Painting & Coating Industry (PCI) logo Powder coating summit logo
  • Sign In
  • Create Account
  • Sign Out
  • My Account
  • NEWS
  • PRODUCTS
  • MATERIALS
  • TECHNOLOGIES
  • FINISHING
  • RESOURCES
  • EVENTS
  • DIRECTORIES
  • EMAGAZINE
  • CONTACT
cart
facebook twitter linkedin youtube
  • NEWS
  • Latest News
  • Market Trends & Reports
  • Price Alerts
  • Subscribe to eNewsletters
  • Global Top 10/ PCI 25
  • Weekly Featured Article
  • COATLE Word Game
  • PRODUCTS
  • Product News
  • Must See Products and Services
  • MATERIALS
  • Additives
  • Resins/Polymers
  • Pigments
  • Equipment
  • Distributors
  • TECHNOLOGIES
  • Adhesives
  • Architectural Coatings
  • Industrial Coatings
  • Nanotechnology
  • Powder Coatings
  • Solventborne
  • Special Purpose Coatings
  • Sustainability
  • UV Coatings
  • Waterborne
  • Waterborne
  • FINISHING
  • Finishing News
  • Finishing Technologies
  • Finishing Equipment
  • RESOURCES
  • Columns
  • Blogs
  • Coatings Supplier Handbook
  • Podcasts and Videos
  • PCI Store
  • eBooks
  • Sponsor Insights
  • White Papers
  • COATLE Word Game
  • Columns
  • Ask Joe Powder
  • Did you know?
  • Distribution Dive
  • Focus on Canada
  • Formulating With Mike
  • Innovation Insights
  • Moody's Coatings Conundrums
  • Powder Coating Perspectives
  • Target the Market
  • TiO2 Insider
  • Blogs
  • Editor's Viewpoint
  • Industry Insights
  • Podcasts and Videos
  • COAT-IT! Podcast
  • Videos/PCI TV
  • EVENTS
  • Coatings Trends & Technologies Summit
  • Paint and Coatings Academy
  • Webinars
  • Calendar of Events
  • Lifetime Achievement Award
  • DIRECTORIES
  • Buyer's Guide
  • Equipment Directory
  • Materials Directory
  • EMAGAZINE
  • Current Issue
  • eMagazine Archive
  • China Issue Archive
  • Editorial Advisory Board
  • CONTACT
  • Contact Us
  • Advertise
  • Subscribe to eMagazine
  • Subscribe to eNewsletters
Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Price Alerts
    • Subscribe to eNewsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
    • FINISHING
      • Finishing News
      • Finishing Technologies
      • Finishing Equipment
    • RESOURCES
      • Columns
        • Ask Joe Powder
        • Did you know?
        • Distribution Dive
        • Focus on Canada
        • Formulating With Mike
        • Innovation Insights
        • Moody's Coatings Conundrums
        • Powder Coating Perspectives
        • Target the Market
        • TiO2 Insider
      • Blogs
        • Editor's Viewpoint
        • Industry Insights
      • Coatings Supplier Handbook
      • Podcasts and Videos
        • COAT-IT! Podcast
        • Videos/PCI TV
      • PCI Store
      • eBooks
      • Sponsor Insights
      • White Papers
      • COATLE Word Game
    • EVENTS
      • Coatings Trends & Technologies Summit
      • Paint and Coatings Academy
      • Webinars
      • Calendar of Events
      • Lifetime Achievement Award
    • DIRECTORIES
      • Buyer's Guide
      • Equipment Directory
      • Materials Directory
    • EMAGAZINE
      • Current Issue
      • eMagazine Archive
      • China Issue Archive
      • Editorial Advisory Board
    • CONTACT
      • Contact Us
      • Advertise
      • Subscribe to eMagazine
      • Subscribe to eNewsletters

    UV Protection and Coatings for Plastics in the Automobile Industry

    October 1, 2001


    Since Henry Ford launched his famous Model T, the development of automobile and transport engineering has experienced true quantum leaps. Because of the variety of possible forms, safety considerations and the significant weight savings, the automotive industry is increasingly using plastic components. On average, today's car consists of 14% of various types of plastic. The organic material is, however, subject to a natural aging process that makes the addition of stabilizers necessary. Exposure to sunlight accelerates the process. Often, such plastic components are treated with a topcoat. However, due to undesired migration, the concentration of stabilizer in the plastic and coating decreases over time. The plastic, as well as the coating, is then no longer sufficiently protected. This article describes the mechanism of migration and explains possible methods of delaying it.

    Figure 1

    Plastics

    Plastics are found in the car as cable insulation, interior covering, dashboards, tanks or under the hood. Increasingly, auto body components are also being made of plastic. Some of these are uncoated or appear in the same shade as the rest of the auto body. Some pilot projects even describe auto bodies made entirely of plastic.

    The material itself is subject to a natural aging process, which begins as early as manufacture, due to extreme processing conditions that occur at times. To delay the degradation as long as possible, so-called process and long-term stabilizers are added. If the component is exposed to the elements without protection, degradation is further accelerated. In addition to the compulsory long-term stabilization, the polymer also needs an additional UV-stabilization package.

    Figure 2

    Coatings

    The UV stabilization is an indispensable element of the plastic coating in the automobile exterior. In ideal circumstances, these are multi-layer systems. The coating of plastics begins with the application of a primer, which has a binding effect on the basecoat, that is then applied over the primer. Finally, a clearcoat containing the light stabilizers for UV protection seals the coating system.

    This, however, exacerbates the problem of migration1: the organic substrate makes it possible for the stabilizers to migrate into the plastic and also permits the migration of the plastic stabilizers to the top surface of the coating. With a decrease in the concentration of UV protector in the paint surface, the protective function of the coating, by definition, also decreases. Plastic stabilizers migrating upwards from the substrate cause yellowing in the topcoat or, in the worst case, can even lead to complete loss of adhesion.

    Figure 3

    Polymer Stabilizer Packages

    Every stabilizer has a specific temperature range in which it develops its optimum protective effect. For this reason, a mix of different stabilizers is added to the polymers - so-called stabilizer packages. They generally consist of primary and secondary antioxidants, and ensure sufficient protection of the polymer (see Figure 1).

    The most important primary antioxidants are the sterically hindered phenols. They are suitable as long-term stabilizers in almost all cases. Despite their many benefits, they have one undesirable side effect. As a result of UV radiation and subsequent photolytic degradation, they develop deeply colored quinoid structures which lead to a yellowing of the plastic (see Figure 2).2

    As protection against the often high temperatures during further processing, secondary antioxidants such as phosphites, phosphonites or HALS are also used.

    Coating Stabilizer Packages

    Two groups of stabilizers have been developed for coatings and are suitable for protecting both plastics and the coatings themselves: UV absorbers and sterically hindered amines (also called HALS = Hindered Amine Light Stabilizers).3

    Figure 4

    UV Absorbers

    Most UV absorbers function according to similar mechanisms. The physical absorption process protects both the deeper sections of the coating and the substrate from the high-energy fractions of sunlight. These are absorbed and lead to isomerization, causing the molecule to transform into an excited structure. When the molecule reverts to its original condition, the absorber releases the energy into the environment as thermal energy. The relevant UV absorbers in coatings include 2-hydroxybenzophenones, oxalanilides, 2-hydroxyphenylbenzotriazoles and 2-hydroxy-phenyltriazines.

    According to the Lambert-Beer Law, the absorption of a medium depends, among other things, on the UV-absorber concentration and on the distance traveled within it by the light. The concentration and the thickness of the coating may, therefore, not be permitted to fall short of a certain minimum limit in order to guarantee protection of the substrate through absorption. The deeper the UV ray penetrates the coating, the greater the absorption or the effect of the UV absorber. Due to the very short distance the UV ray is able to travel to the immediate surface of the coating, the protective effect of the UV absorber is at its lowest at this point (see Figure 3).

    Figure 5

    Sterically Hindered Amines (HALS)

    With UV protectors of the hindered amine light stabilizer type, stabilization results from the trapping of the intermediately developed radicals. All UV protectors of this type are based on a single chemical structure: tetramethyl-piperidine. They differ only in terms of the substituents at the nitrogen atom (R) or on the opposite ring side (R' and R'').

    They operate as UV protectors by combining with oxygen when exposed to light to form stable nitroxide radicals. The latter trap the radicals, which have developed from the polymer through exposure to UV rays. The most important feature of the nitroxide radicals is their regeneration capacity. Thus, a cyclical reaction is possible, which can repeat hundreds of times until the HALS itself has been degraded (see Figure 4). Radical chain reactions, which attack the coating and the substrate, are thus prevented.

    HALS, in contrast to UV absorbers, protect chemically rather than physically. Consequently, their effectiveness depends on optimum dispersal in the binding agent. The necessary quantity of HALS is therefore based on the solids content in the binding agent.

    Figure 6

    Migration Processes

    Migration is the undesired movement of the stabilizers between the coating layers and the substrate. Whether migration proceeds from the upper layer to the substrate or vice-versa -- negative effects occur in both cases. Among other things, the stabilizing properties of the coating may be lost or a degradation of the plastic may occur. The speed of migration depends on a variety of factors, including the temperature, solubility of the additives, concentration differences, the thickness of the coating or the mobility of the additive.2

    While migration cannot be completely prevented, it can be effectively delayed and controlled by the following.

    • Harmonization of plastics and coating stabilizers
    • Use of "non-migrating" stabilizers
    • Migration barriers
    In principle, migration can also be reduced through the use of high molecular -- and consequently lower mobile -- additives. The parameters of the molecular weight cannot, however, be varied at will, as it has a simultaneous effect on the secondary properties such as solubility and compatibility.

    Figure 7

    Detection through Microtome Technology

    The microtome technique is a modern method of tracing migration. Working from the outside, it separates coatings into thin layers thus permitting a detailed analysis of the protective layers. Depending on the hardness and brittleness of the material to be examined, suitable setting of the microtome permits sections of as little as 2 mm to be cut. In order to obtain intact and usable sections, the plastic samples are generally somewhat thicker. Subsequently the sections, which can be up to 7 x 9 cm, are placed in test tubes, mixed with an extraction agent and left in an ultrasonic bath for 10 hours. Afterwards, the concentration of the additive in each individual layer can be determined by HPLC (UV absorber) or gas-chromatographic means (HALS and UV-absorber).

    Methods of Reducing Migration

    Harmonization of Plastics and Coating Stabilizer

    HALS stabilize both the plastic and the coating. In the protective coating, the HALS operate together with a suitable UV absorber as light stabilizers. In plastics, on the other hand, they are often needed for process stabilization.

    Whereas it was common up to now for each manufacturer to use the stabilizer of his choice, the latest studies from Clariant prove the benefit of using identical stabilizers in the protective coating and the plastic. Otherwise the additive concentration in the protective layer drops significantly due to the extremely high level of migration, causing stabilization to become ineffective. The adhesive properties of the coating decrease, the component is subject to rapid discoloration and loss of gloss.

    The contrasting results achieved through the use of the same HALS in plastic and protective layer -- the clearcoat -- are shown in Figure 6. Here, too, a migration process occurs under the specified experimental conditions. However, the concentration profile confirms a significantly slower migration process. The use of the same additive therefore leads to a reduced alteration of concentration between plastic and protective layer. The concentration profile presented in Figure 6 is also comparable to the profile in multi-layer systems on a metal substrate. For this reason, greater weathering resistance can also be expected.1

    This new process, however, demands close cooperation between the manufacturers of coatings and the suppliers of plastics. This is because the same stabilizers can only be used following consultation. Apart from the increased stability, the laborious process of manufacturing multi-layer systems can be avoided, considerably reducing production costs. However, the process cannot be universally applied. Further points also remain troubling such as the considerable logistic requirements due to the wide spectrum of colors or the realization of metallic shades.

    Use of "Non-Migrating" HALS

    Various possibilities exist for directly preventing the migration of HALS. Oligomer HALS, for example, are so large that they adhere to the surrounding polymer matrix and migrate very little. A further variant is graftable HALS. These are chemically linked directly to the binding agent and are therefore not capable of any migration. Very special perspectives are offered by the new photo-reactive HALS Sanduvor PR-31.

    With this product, the first photo-reactive HALS (see Figure 7) have been developed. The malonic acid derivative not only exhibits the typical functional groups of the HALS, it also contains a UV absorbing system of conjugated double bonds, which also involves an olefinic double bond. The latter is split under UV light, causing the loss of the UV absorbing effect of the molecule. At the same time, the HALS molecule is chemically attached to the binding agent thus preventing migration. The HALS molecule is also fixed in place where the UV rays are greatest: at the upper surface of the coating. With decreasing strength of the UV rays, these HALS are, of course, capable of migrating into the deeper layers of the clearcoat, but can no longer bloom. As soon as Sanduvor PR-31 has migrated toward the surface, it is photochemically attached to the binding agent through the increased UV radiation. Thus the deeper regions of the clear coat have a reservoir effect for the surface and the proportion of HALS molecules fixed in the surface region increases with time. Overall, Sanduvor PR-31 guarantees not only lasting protection in the surface area but also excellent value, particularly with components subject to strong UV exposure.

    Migration Barriers

    So-called migration barriers block the migration of the additive. Basecoats and primers can have a hindering effect, especially when filled with disc-shaped pigments and extenders. Furthermore, the solubility of additives in the basecoat binder significantly influences the additive concentration in the top clearcoat and, consequently, the migration capacity. But each multi-layer system leads to a different migration speed.

    A higher crosslink density of the polymer matrix may contribute to the reduction of the additive migration speed as well. With increased crosslink density, the gaps in the polymer matrix become smaller, holding back larger additives. This variant is, however, of only limited success as excessive crosslink density leads to embrittlement of the coating.

    Conclusion

    Plastic components are having a determining influence on modern automobile construction and will be a decisive factor in shaping the car of the future due to their manifold advantages. As a result, the development of efficient and cost-cutting coating systems for this special substrate is becoming increasingly important. The most significant finding is that plastic and protective coatings beneficially contain identical stabilizers. The migration process is considerably retarded as a result and the expensive application of a multi-layer system becomes unnecessary. However, close cooperation between plastics supplier and coating manufacturer was highly appreciated.

    This article was originally presented at the Fourth International Coatings for Plastics Symposium, June 4-6, 2001, in Troy, MI.

    For more information on coatings for plastics, contact Gerd Faoro, Pigments and Additives Division, Polymer Additives BL, Boite Postale 149, 68331 Huningue, Cedex, France;

    phone 0033-389-89-6172; fax 0033-389-89-6195; e-mail Gerd.Faoro@clariant.com; or Circle Number 132.

    References

    1 "Distribution of Stabilizers in Multi-Layer-Coatings and Plastic Coatings,"3rd International Coatings for Plastic Symposium, Troy, MI, June 2000.

    2 "Potential Reasons for Yellowing of Coatings over Plastic Substrates," 4th International Coatings for Plastic Symposium, Troy, MI, June 2000.

    3 "Protecting UV-absorbing Clear Coats from Sunburn," Polymers Paint Colour Journal, February 2000.

    Share This Story

    Looking for a reprint of this article?
    From high-res PDFs to custom plaques, order your copy today!

    Recommended Content

    JOIN TODAY
    to unlock your recommendations.

    Already have an account? Sign In

    • PCI-0724-Global10-Feature-1440.png

      2024 Global Top 10: Top Paint and Coatings Companies

      Who ranks on top? PCI’s annual ranking of the top 10...
      Global Top 10 and PCI 25
      By: Courtney Bassett
    • PCI-0724-PCI25-Feature-1440.png

      2024 PCI 25: Top Paint and Coatings Companies

      PCI's annual ranking of the top 25 North American paint...
      Paint and Coating Market Reports
      By: Courtney Bassett
    • pci1022-Kinaltek-Lead-1170.jpg

      A Novel Pigment Production Technology

      Following an extensive R&D program that demonstrated...
      Paint and Coating Pigments
      By: Jawad Haidar and Nitin Soni
    You must login or register in order to post a comment.

    Arezu Saei
    August 12, 2024
    Hello, The article is awesome and very useful. Please give any article for designing a very flexible UV primer for automotive headlamp reflectors, having very good adhesion (tape test by cross hatch test) on Untreated BMC and very good intercoat adhesion to the aluminum metallize layer and pass 200 degree C heat test, and ABS varnish. Arezu Saei

    Report Abusive Comment

    close

    1 COMPLIMENTARY ARTICLE(S) LEFT

    Loader

    Already a Registered User? Sign in now.

    Subscribe For Free!
    • eMagazine
    • eNewsletter
    • Online Registration
    • Subscription Customer Service

    CTT Registration Now Open

    CTT Registration Now Open

    The Coatings Minute: Print Returns with PCI’s New Showcase Issue

    The Coatings Minute: Print Returns with PCI’s New Showcase Issue

    The Coatings Minute: Why Industry News Matters More Than Ever

    The Coatings Minute: Why Industry News Matters More Than Ever

    The Coatings Minute: Your Inside Look at PCInnovations

    The Coatings Minute: Your Inside Look at PCInnovations

    More Videos

    Sponsored Content

    Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

    close
    • Modern arapartment complex painted in bright colors.
      Sponsored byEPS - Engineered Polymer Solutions

      Architectural Polymers Leading the Way in Coatings Innovation

    • paint sprayer in a workshop
      Sponsored byallnex

      Enabling Performance and Compliance: allnex Introduces a New Line of VOC Exempt Solvent-Borne Resins

    Popular Stories

    No. 3 AkzoNobel

    AkzoNobel to Close Two Manufacturing Sites

    A collage of products using non-PFAS

    A Surge in Non-PFAS Releases

    Default Aerospace Image

    PPG Plans Major Aerospace Facility



    PCI Buyers Guide

    Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

    Start your RFP

    Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

    Find Suppliers

    Events

    September 3, 2025

    Coatings Trends & Technologies Summit

    The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

    January 1, 2030

    Webinar Sponsorship Information

    For webinar sponsorship information, visit www.bnpevents.com/webinars or email webinars@bnpmedia.com.

    View All Submit An Event

    Poll

    Longest-running laboratory experiment

    What is the longest-running laboratory experiment?
    View Results Poll Archive

    Products

    CTT Summit Short Courses (Live 9/3/25)

    Coatings Trends & Technologies Summit is expanding its offerings with four short courses. These short courses will offer an extensive day of interactive learning.

    See More Products
    pci  webinar april 2025

    PCI CASE EBOOK

    Related Articles

    • Color Stabilization of Wood and Durability Improvement of Wood Coatings: A New UV Light-Protection Concept for Indoor and Outdoor Applications

      See More
    • Plans In Place for Eighth International Symposium on Coatings for Plastics

      See More
    • UV and EB Coatings for Plastics

      See More

    Related Products

    See More Products
    • corrosion of linings.jpg

      Corrosion of Linings & Coatings: Cathodic and Inhibitor Protection and Corrosion Monitoring

    • durability.jpg

      Increasing the Durability of Paint and Varnish Coatings in Building Products and Construction 1st Edition

    • Kevin-Biller-PC-BOOK.jpg

      Powder Coatings - Foundation for the Novice Formulator (ebook)

    See More Products

    Events

    View AllSubmit An Event
    • September 5, 2024

      Panel Discussion: Navigating ‘Materials of Concern’ in the Coatings Industry

      On Demand Join us as industry experts from across the coatings value chain collaborate to discuss the debate surrounding these materials, how the restrictions are affecting their business, what innovative replacement products are under development, and what the future holds for some of these highly irreplaceable chemicals.
    View AllSubmit An Event

    Related Directories

    • Keyland Polymer UV Powder LLC

      Keyland Polymer develops, formulates, manufactures and sells UV cured powder coatings for wood, plastic, metal, composites, and other substrates. Keyland Polymer has a complete resin synthesis lab with global reach and distribution capabilities for the development, formulation, testing, and manufacturing of UV/EB curable solid resins.
    ×

    Keep the info flowing with our eNewsletters!

    Get the latest industry updates tailored your way.

    JOIN TODAY!
    • RESOURCES
      • Advertise
      • Contact Us
      • Directories
      • Store
      • Want More
    • SIGN UP TODAY
      • Create Account
      • eMagazine
      • eNewsletters
      • Customer Service
      • Manage Preferences
    • SERVICES
      • Marketing Services
      • Reprints
      • Market Research
      • List Rental
      • Survey & Sample
    • STAY CONNECTED
      • LinkedIn
      • Facebook
      • Youtube
      • X (Twitter)
    • PRIVACY
      • PRIVACY POLICY
      • TERMS & CONDITIONS
      • DO NOT SELL MY PERSONAL INFORMATION
      • PRIVACY REQUEST
      • ACCESSIBILITY

    Copyright ©2025. All Rights Reserved BNP Media.

    Design, CMS, Hosting & Web Development :: ePublishing

    Painting & Coating Industry (PCI) logo Powder coating summit logo
    search
    cart
    facebook twitter linkedin youtube
    • Sign In
    • Create Account
    • Sign Out
    • My Account
    Painting & Coating Industry (PCI) logo Powder coating summit logo
    • NEWS
      • Latest News
      • Market Trends & Reports
      • Price Alerts
      • Subscribe to eNewsletters
      • Global Top 10/ PCI 25
      • Weekly Featured Article
      • COATLE Word Game
    • PRODUCTS
      • Product News
      • Must See Products and Services
    • MATERIALS
      • Additives
      • Resins/Polymers
      • Pigments
      • Equipment
      • Distributors
    • TECHNOLOGIES
      • Adhesives
      • Architectural Coatings
      • Industrial Coatings
      • Nanotechnology
      • Powder Coatings
      • Solventborne
      • Special Purpose Coatings
      • Sustainability
      • UV Coatings
      • Waterborne
      • FINISHING
        • Finishing News
        • Finishing Technologies
        • Finishing Equipment
      • RESOURCES
        • Columns
          • Ask Joe Powder
          • Did you know?
          • Distribution Dive
          • Focus on Canada
          • Formulating With Mike
          • Innovation Insights
          • Moody's Coatings Conundrums
          • Powder Coating Perspectives
          • Target the Market
          • TiO2 Insider
        • Blogs
          • Editor's Viewpoint
          • Industry Insights
        • Coatings Supplier Handbook
        • Podcasts and Videos
          • COAT-IT! Podcast
          • Videos/PCI TV
        • PCI Store
        • eBooks
        • Sponsor Insights
        • White Papers
        • COATLE Word Game
      • EVENTS
        • Coatings Trends & Technologies Summit
        • Paint and Coatings Academy
        • Webinars
        • Calendar of Events
        • Lifetime Achievement Award
      • DIRECTORIES
        • Buyer's Guide
        • Equipment Directory
        • Materials Directory
      • EMAGAZINE
        • Current Issue
        • eMagazine Archive
        • China Issue Archive
        • Editorial Advisory Board
      • CONTACT
        • Contact Us
        • Advertise
        • Subscribe to eMagazine
        • Subscribe to eNewsletters