Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!

ABRAFATI 2003

November 1, 2003
The ABRAFATI 8th International Exhibition in Sao Paulo, Brazil, which was held September 3-5, was amazingly upbeat and showed a 46% increase over the 2001 Exhibition. There were 136 exhibitors and 16,000 visitors, including 416 foreign visitors from 29 countries.

The reason for seeing the high energy level at this exhibition could be the continuous reduction of basic interest rates, the increase in real estate sales, the car tax reduction and the incentives for the procurement of electrical appliances. According to ABRAFATI Executive President Dilson Ferreira, "we had a weak first semester, recording 3% less sales when compared against the same period in 2002. We hope that the first detectable recovery signs can intensify now, not only brought about by the measures taken by the government, but also because the end of the year traditionally registers in Brazil greater demand for paints."

Ferreira believes that the industry can close the year with up to 2% growth. In the year 2002, the Brazilian paint industry invoiced US $1.12 billion, of which 60% corresponded to real estate paints ($672 million), 25% to industrial paints in general ($280 million), 9.02% to automotive repainting ($101 million) and 5.98% to the automotive industry ($67 million).

The industry's production capacity amounts to 1 billion liters of paint per year, and last year the total paint production totaled 857 million liters, divided as follows:

  • 77.36% real estate paints;

  • 15.28% industrial paints in general;

  • 3.5% paints for the automotive industry; and

  • 3.85% paints for automotive re-painting.

    When comparing the years 2001 and 2002, the volume of manufactured paints grew 1.7%, whereas in 1994 (the beginning of the economic "Real Plan), this volume grew 21.4%. Low- and middle-cost paints have been gaining more importance and currently represent over 50% of the total volume, while in 1997 they only accounted for 37%. There are approximately 300 paint and varnish manufacturers. The industry accounts for 16,000 direct jobs and is responsible for approximately 300 thousand indirect jobs, comprising suppliers, distributors and painters.
  • Share This Story

    Looking for a reprint of this article?
    From high-res PDFs to custom plaques, order your copy today!

    Recommended Content

    JOIN TODAY
    to unlock your recommendations.

    Already have an account? Sign In

    • pci1022-Kinaltek-Lead-1170.jpg

      A Novel Pigment Production Technology

      Following an extensive R&D program that demonstrated...
      Paint and Coating Pigments
      By: Jawad Haidar and Nitin Soni
    • pci global top 10

      2025 Global Top 10: Top Paint and Coatings Companies

      The following is PCI’s annual ranking of the top 10...
      Paint and Coating Market Reports
      By: Courtney Bassett
    • 2025 pci 25

      2025 PCI 25: Top Paint and Coatings Companies

      PCI's annual ranking of the top 25 North American paint...
      Paint and Coating Market Reports
      By: Courtney Bassett
    You must login or register in order to post a comment.

    Report Abusive Comment

    Manage My Account
    • eMagazine
    • Newsletters
    • Online Registration
    • Subscription Customer Service

    More Videos

    Sponsored Content

    Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

    close
    • wooden kitchen set and shelving
      Sponsored bySirca North America

      Leveraging Coatings to Meet ESG Goals in Manufacturing

    • man woodworking in workshop
      Sponsored byGemini Industries, Inc.

      Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

    Popular Stories

    Akzo, SW, Nippon Logos

    AkzoNobel Rejects Cash Offer From Nippon Paint, Sherwin-Williams

    BASF SE Logo

    BASF Announces Strategic Business Sale

    AkzoSWNipponEndTalks

    Nippon Paint, Sherwin-Williams End AkzoNobel Pursuit

    POB-Point-and-Shoot

    PCI Buyers Guide

    Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

    Start your RFP

    Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

    Find Suppliers

    Events

    September 4, 2025

    N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

    ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

    September 15, 2026

    Coatings Trends & Technologies Summit

    The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

    View All Submit An Event

    Poll

    Longest-running laboratory experiment

    What is the longest-running laboratory experiment?
    View Results Poll Archive

    Products

    Automotive Paints and Coatings, 2nd Edition

    Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

    See More Products
    Inside the AI Shift in Coatings - See the article now

    Related Articles

    • Coatings Industry Report for 2003

      See More
    • Crossword Answers (October 2003)

      See More
    • Coating 2003

      See More
    ×

    Keep the info flowing with our eNewsletters!

    Get the latest industry updates tailored your way.

    JOIN TODAY!
    • RESOURCES
      • Advertise
      • Contact Us
      • Directories
      • Store
      • Want More
      • Manufacturing Division
    • SIGN UP TODAY
      • Create Account
      • eMagazine
      • Newsletters
      • Customer Service
      • Manage Preferences
    • SERVICES
      • Marketing Services
      • Reprints
      • Market Research
      • List Rental
      • Survey & Sample
    • STAY CONNECTED
      • LinkedIn
      • Facebook
      • Youtube
      • X (Twitter)
    • PRIVACY
      • PRIVACY POLICY
      • TERMS & CONDITIONS
      • DO NOT SELL MY PERSONAL INFORMATION
      • PRIVACY REQUEST
      • ACCESSIBILITY

    Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

    Design, CMS, Hosting & Web Development :: ePublishing