, the advantages that films offer will continue to grow. Each of the major automotive OEMs is pushing their supply base to eliminate/reduce VOCs from their processes. Automotive OEMs already using the film technology includes Acura, Audi, Chrysler, Ford, GM, Honda, Mercedes, Saab, Toyota and Volvo.



2006 GMC Envoy Denali. Fascia courtesy of Meridian Automotive Systems.

Film Manufacturing

Film manufacture has some similarities with paint manufacture but has some important differences. The manufacturing process begins much the same way as paint; formulating the clear and color compounds. The color compounds used for film manufacture use the same pigments, metal flakes, etc., as paint. However, this is where the similarities end.

First, films are created as a two-dimensional product, which means that the chemistries used for film manufacture must have a thermoplastic nature until the film is formed into the three-dimensional shape during application. This explains why you can't simply use current paint chemistries to make a film.

Second, films are typically created in reverse of paint constructions. In a painting operation, a primer is typically applied first, followed by the color coat and clear coat. These may be applied wet-on-wet or in separate passes. Films start with the clear being cast on a PET carrier. The PET is heat stabilized so that it can convey the coating into an oven and dried. One advantage of this type of process is that the thickness of the coating can be very precisely controlled AND the coating mix can have a substantially higher solids level than paint. High solids reduce the VOC content from the outset and the confined space of a film dryer allows for more efficient capture of airborne VOCs. Just as in the case of painting, the clear and color layers can be coated wet-on-wet or in separate passes. After the clear and color coating, the appropriate adhesive or "primer" is applied to the back of the color coat. This structure can then be laminated to a variety of substrates including TPO, ABS, PC, PC/ABS, etc.



Figure 1 - 2. Click image for larger view.

Film Advantages

Cost - Several studies have highlighted the actual cost savings associated with the use of film when looking at the system cost to produce decorated parts. These studies show that film can have savings of 15-35% depending on the part design. These savings come from improved yields, reduced energy consumption, reduced inventory and increased flexibility.

Performance - Films have been used since the late 1980s in a variety of exterior applications. These provide a reliable database of experience and performance in very challenging environments. Even after 15-20 years of use, the product still looks good and, in many cases, better than the paint surrounding it.

The thermoplastic nature of paint films and the adhesive or primer used turns out to offer big advantages; primarily it provides a very strong bond to the substrate being used. For example, film has improved chip resistance because of the tie layer and the fact that the film is thermoplastic.

The graph in Figure 1 shows the results of gravelometer testing. The scale is 0 to 10, with 10 being the best. As shown, the paint film consistently outperformed paint in gravelometer testing and it does not flake as paint does, which is why OEMs have replaced paint with paint film on cladding, rocker panels, etc. The number of pints in the Figure refers to the number of pints of gravel thrown at a painted sample; the graph shows that even under tremendous impact the paint film is more resistant. The gravelometer test used was GM9508P; Figure 2 shows the samples after testing.

Environment - The precise nature of the coating, the high solids composition and the dryer efficiency lead to dramatic VOC reductions in film manufacture versus painting. Film manufacture uses technology that has been developed for precision coatings in a variety of industries. The thickness can be very precisely controlled. The color solution (and clear for that matter) can be coated at very high viscosities and solids. This reduces the amount of solvents needed and, as a direct result, the amount of VOCs that are generated in the process. Further, no aerosol has to be generated to apply the paint. The color solution is "extruded" onto the carrier and conveyed into the drying ovens.

Just to provide a frame of reference, let's look at what these advantages mean to the environment. According to Gordon C. Miller, MSPH, C.I.H., C.H.M.M, Q.E.P., who presented a study on "Environmental Sustainability & Recycling in Action" at this year's annual GPEC (SPE's Global Plastics Environmental Conference) in Atlanta, "With the film process, the VOC emissions to the environment are reduced by 90-98%!" Just as a frame of reference, this would mean that if film were used on just five million cars per year, the VOC reduction would be the equivalent of eliminating the current emissions of Charlotte, Atlanta and several other similar-sized cities.



Manufacturing process overview. Click image for larger view.

Energy - The high-solids, high-viscosity nature of the paint film liquids reduces the quantity of solvents that must be removed in the drying process. Further, the film manufacture offers another advantage versus spray painting. The film can be applied and dried in a very confined space, further reducing the amount of air that is drawn into the process. The reduced air content reduces the amount of supplemental natural gas needed to incinerate the VOCs. Since the film is post applied, the film can be processed at much higher temperatures and dried more rapidly and effectively.

The energy savings also are significant. Some studies have suggested that the use of film can save the equivalent of several million gallons of gasoline annually. These savings are becoming more significant as we see escalating costs of natural gas and electricity.

Recycle - Film provides the ability to recycle the entire product back into the system. Since the film is thermoplastic in nature, the film can be recycled with extruded sheet or injection molding resins without harm. Soliant's films are designed for use with less expensive olefin resins that are recyclable. Again, the ability to recycle contributes to the cost savings from film use.



Current Applications

Current automotive market applications include rocker panels, body side moldings, fascias, roofstrips, grilles, pillars, IP trims rings and various bezels. Soliant typically supplies the entire color palettes including tint coats, pearlescents and metallics. These color matches have the same criteria as paint.

Many of the current applications were developed to take advantage of the performance advantages of films, particularly resistance to chipping on impact, as highlighted earlier. Honda and Toyota were the first to recognize the potential benefits of film on TPO rocker panels, with parts being in production since 1998. GM has also incorporated film into several rocker panel and stone shield designs to improve performance or avoid costly urethane paint protection films.

Paint films manufactured by Soliant can be easily integrated in customers' manufacturing processes such as injection and compression molding, thermoforming and extrusion. This integration makes it possible to use the same paint film on multiple applications on a single vehicle. Doing this improves the economic benefit of film and ensures color consistency on the range of parts used. For example, Toyota uses paint film on three different parts on the current Avalon. Film is used to manufacture both the rocker panel and body side moldings using an insert/injection molding process. The roofstrip also incorporates paintfilm in the extrusion of an olefin-based substrate. Three different parts, one film.

As paint film has become more cost effective over time, it has increasingly competed against paint in larger and more price-sensitive applications such as fascia and other body panels. Another major advantage is the avoidance of the large capital outlay for automotive paint facilities and their rising costs of operation, particularly due to ever-tighter environmental regulations and increasing energy costs.



The Next Generation

Soliant is now introducing the next generation of paint film to the industry that offers improved scratch and mar properties as well as improved gloss and distinctness of image of the finish. The products further reduce the system manufacturing cost and are also being improved to widen the processing window. These combined improvements are expected to open the door for larger applications in fascias and body panels.

Films are also being developed to serve as the decorative "skins" for large composite body panels like roof modules, fenders, lift gates, etc. These skins can be used with a variety of glass-reinforced composites that offer the strength and stiffness of steel, but the weight and energy transparency of plastics. For example, using composites in roof modules saves weight and allows the manufacturer to incorporate satellite radio and GPS antennae into the module itself, without having external systems. And the film "skins" solve the traditional issues of painting a glass-filled material.

The painting of structural composites, particularly those incorporating glass fibers, presents several challenges. The use of film eliminates the issues with painting glass-filled materials and provides a way to provide body color on the part.

Some production with these systems is already happening in Europe, and is expected to expand quickly as the technology is further validated.

So the next time you are looking at a vehicle, boat or shaver, see if you can tell the difference. You might like what you see.

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • pci1022-Kinaltek-Lead-1170.jpg

    A Novel Pigment Production Technology

    Following an extensive R&D program that demonstrated...
    Paint and Coating Pigments
    By: Jawad Haidar and Nitin Soni
  • pci global top 10

    2025 Global Top 10: Top Paint and Coatings Companies

    The following is PCI’s annual ranking of the top 10...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • 2025 pci 25

    2025 PCI 25: Top Paint and Coatings Companies

    PCI's annual ranking of the top 25 North American paint...
    Paint and Coating Market Reports
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

Popular Stories

Akzo, SW, Nippon Logos

AkzoNobel Rejects Cash Offer From Nippon Paint, Sherwin-Williams

BASF SE Logo

BASF Announces Strategic Business Sale

AkzoSWNipponEndTalks

Nippon Paint, Sherwin-Williams End AkzoNobel Pursuit

POB-Point-and-Shoot

PCI Buyers Guide

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

Find Suppliers

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

September 15, 2026

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Automotive Paints and Coatings, 2nd Edition

Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

See More Products
Inside the AI Shift in Coatings - See the article now

Related Articles

  • Paints of Our Lives: Improving the Way We Live

    Paints of Our Lives: Improving the Way We Live

    See More
  • Ford and BASF Coatings Share a Vision of the Future in the "Way Forward" Initiative

    See More
  • Researcher analyzing data on computer monitor.

    Paving the Way for Digital Innovation in the Paint and Coatings Industry

    See More

Related Products

See More Products
  • pci may 2020

    PCI May 2020 Issue

  • durability.jpg

    Increasing the Durability of Paint and Varnish Coatings in Building Products and Construction 1st Edition

  • Kevin-Biller-PC-BOOK.jpg

    Powder Coatings - Foundation for the Novice Formulator (ebook)

See More Products

Related Directories

  • American Colors Inc.

    American Colors, Inc. is a customer-focused manufacturer of premium liquid pigment systems and specialty chemicals catering to a diverse range of applications, such as paints, coatings, adhesives, composites, films, landscape and agriculture. Our team of experienced professionals is well equipped with premium processing equipment and state-of-the-art laboratory instruments, ensuring that our products are of the highest quality. We take pride in meeting the unique needs of our customers through product development, toll manufacturing, and private labeling and packaging.
  • American Colors Inc.

    American Colors, Inc. is a customer-focused manufacturer of high-quality liquid pigment systems and specialty chemicals supplied to diverse applications that include paints, coatings, adhesives, composites, films, landscape and agriculture. American Colors utilizes experienced professionals, premium processing equipment, and state-of-the-art laboratory instruments. We are committed to meeting the needs of our customers through product development, toll manufacturing, and private labeling and packaging.
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing