Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!

New Generation of Silica-Encapsulated, Ultramarine Blue High-Performance Pigments for Coatings

By Alex Capuz, Xavier Llovens
January 1, 2009


There are several possible definitions of High-Performance Pigments (HPPs) but all of them go in the same direction. A high-performance pigment is one that:1

• demonstrates high-performance properties in its intended end use;

• commands a premium price based on value-in-use and that has not yet been copied by generic producers; and

• is the right pigment for a specific use with well-defined quality criteria at optimized cost.

The superior performance of such pigments is generally related to a combination of as many key attributes/benefits as possible, e.g., uniqueness of color, ease of dispersion, durability, weather fastness, chemical resistance, processing improvements, thermal resistance and resistance to migration.

Ultramarine Blues - High-Performance Pigments?

Historically, Ultramarine Blue (PB 29) has not been considered a high-performance pigment for coatings. It is however a pigment that shows outstanding technical characteristics that could make it very appealing for paint producers in the 21st century. The most important one is the uniqueness of its reddish undertone. Such a blue color space cannot be reached by any other pigment or combination of pigments; therefore, it becomes an exceptional differentiation factor for coatings producers.

Moreover, Ultramarine Blue pigment is very easy to disperse and to wet, neither migrates nor flocculates, has a high light fastness, is heat resistant, has a high solvent and alkali fastness, and does not show any metamerism. Another key feature in today’s world is its “green” profile, because it contains neither VOCs nor heavy metals in any reportable amount. On the other hand, Ultramarine Blues certainly do not have high tinting strength in comparison to organic pigments; nevertheless, they are better than other inorganic pigments such as Cobalt Blues. And it is true that Ultramarines are very transparent and do not provide opacity. But in many applications this is not a negative but rather a positive, e.g., metallic paints.

Why then has this pigment never been on the list of HPPs for coatings? The answer to this question is the historical perception industry technicians have had of the pigment’s poor weather fastness derived from its lack of acid resistance.

Correlation of Acid Resistance with Weather Fastness

Chemically Ultramarine Blue is a sodium aluminum sulpho-silicate. Due to its polysulfured composition, conventional Ultramarine Blues are not acid resistant. The pigment has a very porous structure. When Ultramarine Blue comes into contact with an acid, the acid penetrates into the pigment and breaks the polysulfur groups, damaging the 3D structure of the pigment (Figure 1). The polysulfur groups are the chromophores of the colorant. Once they have been broken there are no more chromophores available, and the reddish blue color becomes white.

When is Ultramarine Blue, incorporated into a coating, potentially exposed to acids? This occurs mostly in coatings used for outdoor exposure. Exterior coatings are subjected to UV radiation, high temperature, water (both humidity and rainfall) and oxygen for long periods of time. Even when using the most stable organic binders they will progressively degrade in the presence of such conditions. This degradation might generate acid radicals that could be released from the binder and attack the Ultramarine Blue structure.

In addition, when exterior coatings are located in highly industrial areas they can be exposed to “acid-rain”. Traces of acid from the atmosphere can slowly penetrate into the paint (if it is not well protected) and/or if the system is not highly resistant to industrial atmospheres, the binder degradation can lead to a deterioration process that yields acid components. Acid rain could then lead to the decoloration of Ultramarine Blue used in paints located in such environments.

In addition, any coating made with binders of an acidic nature, i.e., PVDF, PVC plastisols, or coatings containing acidic additives, is likely to have in its composition small traces of acid components that could cause the color fading of Ultramarine Blue.

A New Generation of Silica-Encapsulated Ultramarine Blue

Therefore to make Ultramarine Blue a HPP for coatings, Nubiola Inorganic Pigments faced the challenge of developing a new manufacturing technology that protects Ultramarine Blue from being attacked by acids in order to be used in exterior coatings. From all the technologies tested, the silica-encapsulation of the pigment proved to be the most effective. This technology has already been in the market for several years, but the performance of this encapsulation was not the best one. It certainly protected Ultramarine Blue from acids to a limited extent but at the cost of other characteristics of the pigment e.g., lower tinting strength, high oil absorption and poor dispersibility, all of which limited the use of the pigment in coatings.

The newly developed silica encapsulation technology overcame all the limitations of the conventional acid-resistant Ultramarine Blues from the past. This new technology delivered a new product called Nubicoat HWR (High Weather Resistance). It is based on the fact that the new technology encapsulates elemental particles and not agglomerates (Figure 2). A thinner silica layer is deposited therefore on each Ultramarine Blue particle. This results in the encapsulated pigment having a smaller average particle size as well as a narrower particle size distribution. Moreover it provides higher abrasion resistance of the protective silica coating.



In order to demonstrate the upgraded weather fastness of Nubicoat HWR, dozens of accelerated and long-term/natural weatherability studies on different coatings comparing the new product vs. conventional Ultramarine Blues, Pthalocyanine Blues and Cobalt Blues were conducted. Figure 3 summarizes some of the most relevant results. The accelerated weathering tests were made using QUV equipment, with UV-A lamps. The natural weathering tests were conducted on the roof of one of our facilities located in Barcelona (Spain), in a hot, industrial atmosphere with high marine humidity. According to NASA,2 Barcelona is the European city with the fifth highest number of sunlight hours/year.

All color measurements were made with a Spectrophotometer SP-88, with a D65 illuminant and a 10º angle view observant. As a conclusion of all the testing, it can be claimed that the weather fastness of the new generation of silica-encapsulated Ultramarine Blues (Nubicoat HWR) is much better than that of conventional Ultramarine Blues, similar to, or even better than, high-quality Phthalocyanine Blues, and very close to Cobalt Blues - the highly durable blue pigment benchmark.

More than two years after the launch of the breakthrough product, Nubicoat HWR has gained approvals and is regularly used by paint producers in a wide variety of applications e.g., facade paints (waterborne acrylics, styrene acrylics, silicate emulsions), interior decorative paints, powder coatings, coil coatings, coatings for plastics, bicycle and motorbike paints, and tinting systems for architectural and industrial coatings.

Summary

Nubicoat HWR, developed by Nubiola Inorganic Pigments, efficiently encapsulates Ultramarine Blue particles with silica and protects the particles from acid. Dozens of accelerated and natural weathering tests proved the enhanced weather fastness of such a product, similar to or even better than that of Phthalocyanine Blues and close to Cobalt Blues. The improved weatherability performance of the new product, in addition to the unique blue color and excellent properties showed by this “green” pigment, makes Nubicoat HWR a high-performance pigment for coatings.

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Nubiola Inorganic Pigments, Barcelona, Spain
Nubiola Inorganic Pigments, Barcelona, Spain

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • pci1022-Kinaltek-Lead-1170.jpg

    A Novel Pigment Production Technology

    Following an extensive R&D program that demonstrated...
    Paint and Coating Pigments
    By: Jawad Haidar and Nitin Soni
  • pci global top 10

    2025 Global Top 10: Top Paint and Coatings Companies

    The following is PCI’s annual ranking of the top 10...
    Paint and Coating Market Reports
    By: Courtney Bassett
  • 2025 pci 25

    2025 PCI 25: Top Paint and Coatings Companies

    PCI's annual ranking of the top 25 North American paint...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

Popular Stories

Akzo, SW, Nippon Logos

AkzoNobel Rejects Cash Offer From Nippon Paint, Sherwin-Williams

BASF SE Logo

BASF Announces Strategic Business Sale

AkzoSWNipponEndTalks

Nippon Paint, Sherwin-Williams End AkzoNobel Pursuit

POB-Point-and-Shoot

PCI Buyers Guide

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

Find Suppliers

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

September 15, 2026

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Automotive Paints and Coatings, 2nd Edition

Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

See More Products
Inside the AI Shift in Coatings - See the article now

Related Articles

  • A New Generation of Indanthrone Blue Pigments

    A New Generation of Indanthrone Blue Pigments

    See More
  • Potential for a New Generation of Solar-Reflective Coatings

    See More
  • A New Generation of High-Speed Fluorosurfactants

    See More

Related Directories

  • Revelli Chemicals Inc.

    Titanium Dioxide, Fumed Silica, Hydrocarbon Resin, Iron Oxide, Aluminum Paste, Organic Pigments, Zinc Oxide, Ultramarine Blue. Inventory stocked in locations across the USA and in Canada.
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing