Painting & Coating Industry (PCI) logo Powder coating summit logo
  • Sign In
  • Create Account
  • Sign Out
  • My Account
  • NEWS
  • PRODUCTS
  • MATERIALS
  • TECHNOLOGIES
  • RESOURCES
  • EVENTS
  • DIRECTORIES
  • EMAGAZINE
  • CONTACT
  • SIGN UP!
cart
facebook twitter linkedin youtube
  • NEWS
  • Latest News
  • Market Trends & Reports
  • Finishing News
  • Price Alerts
  • Subscribe to eNewsletters
  • Global Top 10/ PCI 25
  • Weekly Featured Article
  • COATLE Word Game
  • PRODUCTS
  • Product News
  • Must See Products and Services
  • MATERIALS
  • Additives
  • Resins/Polymers
  • Pigments
  • Equipment
  • Distributors
  • TECHNOLOGIES
  • Adhesives
  • Architectural Coatings
  • Finishing Articles
  • Finishing Technologies
  • Finishing Equipment
  • Industrial Coatings
  • Nanotechnology
  • Powder Coatings
  • Solventborne
  • Special Purpose Coatings
  • Sustainability
  • UV Coatings
  • Waterborne
  • RESOURCES
  • Columns
  • Blogs
  • Coatings Supplier Handbook
  • Podcasts and Videos
  • PCI Store
  • Classifieds
  • eBooks
  • Sponsor Insights
  • White Papers
  • COATLE Word Game
  • Columns
  • Did you know?
  • Distribution Dive
  • Formulating With Mike
  • Innovation Insights
  • Powder Coating Perspectives
  • TiO2 Insider
  • Blogs
  • Editor's Viewpoint
  • Industry Insights
  • Podcasts and Videos
  • COAT-IT! Podcast
  • Videos/PCI TV
  • EVENTS
  • Coatings Trends & Technologies Summit
  • Paint and Coatings Academy
  • Webinars
  • Calendar of Events
  • Lifetime Achievement Award
  • DIRECTORIES
  • Buyer's Guide
  • Equipment Directory
  • Materials Directory
  • EMAGAZINE
  • Current Issue
  • eMagazine Archive
  • China Issue Archive
  • Editorial Advisory Board
  • CONTACT
  • Contact Us
  • Advertise
  • Subscribe to eMagazine
  • Subscribe to eNewsletters
Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to eNewsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to eNewsletters
  • SIGN UP!
FT Archives

Powder Coating: Enhancing Powder Adhesion on Aluminum

By Rodger Talbert
October 1, 2004

Enhancing Powder Adhesion on Aluminum

We apply powder coatings to HRS steel and extruded aluminum parts that are used outdoors. We use a five-stage washer with a cleaner, rinse, phosphate, rinse and rinse seal. We also use a blast system for the heavy steel parts. The steel product is working out fine, as long as we have good coverage and the correct film build. But we are having trouble with adhesion in the field on the aluminum. We do a crosshatch adhesion test on a regular basis and we always pass. But after the product has been used for a while the adhesion fails. Are there any chemical additives that will enhance adhesion on aluminum?

The challenge in preparing aluminum for powder is the oxide layer that is normally present on the surface. You did not say it, but most spray washers that are set up for multimetals use a fluoride additive in the phosphate solution to etch the aluminum surface and remove the oxide layer. This can be effective for products that are used indoors, but it is usually not sufficient for products that will be subjected to an outdoor environment.

Since there is no conversion coating applied, the surface can begin to oxidize very quickly after it is cleaned and dried, and the powder will not adhere if the part is exposed to moisture and sunlight. Aluminum that is treated in its own process without concern for running steel can be effectively prepared using a chrome seal rinse, a chromate or a dry-in-place nonchrome sealer designed for aluminum. Any of these processes will prevent the reformation of oxide on the aluminum and provide long-term adhesion.

Here are three suggestions for you:

Start coating the hot-rolled steel parts with the blast system and no additional cleaning step. Make sure that the dust from the blast process is blown off, and make sure that your film build is at least three mils thick in all areas. The iron phosphate coating adds marginal additional corrosion protection and is not needed if the surface is completely dry, free from soil, grease, and dust, and has a good, roughened surface to enhance adhesion.

Change the washer over to use a dry-in-place nonchrome seal rinse. If your current supplier does not have this type of product, you should shop for someone who does.

To confirm proper adhesion on aluminum, you should change the procedure. A boiling water adhesion test as described in the American Architectural Manufacturers Association (AAMA) specifications is more conclusive. Prepare the surface as you would for a normal dry adhesion test. Then place the test panel into boiling (210 to 212°F) DI or distilled water for 20 minutes. Remove the test panel, dry it off and then do your tape pull. This is a much more severe test than the dry test, and it will more accurately predict field failure.

Unwanted Moisture in the Lines

We have an air dryer in line to take moisture from our compressed air, and we use coalescing filters. We still seem to get some moisture through the lines. What are we missing?

There could be several reasons why the current system is not properly removing moisture from the lines. For example, the dryer or filters may be undersized or in need of replacement or repair. But the first thing that you should check is the distance between the air dryer and the outlet at the booth. If you have a long run of pipe from the dryer to the booth, you can get moisture in the line from condensation. Adding a high-quality coalescing filter at the booth can help if this is the problem. Have a qualified compressor supplier evaluate your system for flaws.

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Editorial Director, Industrial Paint & Powder

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • pci1022-Kinaltek-Lead-1170.jpg

    A Novel Pigment Production Technology

    Following an extensive R&D program that demonstrated...
    Paint and Coating Pigments
    By: Jawad Haidar and Nitin Soni
  • pci global top 10

    2025 Global Top 10: Top Paint and Coatings Companies

    The following is PCI’s annual ranking of the top 10...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • 2025 pci 25

    2025 PCI 25: Top Paint and Coatings Companies

    PCI's annual ranking of the top 25 North American paint...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • eNewsletter
  • Online Registration
  • Subscription Customer Service

The Coatings Minute: CTT 2025  -  One Summit, Three Audiences, Real Impact

The Coatings Minute: CTT 2025 - One Summit, Three Audiences, Real Impact

The Coatings Minute: Your Guide to the 2025 Coatings Supplier Handbook

The Coatings Minute: Your Guide to the 2025 Coatings Supplier Handbook

The Coatings Minute: Your Inside Look at PCInnovations

The Coatings Minute: Your Inside Look at PCInnovations

The Coatings Minute: See Who’s Leading the Coatings Industry in 2025

The Coatings Minute: See Who’s Leading the Coatings Industry in 2025

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • Modern arapartment complex painted in bright colors.
    Sponsored byEPS - Engineered Polymer Solutions

    Architectural Polymers Leading the Way in Coatings Innovation

  • paint sprayer in a workshop
    Sponsored byallnex

    Enabling Performance and Compliance: allnex Introduces a New Line of VOC Exempt Solvent-Borne Resins

Popular Stories

basf

BASF Advances Coatings Division Sales Talks

The White House in Washington DC at summer day.

Trump Grants HON Rule Exemption to Dow and Others

BCF Logo

EU Court Delivers Crucial TiO<sub>2</sub> Decision



PCI Buyers Guide

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

Find Suppliers

Events

September 3, 2025

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

September 4, 2025

Real-World Successes in AI-Enabled Coatings Innovation

Artificial intelligence is unlocking entirely new opportunities and business models for enterprise R&D organizations.

View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

CTT Summit Short Courses (Live 9/3/25)

Coatings Trends & Technologies Summit is expanding its offerings with four short courses. These short courses will offer an extensive day of interactive learning.

See More Products
pci voices from the top ebook

PCI CASE EBOOK

Related Articles

  • Powder Coating on Aluminum Extrusion

    See More
  • Powder Coating 2004 Focuses on What Powder Coating Can Do For You

    See More
  • ask joe powder pci

    Ask Joe Powder: What is the Best Way to Degrease Steel and Aluminum Prior to Coating?

    See More

Related Products

See More Products
  • Kevin-Biller-PC-BOOK.jpg

    Powder Coatings - Foundation for the Novice Formulator (ebook)

  • marketsandmarketslogo.jpg

    Metallic Powder Coatings Market by Process Type (Bonding, Blending, Extrusion)...

See More Products

Related Directories

  • Micro Powders Inc.

    Micro Powders' additives solve problems and achieve unique coating surface effects, including: slip, rub, abrasion, scratch resistance; gloss reduction, burnish resistance; water repellency; texture, tactile and soft touch effects. We are leaders in creating innovative particle technologies, including natural/biodegradable grades and nanocomposite waxes to replace PTFE.
  • Micro Powders Inc.

    Micro Powders' additives solve problems and achieve unique coating surface effects including: slip, rub, abrasion, scratch resistance; gloss reduction, burnish resistance; water repellency; texture, tactile, and soft touch effects. We are leaders in creating innovative particle technologies, including natural/biodegradable grades and nanocomposite wax PTFE alternatives.
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • eNewsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2025. All Rights Reserved BNP Media.

Design, CMS, Hosting & Web Development :: ePublishing

Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to eNewsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to eNewsletters
  • SIGN UP!