Effective Feb. 1, 2010, DSM NeoResins+ will increase prices in the North American region for NeoCryl™ waterborne acrylic resins and for beads $0.05 to $0.08 per pound, depending on the product line.
BOSTON, MA - Effective Feb. 1, 2010, DSM NeoResins+ will increase prices in the North American region for NeoCryl™ waterborne acrylic resins and for beads $0.05 to $0.08 per pound, depending on the product line. The price increase affects the entire Coating Resins and Graphic Arts portfolio.
BOSTON, MA - Effective Feb. 1, 2010, DSM NeoResins+ will increase prices in the North American region for NeoCryl™ waterborne acrylic resins and for beads $0.05 to $0.08 per pound, depending on the product line. The price increase affects the entire Coating Resins and Graphic Arts portfolio.