LODI, NJ – According to the consulting firm Kusumgar, Nerlfi & Growney, coating biocide consumption in Asia was 30 million pounds, worth $174 million in 2008. Growth, led by China and India, is placed at 9 percent per year through 2013. In-can preservatives and dry-film fungicide consumption was 23 million pounds, worth $97 million, and is growing 9 percent per year. Over 90 percent of these biocides are consumed in water-based architectural paints. Growth in architectural paints will be down significantly in 2009 due to the slumping economies in the region.

Marine fungicide consumption in Asia, excluding cuprous oxide, was just over 7 million pounds, worth $77 million in 2008. An 8-percent annual rate of growth is forecast. Shipbuilding and repair activity is forecast to remain strong over the next couple of years, but the recent drop-off in global ship orders will cause marine biocide growth to slow in the latter part of the five-year forecast. The long-term outlook is dependant on the recovery of world trade.
You must register or login in order to post comments.

Multimedia

Videos

Image Galleries

American Coating Show 2012

The American Coatings Show and Conference, held every two years, took place May 7-10 at the Indiana Convention Center in Indianapolis, IN, in the heart of the Manufacturing Belt, the oldest and largest concentration of industrial companies in the Midwest.

Podcasts

PCI Top 5 - January 12, 2012
PCI's Podcast series on the five most e-mailed/shared articles and stories for the week.

More Podcasts

THE MAGAZINE

PCI Magazine

PCI may 2012 cover

2012 May

Check out PCI's May issue!!

TABLE OF CONTENTS SUBSCRIBE

iPad

Do you own/use an iPad?
If yes, do you use your iPad for business or personal reasons?
Have you purchased a business app within the last 6 months?
See Poll Results Poll Archive

THE PCI STORE

PCI-June-2011-Coversmall.gif
PCI Additives Handbook

Encyclopedia of information on the properties and uses of coatings additives.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

Virtual Brochures

PageCollageClick on the Virtual Brochures page to view multiple categories that list downloadable product literature from leading industry suppliers.

STAY CONNECTED

Facebook Twitter  LinkedIn YouTube