Global Coatings Market: $99 Billion in 2011

LONDON – In 2010, the global coating market hit about $90 billion and is expected to grow about 10 percent to $99 billion in 2011. This information is presented in “Global and China Coating Industry Report, 2010-2011,” a new research report developed by ResearchInChina that has been recently published by Market Publishers Ltd. 

Decorative coatings is the largest application area, accounting for approximately 45 percent of the total market, followed by vehicle coating, making up roughly 15 percent, and protective and marine coating (PMC), accounting for about 12 percent. General industrial coatings stand at roughly 10 percent, followed by powder coatings, wood coatings, coil coatings and packaging coatings. 

According to the report, China is the world's largest market for coatings, with a value of $18.9 billion in 2011. Of that, 54 percent was attributed to decorative coatings. The report estimates that an expected rebound in China’s real estate market will increase the value of the decorative coatings market to over $12 billion. 

The study reports that while China is the world’s largest market for coatings, its domestic coatings production is relatively small. While the number of domestic coatings companies is over 2,500, revenue from these companies only accounts for about 11 percent of the total Chinese coatings market. Guangdong Carpoly Chemical Co. Ltd., the largest domestic coatings company, is expected to report 2011 revenue of roughly $350 million. 

For additional information about the report, visit http://marketpublishers.com.

You must register or login in order to post comments.

Multimedia

Videos

Image Galleries

American Coating Show 2012

The American Coatings Show and Conference, held every two years, took place May 7-10 at the Indiana Convention Center in Indianapolis, IN, in the heart of the Manufacturing Belt, the oldest and largest concentration of industrial companies in the Midwest.

Podcasts

PCI Top 5 - January 12, 2012
PCI's Podcast series on the five most e-mailed/shared articles and stories for the week.

More Podcasts

THE MAGAZINE

PCI Magazine

PCI may 2012 cover

2012 May

Check out PCI's May issue!!

TABLE OF CONTENTS SUBSCRIBE

iPad

Do you own/use an iPad?
If yes, do you use your iPad for business or personal reasons?
Have you purchased a business app within the last 6 months?
See Poll Results Poll Archive

THE PCI STORE

PCI-June-2011-Coversmall.gif
PCI Additives Handbook

Encyclopedia of information on the properties and uses of coatings additives.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

Virtual Brochures

PageCollageClick on the Virtual Brochures page to view multiple categories that list downloadable product literature from leading industry suppliers.

STAY CONNECTED

Facebook Twitter  LinkedIn YouTube