Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!
Paint and Coating Resins & PolymersArchitectural CoatingsIndustrial CoatingsSpecial Purpose CoatingsSustainableInnovation Insights

Chitosan: A Next-Generation Functional Material for Paint and Coatings Innovation

By Victoria Scarborough Ph.D., Vice President for Collaborative Innovation, The ChemQuest Group
1-InnovationInsights.png
Background image credit: DrAfter123, DigitalVision Vectors / Getty Images
March 11, 2026

This quarterly column, written by Victoria Scarborough, Ph.D., Vice President Collaborative Innovation of The ChemQuest Group, Inc., provides a look into the latest trends and technologies within the coatings and adjacent industries that impact the value chain.


Sustainability commitments, environmental,  social and governance (ESG) reporting, and tightening global regulatory pressures are transforming coating design strategies.¹ Coatings manufacturers are being driven to reduce petrochemical dependency, lower environmental impact, and deliver safer chemistries while maintaining performance.² Among emerging biobased polymers, chitosan stands out as a multifunctional renewable material offering environmental compatibility alongside meaningful performance benefits for coatings.3 Derived from crustacean shells, fungal biomass, and insect exoskeletons, chitosan is abundant and chemically unique as the only naturally occurring alkaline polysaccharide that can be engineered by controlling degree of deacetylation, molecular weight, and salt form.4,5 

Figure 1. Structure of chitosan.4

Structure of chitosanSource: The ChemQuest Group, Inc.


Figure 2. Chitosan production.5

Chitosan productionSource: The ChemQuest Group, Inc.


Using crustacean waste in the process illustrated in Figure 2, chitosan pricing translates to a range of $2.50 - 5.50/lb. The global chitosan market is valued at $7.8 billion and is forecast to reach $42.8 billion by 2033, expanding at a CAGR of 18%.6 

Chitosan’s structural tunability allows formulators to manage viscosity, reactivity, solubility profile, and interaction behavior in coatings systems. It is biodegradable, aligning with circular economy goals, breaking down to CO₂, water and nutrients.6 Its protonated amino groups, present under acidic conditions, enable charge interaction, adhesion capability, antimicrobial performance, and strong metal chelation properties.7 These attributes enable coatings engineers to treat chitosan not merely as a “green binder replacement” but as a functional performance platform.

Antimicrobial and Antifungal Performance

Microbial preservation has become increasingly challenging as traditional preservatives face regulatory restrictions and declining market acceptance. Chitosan provides inherent antimicrobial, antifungal, and antiviral functionality via electrostatic binding to negatively charged microbial membranes, leading to membrane disruption and inhibition of replication. 

Figure 3. Proposed antimicrobial mechanism of chitosan.7

Proposed antimicrobial mechanism of chitosan7Source: The ChemQuest Group, Inc.


Chitosan-containing coatings have demonstrated application in hygiene-sensitive environments, architectural interiors, institutional surfaces, and cultural‐heritage protection systems.7 Unlike conventional preservatives used solely as additives, chitosan can function simultaneously as structural polymer + antimicrobial, reducing the need for synthetic biocides.8 

Film-Forming and Barrier Capabilities

Chitosan forms clear, continuous films when processed under mildly acidic aqueous conditions due to strong hydrogen bonding in the polymer network. These films can serve as oxygen and aroma barriers and support protective surface coating development in eco-focused systems.3

Figure 4. Chitosan film.9

Chitosan filmSource: The ChemQuest Group, Inc.


Because the material is hydrophilic, coatings exposed to moisture require crosslinking, hydrophobic modification, or incorporation of nanocomposites to achieve durable long-term performance. 

Corrosion Protection and Metal Chelation

Corrosion protection represents one of the most compelling application areas for chitosan in coatings.3 Chitosan’s amine and hydroxyl groups coordinate metallic ions and absorb to metal substrates, creating protective complexes that limit penetration of corrosive species such as oxygen, water, and chloride ions. 

Figure 5. Anticorrosive mechanism of chitosan.3

Anticorrosive mechanism of chitosanSource: The ChemQuest Group, Inc.


Chitosan coatings have demonstrated passivation capability by forming adherent chitosan–metal complexes that stabilize the substrate and retard electrochemical corrosion reactions. Reinforcement through nanomaterials such as graphene oxide, silica, or zinc oxide (ZnO) further enhances structural integrity and electrochemical resistance.10 Reported results include promising protection of steel, aluminum, and copper while eliminating heavy metals and phosphate-based inhibitors.11

Formulation Considerations12

As a unique cationic multifunctional raw material, chitosan does not conform to traditional formulating guidelines. Instead, it requires an understanding of several variables that can affect its overall behavior in paint formulas. It is likely that these complications have contributed to its nascent use. Special attention should be given to these areas.

Solubility and pH Sensitivity

Native chitosan is only soluble in acidic aqueous solutions by protonation of amine groups, which complicates direct blending into neutral or alkaline latex paints or many waterborne binder systems. To incorporate chitosan, you often must use water-soluble salts (acetate, lactate) or chemically modified chitosan derivatives that are soluble at neutral pH. This adds processing steps or requires careful pH control.

Viscosity and Rheology

Chitosan solutions can be highly viscous even at low solids when using high MW grades. This affects sprayability, film formation, and compatibility with typical paint rheology modifiers. Precise use and control of chitosan MWs and solids level is necessary. Blending into existing paint formulas may require adjustments to the rheology package.

Water Sensitivity and Barrier Performance

Pure chitosan films are hydrophilic and can be water-sensitive and swell in high humidity conditions, leading to reduced film integrity. For more durable coatings exposed to moisture, chitosan typically requires crosslinking, blending with hydrophobic polymers, or incorporation of nanofillers to reach acceptable water resistance.

Adhesion and Mechanical Performance

High-MW chitosan used in coatings can be brittle, requiring plasticizers or copolymers to add more flexibility. Substrate adhesion and long-term toughness can be increased by adding crosslinking agents or compatibilizers to create a stronger composite matrix.

Antimicrobial Effects 

While chitosan is antimicrobial, it can interact with other formulation ingredients like anionic pigments, surfactants, and binders. Its cationic nature leads to complexation and potential pigment flocculation or binder destabilization if not managed with proper dispersants and pH control. Long-term formula stability should be evaluated under standard testing conditions. 

Regulatory and Sensory Constraints (for Edible Applications)

Chitosan is approved by the U.S. Food and Drug Administration for use in food contact. For edible coatings, regulatory acceptance, organoleptic (taste/feel) impacts, and traceability of raw material sources (shellfish allergens) must be addressed if such coatings contact food. Non-animal fungal chitosan helps mitigate allergen concerns but may require separate regulatory validation. 

Other Considerations

Native chitosan is acidic-soluble only, requiring salt derivatives or modifications for latex systems. High-MW grades significantly influence viscosity and rheology. Hydrophilicity requires compensation strategies in humid environments. Cationic behavior requires management when interacting with anionic pigments or resins. These complications explain its nascent emerging adoption, as formulators must compensate for varying chemical behaviors of chitosan.

Sources of Chitosan

There are multiple domestic suppliers and specialty producers of chitosan and its derivatives (Figure 6).  Products are divided into commercial and USP (pharmaceutical) grades and offer multiple grades and forms (salts, low MW, high MW, water-soluble derivatives) used by formulators. Commercial chitosan grades are tailored for use in packaging, food, cosmetics, agriculture, coatings, water quality, and other industrial uses, while medical and pharmaceutical grades meet the needs of those formulating medical devices and implant coatings and pharmaceuticals.

Recently, Milliken & Co., a large privately held chemical manufacturer serving the textile, flooring, chemical, and healthcare sectors, has invested in Tidal Vision, a regional chitosan supplier.13 The partnership is designed to accelerate the introduction of biodegradable chemistries across Milliken’s served markets and helps drive the company’s sustainability goals.

Figure 6. Chitosan suppliers (Source: The ChemQuest Group, Inc.).

Chitosan suppliersSource: The ChemQuest Group, Inc.


Conclusion

Chitosan represents a next-generation opportunity material for coatings innovators, delivering sustainability claims alongside functional coatings benefits such as antimicrobial performance, barrier ability, chelation-driven corrosion mitigation, and environmental compatibility. Supplier availability and patent activity continue to expand. Multiple granted patents and industry investment demonstrate movement toward chitosan-enabled coatings addressing antimicrobial, anticorrosion, and structural innovation. Academic research further supports reinforcement strategies, nanocomposites, and hybrid chitosan-binder systems. These developments indicate accelerating readiness for broader use across architectural, marine, protective, and specialty coatings.

While formulation integration demands technical rigor, advancements in derivative chemistry, composite design, and processing methodology are rapidly expanding opportunities for commercialization. In response to increasing sustainability pressure and performance expectations, chitosan is positioned to play a meaningful role in the future of coatings technology.

To learn more, contact the author at vscarborough@chemquest.com or visit https://chemquest.com. 

References

¹ EU Corporate Sustainability Reporting Directive (CSRD), Canadian CSA ESG Guidance (2022), and U.S. SEC Climate Disclosure Rules. All require public companies to report GHG emissions, climate risks, governance, and strategies.

² “U.S. Market Analysis for the Paints & Coatings Industry (2023–2028),” American Coatings Association and The ChemQuest Group, https://www.paint.org/programs-publications/publications/us-and-global-market-analysis/.

³ Sarfraz, M. H.; Hayat, S.; Siddique, M. H.; Aslam, B.; Ashraf, A.; Saqalein, M.; Khurshid, M.; Sarfraz, M. F.; Afzal, M.; Muzammil, S. Chitosan-based Coatings and Films: Perspective on Anticorrosion and Sustainable Coatings. Progress in Organic Coatings 2024, 188, 108235.

⁴ Comprehensive Biomaterials II 2017, 2, 279–305.

⁵ Mawazi, S. M.; Kumar, M.; Ahmad, N.; Gi, Y.; Mahmood, S. Recent Applications of Chitosan and Its Derivatives in Antibacterial, Anticancer, Wound Healing, and Tissue Engineering Fields. Polymers 2024, 16 (10), 1351.

⁶ “Chitosan Market by Source (Shrimp, Crab, Squid, Fungal), Application (Water Treatment, Biomedical, Food & Beverages, Cosmetics, Agriculture), End-Use Industry, and Region – Global Forecast to 2034,” Reports and Data, April 2024.

⁷ Zheng, M. Antiviral Activity of Chitosan and Its Derivatives: A Review. Carbohydrate Polymers 2020, 227, 115831.

⁸ Chitosan-containing Coating Compositions that Improve Elongation, Thermocycling, Reduce Leaching and Diminish Fungal/Mildew Defacement. The Sherwin-Williams Co. U.S. Patent 12,398,278 B2, 2025.

⁹ Cazón, P.; Vázquez, M. Mechanical and Barrier Properties of Chitosan Combined with Other Components as Food Packaging Film. Environmental Chemistry Letters 2020, 18, 257–267.

¹⁰ Wang, L. Chitosan–ZnO Nanocomposite Coatings for Steel Corrosion Protection. Applied Surface Science 2019, 493, 625–635.

¹¹ Bahari, H. S.; Ye, F.; Carillo, E. A. T.; Leliopoulos, C.; Savaloni, H.; Dutta, J. Chitosan Nanocomposite Coatings with Enhanced Corrosion Inhibition Effects for Copper. International Journal of Biological Macromolecules 2020, 162, 1566–1577.

¹² Thambiliyagodage, C.; Jayanetti, M.; Mendis, A.; Ekanayake, G.; Liyanaarachchi, H.; Vigneswaran, S. Recent Advances in Chitosan-Based Applications—A Review. Materials 2023, 16, 2073.

¹³ “Milliken & Company Announces Investment in Tidal Vision,” https://www.milliken.com/en-my/blogs/milliken-and-company-announces-investment-in-tidal-vision.


 

KEYWORDS: antimicrobial coatings bio-based bio-based coatings bio-based materials Corrosion Control corrosion inhibitors manufacturing polymer dispersions polymerization raw materials specialty chemicals sustainability

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Victoria Scarborough, Ph.D., Vice President for Collaborative Innovation, The ChemQuest Group, Cincinnati, OH

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • pci1022-Kinaltek-Lead-1170.jpg

    A Novel Pigment Production Technology

    Following an extensive R&D program that demonstrated...
    Paint and Coating Pigments
    By: Jawad Haidar and Nitin Soni
  • pci global top 10

    2025 Global Top 10: Top Paint and Coatings Companies

    The following is PCI’s annual ranking of the top 10...
    Paint and Coating Market Reports
    By: Courtney Bassett
  • 2025 pci 25

    2025 PCI 25: Top Paint and Coatings Companies

    PCI's annual ranking of the top 25 North American paint...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

  • colorful building exterior
    Sponsored byDow

    Insights into Exterior Architectural Coating Degradation: Bridging Accelerated and Natural Weathering

Popular Stories

Supply chain question and cargo piles up and piling shipping containers question concept

Energy Disruptions Begin to Hit Coatings Supply Chain

basf

BASF Coatings Names Incoming CEO Ahead of Separation

PPG announced the installation of a state-of-the-art pilot finishing line that features IPG’s PhotoniCURE™ laser curing system at its powder manufacturing and technical facility in Strongsville, Ohio.

PPG Tests Laser Curing for Powder Coatings

POB-Point-and-Shoot

PCI Buyers Guide

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

Find Suppliers

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

April 28, 2026

Next Gen Dispersion Technology in Paint Production: Driving Higher Quality at Lower Costs

Join this webinar to see how manufacturers reduce costs, energy use, raw materials, labor, and floor space while improving quality.

View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Automotive Paints and Coatings, 2nd Edition

Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

See More Products
Register for webinar: Next-Gen Dispersion Technology in Paint Production

Related Articles

  • a handshake over a horizon with individuals superimposed over the hands

    Arkema Partners with Research Institute to Open a Lab in France for Next-Generation UV-Curable Materials

    See More
  • lubrizol

    Next-Generation Matting Agents for UV Coatings

    See More
  • image of BCFs logo

    BCF Advocates Apprenticeships for Next Generation of the U.K. Coatings Industry

    See More

Related Products

See More Products
  • nanostructured.jpg

    Nanostructured Thin Films and Coatings: Functional Properties

  • Kevin-Biller-PC-BOOK.jpg

    Powder Coatings - Foundation for the Novice Formulator (ebook)

  • intelligent.jpg

    Intelligent Coatings for Corrosion Control 1st Edition

See More Products

Related Directories

  • Atlas Material Testing Technology LLC

    For more than 100 years, Atlas has been a leader in materials testing, offering a complete line of weathering testing instrumentation, laboratory, and outdoor testing services.
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing