Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Join Today
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • PCI News Now
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • JOIN!
Industry News

Antifouling Coating Could Help Clinicians See Clearly During Endoscope Procedures

November 6, 2016

BOSTON – With the help of camera-guided endoscopes, clinicians get a look inside the body’s cavities to diagnose and treat many different conditions. In the United States alone, up to 20 million endoscopies are performed on patients every year. But even for the most seasoned endoscope users, the instruments can prove very challenging to use effectively; this is due to the fact that blood and other bodily fluids quite commonly obscure the camera lens in the midst of critical procedures.

This problem inspired a team led by Wyss Core Faculty member Joanna Aizenberg to engineer a transparent surface coating for an endoscope lens that could effortlessly keep blood and other fluids at bay. The idea took roots in conversations Aizenberg had with clinician collaborators, who were quick to lament the propensity for endoscopes to become clouded mid-procedure.

Turning to the portfolio of SLIPS (Slippery Liquid-Infused Porous Surfaces) technologies already invented by Aizenberg, they set out to design a specialized SLIPS coating that could prevent bodily fluids from blocking the optical field of view of camera-guided endoscopes. The demonstrated results of their work are published in the Proceedings of the National Academy of Sciences (PNAS) journal.

“Endoscopes are used by many physicians around the world for a variety of procedures, and ironically, the moment when bleeding occurs and the optical field is blocked is also precisely when physicians most need to see what’s happening,” said Aizenberg, who is also the Amy Smith Berylson Prof. of Material Sciences at the Harvard John A. Paulson School of Engineering & Applied Sciences (SEAS), Professor of Chemistry and Chemical Biology, as well as Co-Director of the Kavli Institute for Bionano Science and Technology.

Aizenberg’s SLIPS technology creates non-wetting and robust self–cleaning surfaces that can resist almost any fouling challenge a surface may face. But to develop the technology for endoscopic use, the team needed to adapt SLIPS specifically to weather the harsh environment of a living body’s cavities.

“In addition to being entirely transparent and able to coat the curvature of the glass camera lens on the endoscope, the coating also needs to withstand constant contact and abrasion with soft tissues and corrosive bodily fluids,” said Steffi Sunny, a co-first author on the study and a graduate researcher at the Wyss currently pursuing her Ph.D. in bioengineering at SEAS.

To achieve this, the team deposited silica nanoparticles layer by layer onto an endoscope’s glass camera lens. These silica layers create a porous surface that, at the nanoscale, would be considered “rough” and filled with caverns. They then functionalized this “rough” surface and infused it with a medical-grade silicone oil, filling in the porous cavities and creating a self-replenishing liquid layer. The end result, an entirely biocompatible coating, can endure many procedural uses and standard sterilization protocols, and can be even re-applied with silicone oil intermittently to maintain its extreme repellency.

A test in which a bronchoscopy was performed on an anesthetized pig using an antifouling endoscope, the coating performed very well, easily repelling blood and mucus and dramatically reducing the complexity of the procedure by eliminating the need to repeatedly clean and wipe away fluids that obscure the optical field.

SLIPS-coated endoscopes could even expand our view into new areas of the body that we have not yet been able to access with a camera. Today’s endoscopes, which contain irrigation and suction channels to flush away build up from the lens mid-procedure, are limited in how small they can be made due to this important cleansing feature. But the super-repellent coating on the lens could potentially eliminate the need for a wash port, leading to more miniaturized endoscopes, which would allow physicians to reach, observe and treat the areas of the body that are off-limits to endoscopes of current sizes.

Looking ahead, the team also hopes that their slippery lens coating could have applications in other camera-guided instruments that operate in harsh, contaminated environments and rely on an unobstructed optical field, such as oil exploration, robotics, marine exploration, plumbing and sanitation, and drain pipe maintenance.

In addition to Aizenberg, Sunny, and Cheng, other authors on the new study include: Daniel Daniel (SEAS); Peter Lo (Interventional Pulmonary at BIDMC); Sebastian Ochoa (Interventional Pulmonary at BIDMC); Caitlin Howell (SEAS, University of Maine — Orono, Wyss Institute); Nicolas Vogel (Institute of Particle Technology and Interdisciplinary Center for Functional Particle Systems at Friedrich-Alexander University Erlangen-Nürnberg); and Adnan Majid (Interventional Pulmonary at BIDMC).

 

KEYWORDS: Medical Coatings paint and coating research and development

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • Double exposure of creative chemistry concept on laptop background, research and development concept

    Inside the AI Shift in Coatings

    Industry leaders share real-world examples of how AI is...
    Paint and Coating Pigments
    By: PCI Editorial Staff
  • Global Top 10 and PCI Logo

    2026 Global Top 10: Top Paint and Coatings Companies

    See how the world’s largest paint and coatings companies...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • The 2026 PCI 25

    2026 PCI 25: Top Paint and Coatings Companies

    See how North America's largest paint and coatings...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • Join Paint & Coatings Industry
  • Manage My Preferences
  • Customer Service

More Videos

Popular Stories

Mergers and aquisitions

Evonik Holds Off on BASF Takeover Talks

industry news

Dozens Treated After Toledo Chemical Release

Breaking News

H.B. Fuller to Close Seven Sites in Supply-Chain Overhaul

Events

December 2, 2026

Self-Activated Binder Technology: A New Path to Tin-Free Polyurethane Coatings

Through examples from protective and general industrial coating applications, attendees will learn how these innovative technologies can help maintain, and in some cases improve, coating performance while supporting safer, more sustainable formulations that align with evolving regulatory expectations

December 10, 2026

PC Academy: Waterborne Polymers and Film Formation

The trend towards waterborne polymers in the paint and coatings industry is clear; highlighting their environmentally friendly nature, regulatory considerations, growing market demand, and meeting sustainability goals.

View All Submit An Event

Products

Powder Coatings - Foundation for the Novice Formulator (ebook)

Powder Coatings - Foundation for the Novice Formulator (ebook)

See More Products
PCI news now promo ad

Related Articles

  • Nanotube Coating Could Help Shrink Mass Spectrometers

    See More
  • Web-GettyImages-873600660-1170x658.jpg

    Anti-Fatberg Invention Could Help Unclog City Sewers

    See More
  • Coatings Could Help Medical Implants Function Better

    See More
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Manufacturing Division
  • JOIN TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing