Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!
FT Archives

Faster, Friendlier and Fewer Rejects

April 28, 2004
When an automotive supplier needed a new finishing system, it turned to 100%-solid UV coatings. The company increased productivity while reducing defects and VOCs.

The spray booth at Unit Parts, an automotive parts supplier, incorporates stainless-steel baffles to collect most of the overspray, which is recycled. (Photos courtesy of Nutro Corp.)
Unit Parts, a major automotive aftermarket supplier of starters and alternators in Oklahoma City, was looking for a cost-effective and environmentally friendly solution for its finishing needs. Unit Parts had several goals: improve the aesthetic quality of its coating, eliminate or reduce VOCs from the painting process and double painting capacity.

Mike Jones, Unit Parts' director of process coating and finishing, was given the task of investigating and ultimately recommending a solution. Based on his previous experience in the paint industry and ownership of a powder coating shop, Jones' first instinct was to install a powder line and benefit from the positive features of powder coating technology, namely ease of application, environmental friendliness, and the ability to reclaim and reuse the powder.

However, there were challenges with installing a powder coating system. A conventional powder system would have required installing the cure oven and cooling tunnel on the roof of the facility due to floor space limitations. A powder system would also have required much more work in process (approximately 40 minutes total cycle time) than the company's conventional coating system. In addition, there were concerns about a production bottleneck. The system would not allow Unit Parts to process its heat-sensitive subassemblies, another transition from its current process.

In 1999, Jones attended the Finishing Show in Cleveland, looking for paint options other than powder. At the show, he was exposed to 100%-solid UV-pigmented coatings. A manufacturer of 100%-solid UV coating introduced Jones to its coating technology, which led him to re-evaluate the decision to install a new powder system.

Figure 1: Typical UV-Liquid Finishing System

100%-solid UV coatings

100%-solid UV coatings are cured using various wavelengths of ultraviolet light. UV coatings are formulated with 100%-solid reactive liquid vehicles, such as oligomers, monomers, photoinitiators, additives, resins and catalysts. A unique feature of 100%-solid coating is that the wet-film thickness is close to the dry-film thickness when cured. The monomers and oligomers react within the coating rather than flash off the coating. Pigments may be applied to the coating to color match practically any color, with the exception of a few shades of yellow and orange.

Considerations for handling UV coatings revolve around the fluid delivery and surrounding atmosphere where the coatings will be applied. All wetted components in the fluid stream must be made of stainless steel or Teflon. Fluid lines should be opaque, and light sources should be filtered where exposure of the coating is possible. UV coatings are shear-sensitive and are not compatible with piston or gear pumps.

In addition, variation in coating temperature may have an adverse effect on applying paint to the substrate. Cooler temperatures may raise the viscosity, making it difficult to atomize and apply the proper film build. Heating the material slightly above ambient temperature helps alleviate variation in outside temperature.

The UV chamber was designed to be large enough to allow operators easy access to the lamps.

Selecting UV coatings

100%-solid UV coatings were selected because of their low-temperature process, low VOCs and instantaneous cure time. The low-temperature process is ideal for heavy metallic parts, which would typically require a long cool-down time if cured in a conventional thermal oven. Moreover, temperature-sensitive components on internal assemblies are not affected.

Other benefits of UV coating are its high abrasion and stain-resistance properties. Unit Parts' finished product was subjected to multiple processes after coating and had to be durable enough to withstand handling. Finally, the part had to look superior to the competition's part. 100%-solid UV coatings provided Unit Parts the finished product it was looking for.

"I recognized that UV technology was on the cutting edge," Jones says. "I knew that there would be a lot of R&D dollars involved and that the technology would advance very quickly. We wanted to get in, get situated and then wait for the technology to catch up."

Developing the process

Unit Parts conducted preliminary testing at two equipment suppliers' facilities. Coating samples from two different vendors were evaluated at each facility. Testing was required to determine the film thickness needed to achieve the customer's performance properties. Lamp suppliers were involved in the testing to match the correct wavelength of the bulb with the photoinitiator in the coating.

The testing was conducted on a portable chain-on-edge system. Once the preliminary testing was conducted, Unit Parts assembled the team that would be responsible for implementing the technology at its facility.

Flexible mounting allows Unit Parts to add capacity.

The final process

Once the parts are manually loaded onto the conveyor, they enter the spray booth and are rotated in front of a rotary atomizer. The spray booth design incorporates stainless steel baffles to collect the majority of overspray coating. The overspray is collected in a stainless steel trough and then pumped into a container for recycling.

UV materials may be applied with a wide variety of application equipment. Unit Parts chose a rotary atomizer for its application. A rotary atomizer uses centrifugal force to atomize the coating, which is essential due to the typical high viscosity of 100%-solid UV coatings. The rotary atomizer also uses electrostatics to yield high transfer efficiency to the substrate, minimizing waste.

A heated, recirculating fluid-delivery system was used to maintain proper viscosity of the paint independent of the plant temperature. The paint was heated slightly higher than typical summer ambient temperatures. Once the parts are coated, they immediately enter the UV chamber where they are cured with four lamps within several seconds. The UV chamber was designed to be large enough to allow operators easy access to the lamps and to provide a window for viewing the parts.

Unit Parts chose microwave lamps because of their reliability and extended bulb life. Flexible mounting provides Unit Parts the ability to add additional capacity to the system based on line speed and part geometry.

Once the parts are cured, they exit the UV chamber through a shrouded chamber that provides a safe working environment for the operators. The finished product is cured and ready to be unloaded. The parts are then manually unloaded and placed in dunnage prior to final assembly.

A typical UV-liquid finishing system is depicted in Figure 1 (page 17). The total cycle time is less than four minutes from load to unload. The system consumes approximately 800 square feet of floor space, approximately 10 times less than a typical powder system with the same capacity.

Since installing the new system, Unit Parts has reaped the rewards of adopting 100%-solid UV liquid coatings. Production has more than doubled, paint defects have been reduced from 12% to less than 1/10th of one percent, and VOCs have been dramatically reduced in the painting process. More importantly, Unit Parts is supplying its customers with a superior coated product.

"UV curing is very reliable," Jones says. "We have had excellent results, as far as rejects. The system is very repeatable from hour to hour, day to day, week to week. We can come in on Monday morning after a weekend of being shut down, turn on the system and have it run just as it did on Friday when we shut it off."

Dennis Kaminski is an account manager for Nutro Corp. Reprinted with permission from RadTech International North America, RadTech Report.

Sidebar: Is It Safe?

UV/EB materials are increasingly being used in a wide variety of automotive operations. They typically are much less toxic than some of the ingredients in waterborne or solventborne systems that they replace.

They have a very high or no flashpoint, emit little to no VOCs, have very low systemic toxicity, as a class are not carcinogens (recent long-term skin painting tests showed no carcinogenic effect, and the test materials showed no systemic toxicity), and are not fetal or reproductive toxins. Moreover, UV-curing materials are not readily absorbed through the skin like solvents. And since these materials have very low vapor pressures, hazards due to inhalation are less likely.

Nevertheless, as in the case of other types of industrial coatings, certain regulations aimed at assuring worker safety do apply when handling UV/EB materials. Additional specialized requirements apply to automotive OEM and refinish coatings. The following references are recommended for further review:

29 CFR § 1910.1200-Hazard Communication

29 CFR § 1910 Subpart I-Personal Protective Equipment

29 CFR § 1910.134-Respiratory Protection

29 CFR § 1910.123-Dipping and coating operations

29 CFR § 1910.124-General requirements for dipping and coating operations

29 CFR § 1910.125-Additional requirements for dipping and coating operations that use flammable or combustible liquids

29 CFR § 1910.126-Additional requirements for special dipping and coating operations

-Ron Golden, Surface Specialties-UCB, and Martha Marrapese, a partner with the law firm of Keller and Heckmal LLP, from the RadTech Report.

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • pci1022-Kinaltek-Lead-1170.jpg

    A Novel Pigment Production Technology

    Following an extensive R&D program that demonstrated...
    Paint and Coating Pigments
    By: Jawad Haidar and Nitin Soni
  • pci global top 10

    2025 Global Top 10: Top Paint and Coatings Companies

    The following is PCI’s annual ranking of the top 10...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • 2025 pci 25

    2025 PCI 25: Top Paint and Coatings Companies

    PCI's annual ranking of the top 25 North American paint...
    Paint and Coating Market Reports
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

Popular Stories

Akzo, SW, Nippon Logos

AkzoNobel Rejects Cash Offer From Nippon Paint, Sherwin-Williams

BASF SE Logo

BASF Announces Strategic Business Sale

AkzoSWNipponEndTalks

Nippon Paint, Sherwin-Williams End AkzoNobel Pursuit

POB-Point-and-Shoot

PCI Buyers Guide

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

Find Suppliers

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

September 15, 2026

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Automotive Paints and Coatings, 2nd Edition

Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

See More Products
Inside the AI Shift in Coatings - See the article now

Related Articles

  • Reducing Rejects with Color Verification

    See More
  • Faster E-Coating with Advanced Ultrafiltration

    See More
  • ICI Rejects Akzo Nobel Takeover Bid - Posted 6/20/07

    See More

Related Products

See More Products
  • marketsandmarketslogo.jpg

    Metallic Powder Coatings Market by Process Type (Bonding, Blending, Extrusion)...

See More Products
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing