Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!
FT Archives

Powder on Plastics

June 1, 2005
Alliance Surface Finishing puts powder on a wide range of plastics used in many markets, including office furniture.
For years, the high temperatures involved with powder coating, along with the need to make parts electrically conductive, have posed seemingly insurmountable obstacles to the possibility of powder on plastic parts. This is no longer the case for Robert Langlois, owner of Alliance Surface Finishing. In June 2001, Langlois saw the possibilities for powder in the wide range of plastics used to manufacture parts for the office furniture, automotive, appliance and electronics markets.

He says he knew how important it was that manufacturers produce a quality finished part for a lower bottom-line cost. Langlois' background in physical vapor deposition gave him a feel for trends in coatings. Bringing together varying technologies, Langlois developed a pretreatment process to make plastic more conductive as it is cleaned for powder coating. "We patented our proprietary ‘magic solution,'" says Langlois.

Pretreatment in hand, Langlois worked with Nordson (headquartered in Westlake, Ohio) and PPG (headquartered in Pittsburgh) to develop the rest of the solution in the Canadian laboratories of Nordson Corp., Markham, Ont.

Paul Kroes, Nordson's Canadian sales manager, says that there was a huge learning curve to overcome because spraying powder on plastics was new turf. "ASF documented every step of the process, and built a tremendous database of knowledge to succeed," he says.

The powder coatings for the Alliance Surface Finishing project were exclusively developed and supplied by PPG Industries in its Strongsville, Ohio, facility. "Our chemists in Allison Park (Pennsylvania) had been developing much of this technology for some time," says Paul Mills, PPG's marketing manager for heat-sensitive substrate powder coatings. He says PPG was able to transfer this technology to the Alliance project to give Robert and the Nordson team materials formulated for the plastics they were using.

For Alliance, these plastics include a range of materials from PBT and nylons to blends of these materials along with higher temperature versions of Lexana and polycarbonate. "We believed that manufacturers would switch to higher temperature plastics to get a better product at a better price," says Langlois. "The overall results can demonstrate it is worth a conversion."

Alliance has had a full plate of coating opportunities since installing its pilot line in Vaughan, Ont. The trial work and commercial production achieved at Vaughan has been so successful that Langlois has opened a second facility, an 80,000 ft2 production site in nearby Mississauga. Shannon Matwey, director of business development, says there is enough demand in the United States to warrant the possibility of opening two coating facilities stateside.

"The days of the all-black office chair are numbered," says Kevin Mehring, director of sales and marketing at Alliance. "We've introduced a new way of thinking about color and texture to an industry that had been forced to think in terms of limited choices of molded-in color technology." Mehring, who worked for PPG on the project, is excited about the opportunities at ASF. "[We] are paving new ground, and the market is responding enthusiastically."

"We've worked hard to develop a set of tools that help us coat a wide range of materials and shapes," says Alliance's vice president of operations, Alan Stokes. "As a custom coater, we need a process that's both flexible and robust, that gives us capability to paint every part a customer sends to us, regardless of size or configuration."

For powder coating flexibility, Stokes has worked closely with Nordson to implement a powder system with significant features that make it ideal for custom coating. "The iControl System is the ‘brain' of our powder coating line, allowing recall of stored recipes of gun settings and booth parameters that get us 90 percent of the way there within a few minutes," says Stokes. "Then we can fine tune the recipe for the variations of a new job."

The Alliance pilot system, which consists of two Nordson chain-on-edge spray booths, allows technicians to coat parts both automatically and manually using oscillating guns mounted on variable-position bases. Alliance's new production facility also combines automatic and manual capabilities, along with the advanced iControl system package.

"From the outset, we believed a pilot facility needed to be just that," says Langlois. "We didn't skimp with something that could be just scaled up a bit for production; using other technology and taking short cuts. For us it was clear that the work we did in developing this technology would need to be scaled up quickly when customers saw how well it works.

Langlois says that the pilot line in Vaughan paved the way for ASF to begin operation in Mississauga "without missing a beat."

For information about Alliance Surface Finishing, call 866-749-4273 or visit www.asf-powder. com. For information on Nordson, call 440-892-1580 or visit www.nordson.com. For more on PPG, call 412-434-3131 or visit www.ppg.com.

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • pci1022-Kinaltek-Lead-1170.jpg

    A Novel Pigment Production Technology

    Following an extensive R&D program that demonstrated...
    Paint and Coating Pigments
    By: Jawad Haidar and Nitin Soni
  • pci global top 10

    2025 Global Top 10: Top Paint and Coatings Companies

    The following is PCI’s annual ranking of the top 10...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • 2025 pci 25

    2025 PCI 25: Top Paint and Coatings Companies

    PCI's annual ranking of the top 25 North American paint...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

Popular Stories

Akzo, SW, Nippon Logos

AkzoNobel Rejects Cash Offer From Nippon Paint, Sherwin-Williams

BASF SE Logo

BASF Announces Strategic Business Sale

AkzoSWNipponEndTalks

Nippon Paint, Sherwin-Williams End AkzoNobel Pursuit

POB-Point-and-Shoot

PCI Buyers Guide

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

Find Suppliers

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

September 15, 2026

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Automotive Paints and Coatings, 2nd Edition

Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

See More Products
Inside the AI Shift in Coatings - See the article now

Related Articles

  • Research Explores Effect of Electron Beams on Plastics - Posted 2/13/08

    See More
  • pci0220-Allnex-468495842-900.jpg

    UV Coatings on Plastics

    See More
  • New Resins for Durable Coatings on Plastics

    New Resins for Durable Coatings on Plastics

    See More

Related Products

See More Products
  • Powder Coatings Processing (Virtual Course - 6/25/26)

  • marketsandmarketslogo.jpg

    Metallic Powder Coatings Market by Process Type (Bonding, Blending, Extrusion)...

See More Products

Related Directories

  • Micro Powders

    Micro Powders' additives solve problems and achieve unique coating surface effects including: slip; rub, abrasion, and scratch resistance; gloss reduction, burnish resistance; water repellency; texture, tactile, and soft touch effects. We are leaders in creating innovative particle technologies, including natural/biodegradable grades and nanocomposite wax PTFE alternatives.
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing