Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Join Today
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • PCI News Now
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • JOIN!

Environmentally Friendly Corrosion-Protective Polyester Resins for Powder Coatings

By Dana Ionescu, Eric Blokhuizen, Paul Vercoulen, Marcel Schutte
March 3, 2009
DSM Uralac® Corres opens a new window of opportunity for corrosion-protective coatings.



Powder coatings are increasingly preferred over conventional solventborne and waterborne coatings. These types of coatings offer a high environmental advantage and, in addition, they are key to the economic benefit in the coating process. One of the reasons is that powder coatings are 100% solid, solvent-free materials that process with close to 100% utility. Even more important is their high technical performance.

Corrosion Protection

As the global market leader, DSM Powder Coating Resins specializes in the innovation, development and manufacture of polyester resins for powder coatings. Corrosion-protective powder coatings, based on environmentally friendly polyester, are a new DSM development in line with the company strategy on sustainability. Coatings are the primary solution to prevent corrosion of metal, and steel is the most commonly used metal. Depending on the environment where the product is in use, it needs protection from corrosion.

Uralac® Corres

Uralac® Corres is especially developed for corrosion protection on steel and can be used in many market segments. The main target segments range from thin, flat steel applications like metal furniture, shelving, heating/ventilation and domestic appliances to equipment, automotive parts and even heavy steel applications like ACE and construction beams. Corrosion protection is needed for every single application; depending on the expected lifetime and conditions of use it has its own specified requirements.

Industry Requirements



Direct Comparison Study

To support and prove the above claims, DSM ran a direct comparison with common powder coating systems. Uralac® P 7604 Corres was applied on R 46 Q-panels and compared after a 480 h natural salt spray test according to ISO 9227 with standard references like a pure epoxy, a 70/30 hybrid and a 95/ Primid system. Figure 2 clearly shows the good performance of Uralac® Corres P 7604 Corres against all three references.

In addition to passing the industry requirements, DSM used analytical tools to support its theory on the enhanced barrier properties.

Resistance Monitoring

To support the practical results on salt spray, the Dutch research and test institute TNO Science & Industry Den Helder monitored the resistance against corrosion with Electrochemical Impedance Spectroscopy (EIS). The EIS technique determines the anti-corrosive properties of a coating. This is done by measuring the resistance to an alternating current in an electrochemical cell system. The higher the measured coating resistance, the better the anti-corrosion performance.

Figure 3 shows that the anti-corrosive performance of Uralac® Corres remains good before and after the natural salt spray test, and is better than the tested reference systems. The high resistance values, also in comparison with TNO industry classification, support the theory on the high barrier against corrosion of the Uralac® Corres polyester. Due to the exceptionally good corrosion protection in metal coating, the Uralac® Corres technology offers the possibility to significantly reduce and sometimes completely eliminate chemical pre-treatment steps.



Figure 4 illustrates the reduction in process steps for a nine-stage iron phosphate pretreatment process compared to a simple cleaning process needed for Uralac® Corres.

In addition to the good technical performance, Uralac® Corres can save production space and reduce new investments especially for new lines.

Environmental Impact

Because Uralac® Corres significantly reduces or completely eliminates pretreatment steps it removes the usage of environmentally hazardous chemicals. Uralac® Corres fulfills all requirements up to 480 h NSS without any pretreatment. This is a 100% saving on hazardous phosphate chemicals, a significant risk reduction in handling and waste disposal related to the phosphate chemicals. It translates to a better work environment.

Conclusion

With high-performance corrosion protection and an ability to eliminate pretreatment steps and replace epoxy-based primers in the coating process, DSM Uralac® Corres opens a new window of opportunity for corrosion-protective coatings. DSM Powder Coating Resins continues to contribute with its cutting-edge innovation to the development of the coating industry.

For more information about the current and future portfolio of DSM Powder Coating Resins, visit www.dsmpowdercoatingresins.com, or contact your local account manager.

This article was first published in PPCJ, October 2008.

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

DSM Powder Coating Resins, The Netherlands
DSM Powder Coating Resins, The Netherlands
DSM Powder Coating Resins, The Netherlands
DSM Powder Coating Resins, The Netherlands

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • Double exposure of creative chemistry concept on laptop background, research and development concept

    Inside the AI Shift in Coatings

    Industry leaders share real-world examples of how AI is...
    Paint and Coating Equipment
    By: PCI Editorial Staff
  • Global Top 10 and PCI Logo

    2026 Global Top 10: Top Paint and Coatings Companies

    See how the world’s largest paint and coatings companies...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • The 2026 PCI 25

    2026 PCI 25: Top Paint and Coatings Companies

    See how North America's largest paint and coatings...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • Join Paint & Coatings Industry
  • Manage My Preferences
  • Customer Service

More Videos

Popular Stories

Mergers and aquisitions

Evonik Holds Off on BASF Takeover Talks

industry news

Dozens Treated After Toledo Chemical Release

Breaking News

H.B. Fuller to Close Seven Sites in Supply-Chain Overhaul

Events

November 19, 2026

Reformulating Paints with AI: Turn Change into a Competitive Advantage

Join industry leaders and experts for real case studies showing how AI helps R&D teams use existing paint formulation and test data to evaluate alternatives, predict trade-offs, and prioritize experiments.

December 10, 2026

PC Academy: Waterborne Polymers and Film Formation

The trend towards waterborne polymers in the paint and coatings industry is clear; highlighting their environmentally friendly nature, regulatory considerations, growing market demand, and meeting sustainability goals.

View All Submit An Event

Products

Powder Coatings - Foundation for the Novice Formulator (ebook)

Powder Coatings - Foundation for the Novice Formulator (ebook)

See More Products
PCI news now promo ad

Related Articles

  • resins, powder coatings

    Crosslinker Resins for Powder Coatings

    See More
  • Resins for Powder Coatings from Arkema Inc.

    See More
  • Sustainable Polyesters for Powder Coatings

    See More

Related Products

See More Products
  • Kevin-Biller-PC-BOOK.jpg

    Powder Coatings - Foundation for the Novice Formulator (ebook)

  • marketsandmarketslogo.jpg

    Metallic Powder Coatings Market by Process Type (Bonding, Blending, Extrusion)...

See More Products

Events

View AllSubmit An Event
  • November 5, 2026

    Advancing Polyester Powder Coatings: Breakthroughs in Flexibility and Low-Cure Performance

    On Demand This webinar will explore two advancements in polyester powder coating technology designed to address these distinct challenges.
View AllSubmit An Event

Related Directories

  • SUN POLYMERS International Inc.

    Sun Polymers manufactures and supplies specialty resins, curing agents, and additives for powder coatings. Sun Polymers provides polyester resins to powder coating manufacturers in a manner that is wide ranging, consistent in quality, and environmentally friendly. Sun Polymers also sells resins manufactured by our parent company, Chan Sieh Enterprises, including a wide range of acrylics, waterborne, and solvent borne resins.
  • SUN POLYMERS International Inc.

    Sun Polymers manufactures and supplies specialty resins, curing agents, and additives for powder coatings. Sun Polymers provides polyester resins to powder coating manufacturers in a manner that is wide ranging, consistent in quality, and environmentally friendly. Sun Polymers also sells resins manufactured by our parent company, Chan Sieh Enterprises, including a wide range of acrylics, waterborne, and solvent borne resins.
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Manufacturing Division
  • JOIN TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing