Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!

A New Approach to Understanding Rheological Additives

June 1, 2004
Rheological additives play a major role concerning storage and application properties of liquid systems. In waterborne coatings they have a major influence on such key properties as vertical flow, leveling, gloss, film thickness, covering power, spattering tendency, brush and roll resistance, sedimentation tendency and pigment stabilization. They have always been an important component in the production of paints and lacquers. Even at the beginning of the production process, it is possible to optimize the energy input into the material to be ground, thus leading to a better dispersibility in those systems.

At the same time, rheological additives can considerably improve shelf life by reducing the settling tendency of pigments and fillers in a paint or lacquer formulation. Without adequate rheological control, those systems very often show syneresis effects (Figure 1).

With spray application, an optimum compromise has to be found between good vertical flow characteristics (to achieve an adequate film thickness) and good leveling (to obtain a smooth finish). For this reason, in the low-shear range, the viscosity must be set just high enough to prevent vertical flow. At the same time, the viscosity should be kept as low as possible to ensure good leveling. Inappropriate rheological control might be the reason for building curtains or runners that will strongly impact the quality of the resulting surface coating (Figures 2a and 2b).

A comparatively high viscosity at high shear prevents centrifugal forces from expelling the coating too easily from the brush or roller. This spatter resistance, modified via the rheology, is an important quality characteristic of a coating. Figure 3 shows the influence of the high-shear viscosity on a roller-applied finish.

The reason why setting the high-shear viscosity is so important is that it basically governs the brush/rolling resistance during application of the coating. If the brush resistance is inadequate, a considerable proportion of the coating applied to the surface is pushed along in front of the brush or roller without adhering to the substrate. This results in poor hiding power, uneven application and poor leveling (Figures 4a and 4b). Apart from these optical defects, an uneven coating provides less protection from environmental influences because such inhomogeneous films frequently have weak points. All in all, the life expectancy of a coating is often shorter if the coating material is not optimized according to the method of application.

Also, the phenomenon of edge marks (Figure 5), in addition to wetting problems, is due to an inadequate rheological profile of a coating.

Adequate effectiveness of modern thickeners is not only extremely important in the field of emulsion paints, but it also plays a major role in industrial coating systems. Unlike emulsion paints, which are usually applied by brush or roller, industrial coatings are normally applied by spraying or dipping. With spray application, an optimum compromise has to be found between good vertical flow characteristics and good leveling. It is logical that in such cases, use is frequently made of an associative thickener that has more of a pseudoplastic rheology profile. In parallel with this, however, it must have a certain efficacy in the high-shear range in order to ensure satisfactory spray application.

With the transition from solventborne to low-solvent or solvent-free coating systems, high demands are made on rheological additives. The trade normally wants the same application properties as they have customarily had with solventborne coatings. In addition, special flow properties1-4 are sometimes specified. Rheological additives, therefore, rank among the most important components in modern coating systems.

Non-Associative Rheological Additives

The thickening effect of the non-associative rheological additives is based primarily on a thickening of the aqueous phase as a result of polymer chain entanglement. There is virtually no interaction with other components of the coating system. Whereas the water-binding behavior of the polymer (e.g. water retention by cellulose ethers) prevents the undesirable effect of the water disappearing into highly absorbent substrates, it does create the risk that the dispersed particles are displaced from the aqueous phase, leading to flocculation due to volume restriction. This flocculation can result not only in a deterioration of the gloss, but it can also have a negative effect on the corrosion resistance of the coating system.5

Associative Thickeners

With associative thickeners, this effect occurs only in rare cases. The mode of action of these additives is primarily based on the interaction (association) of the hydrophobic components of the thickener molecule with components of the coatings such as latex particles, pigments and extenders. The hydrophilic segments of the thickener remain in the aqueous phase. As a result of the interaction, a three-dimensional reversible physical crosslinking occurs in the dispersion, which has a major influence on the flow properties of such a system.

By varying the chemical structure of the rheological additive, the flow properties of modern coating systems can be adapted to the respective requirements.4,6-10 For example, highly effective polyurethane thickeners can be specifically synthesized for emulsion paints (for roller or brush application), which are especially suitable for the high shear rates typical of this kind of application. Apart from this, rheological additives must be such that, in combination with other thickeners (for example, with the cellulose derivatives used for the low-shear sector), they can create an overall rheology profile that combines adequate storage stability and good vertical flow/leveling characteristics with optimum application properties.

Special Aspects When Using Associative Thickeners in Aqueous Systems

Water-thinnable coatings are complex, multi-component systems whose application properties depend not only on the proportion and properties of the individual components, but also on their respective interactions. This becomes particularly evident when adjusting the flow properties of aqueous coating systems because the flow requirements can vary considerably according to the particular application.

The flow behavior of such systems is affected in particular by the following factors:

    •Disperse phase (volume content, particle size, particle size distribution, degree of dispersion, interaction of the individual particles);
    •Medium (water, co-solvents);
    •Temperature;
    •pH;
    •Additives.
It is not only the total quantity of dispersed particles that influences the rheological behavior of coatings, but also their size distribution. In real systems, the flow properties of the entire system essentially depend on the extent to which the entire volume can be filled. For example, at equal volume content (percent by volume), combinations of large and fine particles (e.g. extender/pigment combinations) can have a lower viscosity than dispersions consisting only of comparatively large particles. The fine particles find their way into the gaps between the larger particles and thus fill up the volume better, which can in turn, lead to improved flow characteristics of the overall system.

One of the key factors affecting the flow behavior of coating systems is the interaction of the individual particles. With regard to pigments and extenders, instability of the coating can be caused by coagulation, which is due to the effects of surface charging. In addition, problems can also arise, for instance, through the interaction of water-insoluble coalescing agents with the polymer particles.

As far as the rheological profile of liquid systems is concerned, we can basically distinguish between three groups (we refer here, above all, to surface coatings) (Figure 6):

    •Newtonian: The viscosity of the system does not depend on the shear gradient applied.

    •Dilatant: Viscosity rises with increasing shear (which is normally extremely undesirable in surface coatings).

    •Pseudoplastic (non-Newtonian, thixotropic): The viscosity decreases with increasing shear gradient and then, when the external forces decline, returns immediately (non-Newtonian) or with a certain delay (thixotropic) to approximately its original value.

The effectiveness of an associative thickener is governed primarily by its structure. Here, the length of the polymer, its hydrophilic/hydrophobic characteristics (polarity) at the assigned segments, the conformation of the polymer chains and the ratio between polymer chain length and binder particles/solid particles play a key role. Through the skillful adjustment of all these parameters, it is possible to produce highly effective associative thickeners with an optimized profile of efficacy. Nevertheless, initial trials with highly active polyurethane thickeners frequently lead to stability problems in the coating. These can be avoided by observing in particular the following points:
    •Optimum addition of the thickener;
    •Salt content of the coating;
    •Selection of suitable rheological additives when using combinations of low- and high-shear thickeners;
    •Careful adjustment of the pH.


Structure/Rheological Effectiveness of Associative Thickeners

The efficient use of rheological additives presumes a deeper knowledge of the relationship structure/rheological effectiveness of associative thickeners and their interaction with other components in aqueous coating systems.

One of the basic methods used to create linear associative polyurethane thickeners is to combine linear OH-bifunctional polyethers e.g. H-[O-CH2-CH2]x-OH together with mono isocyanates such as octadecyl isocyanate (C18H37-NCO):

As the Type A method is limited to the availability of mono isocyanates, it is sometimes more convenient to combine OH-bifunctional polyethers e.g. H-[O-CH2-CH2]x-OH together with diisocyanates OCN NCO and aliphatic alcohols OH

This method (type B) allows more variation concerning the endcapping of the polymer chain. It is evident that the above given structure of type B is an idealized one.

The hydroxyl groups of the polyether compete with the hydroxyl group of the alcohol in the same manner while reacting with the isocyanate groups and, therefore, lead to a statistically determined distribution of polymer chains of type C:

Although it is not possible in this case to obtain pure material having a definite chain length, the distribution of the polymer chain lengths can principally be influenced by adjusting the molar quantities of the corresponding raw material. e.g.

This reaction method also leads to by-products of low molecular weight such as those of type D.

The situation becomes even more complex when using polyfunctional branched polyethers or polyfunctional branched isocyanates resulting in polymers of type E.

Examinations of C. D. Eisenbach et al.8 pointed out that length and nature of the hydrophilic and hydrophobic segments of a PU-thickener from type A and B have a large influence on rheological behavior of aqueous emulsion paints along a wide range of shear stress.

At very low concentrations, the polyurethane thickener can be considered as monomolecular dissolved in the aqueous phase. With increasing concentration of the polyurethane thickener material, a formation of micelles is observed. The corresponding CMC-values (critical micelle concentration) are relatively low.8,12

A solution of PU-thickener in water can, depending on the quantity and type of polymer used, result in separation of the liquid into a low viscous phase containing only a low concentration of PU-thickener and a comparatively high-viscous phase that is relatively rich in PU-thickener material.8 Additional polymer increases the portion of the highly viscous phase up to the point where the low viscous phase disappears.

This behavior can be interpreted as a tendency of the system to reduce the surface energy of the hydrophobic segments in a polar medium by forming micelles, which are concentrated in one phase.

The binder content of a paint or lacquer formulation is also of great importance for the rheological efficiency of an associative thickener. Figure 7 shows the flow curves of two similar emulsion paints with different binder content but containing the same amount of PU-thickener. Formulations with higher solids (binder) are more sensitive against associative thickening effect.

Reversible Formation of Networks Through Micelles and Hydrophobic Segments

What really does happen in a coating system that normally contains several different components such as latex particles, emulsifiers, wetting agents, surfactants, pigments and extenders etc.?

In various formulations containing water, wetting agent, pigments (TiO2) and extenders, only a weak rheological effect with associative thickeners is observed. At the same time, when a latex emulsion is added to this mixture, the rheological profile increases substantially. Therefore, it can be concluded that the interaction between latex particles and associative thickeners is mainly responsible for a thickening effect in such a system.

If additional amounts of emulsifier or glycol are added to a ready-for-use coating system, there is often a remarkable decrease in the rheological profile, especially in the low shear range. The reason for this could be a displacement of linking groups of the associative thickener from the surface of a latex particle or pigment through the surfactant.

As for the formation of associative structures, i.e. reversible networks, two possible versions are discussed11 (Figure 8):

    a) Formation of hydrophobic clusters, as well as micelles, through the rheological additive.

    b) Association of dispersed particles with the hydrophobic segments of the rheological additive.

Due to the fact that any associative additive has at least two linking groups, reversible networks of either linked micelles or particles would be obtained in any case. Nevertheless, the details of this process are not exactly known. All components of a coating system can interact with each other. A transfer of detailed information of a special system to another coating formulation cannot be made without caution.

Moreover, it is most likely that the dispersed particles in a paint or lacquer formulation have a protective layer, which is normally built up of wetting and dispersion agents. If we assume that the major part of a dispersed particle is blocked with those substances, then it is inevitable that dynamic replacement processes must take place in order to realize a significant association with a PU-thickener and therefore a remarkable thickening effect.

The affinity of both a surfactant and an associative thickener respectively to such a particle surface has a large impact on the rheological efficiency. Therefore, diffusion processes also play an important role in this connection and have to be taken into consideration.

References

1 Prideaux, J. Surf. Coat. Int. 76 (1993) (4), 180-183.

2 Schaller, E.J.; and Sperry, P.R. Handbook of Coatings Additives, Marcel Dekker Inc., New York, Basel, Hong Kong, Vol. 2 (1992), Chap. 4, 105-163.

3 Kaczmarski, J. Ph.; Fernando, R.H.; and Glass, J.E. J. of Coat. Technol. 65 (1993) 818, 39-46.

4 Mavex, T.L. J. of Coat. Technol. 64 (1992) 812, 45-58.

5 Sperry, P.R.; Thibeault, J.C.; and Kostansek, E.C. 11th Proc. Int. Cont. Org. Coat. Sci. Technol., New Paltz, N. Y., 1-11.

6 Bielemann, J.H.; Riesthuis, F.J.J.; and van der Velden, P.M. Polym. Paint Col. J. 176 (June 1986), No. 4169.

7 Naé, H.N.; and Bank, R.H. Rheology 91 (October 1991), 170-178.

8 C. D. Eisenbach et al. Farbe & Lack, 5/2002, S. 44 ff.

9 Nae, H. Polymers Paint Colour J., 183 (4328), 226, 1993.

10 Bielemann, J.H.; Riesthuis, F.J.J.; and v.d. Velden, P.M. Polymer Paint Col. J., 176 (4169), 1986.

11 Hester, R.D.; and Squire, D.R. J. of Coat. Technol., 69 (864), 109, 1997.

12 Pham, Q.T.; Russel, W.B.; Thibeault, J.C.; and Lau, W. Macromolecules 32, 2996-3005, 1999.

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • pci1022-Kinaltek-Lead-1170.jpg

    A Novel Pigment Production Technology

    Following an extensive R&D program that demonstrated...
    Paint and Coating Pigments
    By: Jawad Haidar and Nitin Soni
  • pci global top 10

    2025 Global Top 10: Top Paint and Coatings Companies

    The following is PCI’s annual ranking of the top 10...
    Paint and Coating Market Reports
    By: Courtney Bassett
  • 2025 pci 25

    2025 PCI 25: Top Paint and Coatings Companies

    PCI's annual ranking of the top 25 North American paint...
    Paint and Coating Market Reports
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

Popular Stories

Akzo, SW, Nippon Logos

AkzoNobel Rejects Cash Offer From Nippon Paint, Sherwin-Williams

BASF SE Logo

BASF Announces Strategic Business Sale

AkzoSWNipponEndTalks

Nippon Paint, Sherwin-Williams End AkzoNobel Pursuit

POB-Point-and-Shoot

PCI Buyers Guide

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

Find Suppliers

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

September 15, 2026

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Automotive Paints and Coatings, 2nd Edition

Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

See More Products
Inside the AI Shift in Coatings - See the article now

Related Articles

  • Covaron-Figure-1-900.jpg

    A New Approach to Ceramic Matrix Composites

    See More
  • pci1120-Lumishield-1044079238-900.jpg

    A New Approach to Sustainable Pretreatments for Industrial Coatings

    See More
  • Sherwin-Williams Introduces a New Approach to Colormix® Forecast 2024 2.png

    Sherwin-Williams Introduces a New Approach to Colormix® Forecast 2024

    See More

Related Products

See More Products
  • Hansen Solubility Parameters – A Scientific Approach for Coating Formulators (Virtual Course - 8/20/26)

See More Products

Related Directories

  • BYK USA LLC

    BYK USA is a leading supplier of specialty additives that are used to optimize production and application processes and visibly improve the qualities of the finished products. Additives range: wax additives, adhesion promoters, wetting and dispersing additives, surface additives, defoamers, rheological additives, surfactants, nanotechnology and more.
  • BYK USA

    BYK USA is a leading supplier of specialty additives that are used to optimize production and application processes and visibly improve the qualities of the finished products. Range of additives includes wax additives, adhesion promoters, wetting and dispersing additives, surface additives, defoamers, rheological additives, surfactants, nanotechnology and more.
  • BASF Corp., Dispersions, Resins & Additives

    BASF offers a strong portfolio of industry-leading additives for the Coatings Industry to deliver eco-efficient solutions that meet performance requirements. The BASF Performance and Formulation additives portfolio encompasses a technology base of dispersing agents, wetting agents and surface modifiers, defoamers, rheology modifiers, film forming agents, antioxidants, light stabilizers and UV absorbers.
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing