Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Join Today
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • PCI News Now
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • JOIN!

Color Management - CCI and X-Rite Provide Color Accuracy on the Factory Floor

By Matthew Gryczan
March 7, 2008
As one of the world’s largest manufacturers of color cards and color systems, Chicago-based Color Communications Inc. (CCI) specializes in exact duplication of the colors consumers see when they apply paints and stains to the interior and exteriors of their homes. True to its reputation as an innovator, CCI has recently employed an X-Rite inexpensive in-line, non-contact spectrophotometer that provides laboratory accuracy in reading colors on the factory floor



As one of the world’s largest manufacturers of color cards and color systems, Chicago-based Color Communications Inc. (CCI) specializes in exact duplication of the colors consumers see when they apply paints and stains to the interior and exteriors of their homes. Over the past 35 years, CCI has produced billions of color merchandising products for companies around the globe, such as the paint chips offered by the paint manufacturers at home improvement retailers like Home Depot and Lowe’s to the paint samples in brochures and displays used in automotive showrooms enabling consumers to select the color of their new cars and trucks.

True to its reputation as an innovator, CCI has recently employed an X-Rite inexpensive in-line, non-contact spectrophotometer that provides laboratory accuracy in reading colors on the factory floor. The company estimates that the instrument will pay for itself in less than a year through savings in scrap, equipment downtime and labor costs.

CCI employs more than 500 people at its main Chicago facility and an Auckland, New Zealand plant. The company’s work is so precise that some color tools produced by CCI are used by its customers as standards for their internal color quality control.

“Customers come to us because they have a need for accurate color,” said Jerald Dimas, Vice President-Technical at CCI. “There is a premium cost to our product because of that accuracy. You can’t print colors using four-color process printing for an accurate representation. We use the actual paint in our process. That’s one of our competitive advantages: High-speed production with a high degree of accuracy.”

Ensuring Color Quality

To ensure color quality during a production run, CCI technicians take test samples by stopping the equipment, cutting the desired sample from the production roll and conducting spectrophotometer tests. A high-profile project for Akzo Nobel Coatings required more than 20,000 such measurements in the last eight months alone. The costs of quality add up quickly because part of the production run is spoiled by taking the sample, and the equipment remains idle during the testing process. In addition, quality control personnel spend time conducting the tests and transporting samples to and from the factory floor.

By multiplying the resources expended to test one sample by the tens of thousands of tests it performs annually, CCI determined it had a great opportunity for cost savings and enhanced quality control practices.

To pursue this opportunity, CCI agreed to act as one of a number of beta test sites this past year for a new-generation spectrophotometer developed by X-Rite that can measure samples without destructive testing, match the accuracy of lab-confined spectrophotometers on a relative basis, and withstand the harsh environments of a factory floor.

Cost - A Key Factor

And there was one final key to make the system work for CCI: cost. By using innovations from a variety of industries, X-Rite offers the instrument at less than $20,000 a unit, nearly one-fifth the cost of other lab-bound or non-contact spectrophotometers. Michigan-based X-Rite, the world’s largest manufacturer of color measuring instruments, has begun introduction of the product worldwide following its successful trials at CCI.

“When we first started looking at non-contact spectrophotometers, everything was in excess of $100,000,” Dimas said. “We were still looking at them to see if they could pay for themselves, but the cost really didn’t look that attractive at those prices. “With the VeriColor® Spectro, the return on investment is excellent. There isn’t a reason not to use this sort of equipment in the factory now.”

VeriColor Spectro System

CCI uses the VeriColor Spectro system to measure color at a distance of up to 4 inches from the sample, which Dimas said is more than adequate for his company’s needs and allows for versatility in mounting the instrument. Because the instrument does not employ destructive testing, CCI has been able to compile data as often as it wishes while the process is running. Under the destructive testing system, CCI conducts tests at the beginning, middle and end of the product run simply because of the resources required for each test.

“We have a very active Six Sigma program here, and one of its tenets is to define and measure for constant improvement,” Dimas said. “We want to catch a problem at the source and, in order to catch it, we have to measure it.”

CCI has begun to correlate the process data that it collects from the VeriColor Spectro instrumentation with other quality control systems that monitor dwell and cure times, film thickness and substrate variations to “engineer the quality into our products,” Dimas said.

Dimas said the robust nature of the VeriColor Spectro in harsh environments was critical to CCI. The basic VeriColor Spectro instrument shows lab-quality reproducibility in temperature conditions ranging from 32 – 125 °F and can show the same reproducibility up to 167 °F with a special enclosure that uses compressed air to cool the system and keep optics clean. “A lot of spectrophotometers are very sensitive when it comes to temperature for reproducibility, and the VeriColor hasn’t shown that,” Dimas said.

Initial results indicate that the VeriColor Spectro will allow CCI to reduce the number of off-line samples from tens of thousands of trials to hundreds over the course of a year. For instance, the 20,000 off-line readings that were required for Akzo Nobel could be replaced with digital readings by using the VeriColor in the future.

“One of the reasons why we need something like this is because our industry is so demanding,” Dimas said. “It really depends on the norm in your industry. It is not uncommon for us to maintain our tolerances below a half unit or less. That is very, very tough to do.”

For more information, contact gryczan@seyferthpr.com.

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Vice President | Seyferth Spaulding Tennyson, Inc., Grand Rapids, MI

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • Double exposure of creative chemistry concept on laptop background, research and development concept

    Inside the AI Shift in Coatings

    Industry leaders share real-world examples of how AI is...
    Paint and Coatings Additives
    By: PCI Editorial Staff
  • Global Top 10 and PCI Logo

    2026 Global Top 10: Top Paint and Coatings Companies

    See how the world’s largest paint and coatings companies...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • The 2026 PCI 25

    2026 PCI 25: Top Paint and Coatings Companies

    See how North America's largest paint and coatings...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • Join Paint & Coatings Industry
  • Manage My Preferences
  • Customer Service

More Videos

Popular Stories

Mergers and aquisitions

BASF Ends Evonik Takeover Pursuit

Breaking News

H.B. Fuller to Close Seven Sites in Supply-Chain Overhaul

AkzoNobel Axalta

EU Clears $25B Akzo-Axalta Merger with One Big Condition

Events

December 2, 2026

Self-Activated Binder Technology: A New Path to Tin-Free Polyurethane Coatings

Through examples from protective and general industrial coating applications, attendees will learn how these innovative technologies can help maintain, and in some cases improve, coating performance while supporting safer, more sustainable formulations that align with evolving regulatory expectations

December 10, 2026

PC Academy: Waterborne Polymers and Film Formation

The trend towards waterborne polymers in the paint and coatings industry is clear; highlighting their environmentally friendly nature, regulatory considerations, growing market demand, and meeting sustainability goals.

View All Submit An Event

Products

Powder Coatings - Foundation for the Novice Formulator (ebook)

Powder Coatings - Foundation for the Novice Formulator (ebook)

See More Products
PCI news now promo ad

Related Articles

  • Lucideon-lead-image

    Color Accuracy Depends on These Best Practices

    See More
  • X-Rite Showcases Color Management Solutions

    See More
  • COYPR800x400.jpg

    X-Rite's Color Management Solutions to Support Pantone's 2025 Color of the Year

    See More

Related Products

See More Products
  • pci may 2020

    PCI May 2020 Issue

See More Products

Related Directories

  • Datacolor Color Management Solutions Limited

  • X-Rite Pantone

    X-Rite delivers advanced color measurement and management solutions for the paints and coatings industry. Its instruments and software support precise color formulation, quality control, and consistency across production. X-Rite empowers manufacturers to achieve accurate, repeatable color, reduce waste, and enhance product appeal in decorative, industrial, and automotive coatings.
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Manufacturing Division
  • JOIN TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing