Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Join Today
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • PCI News Now
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • JOIN!
Home » Testing Equipment

Articles Tagged with ''Testing Equipment''

Ultrasonic Pulse Echo

September 9, 2015
No Comments

The Pundit PL-200PE employs state-of-the-art pulse echo technology to extend the ultrasonic application to objects where access is restricted to a single side.


Read More

Industrial Physics Acquires Ray-Ran Test Equipment

August 9, 2015
No Comments

Industrial Physics ROW Holdings Inc. has acquired UK-based Ray-Ran Test Equipment Ltd.


Read More

Q-Lab Corp. Celebrates Milestones in China

August 5, 2015
No Comments

Q-Lab Corp. announced that 2015 marks the 10th anniversary of its representative office Q-Lab China.


Read More

Bend Test

Paul N. Gardner Co. Inc.
August 1, 2015
No Comments

The TQC Cylindrical Bend Test instrument indicates the elasticity, elongation and adhesion of a paint film at bending stress.


Read More

Coating Thickness Gauges

Oxford Instruments
August 1, 2015
No Comments

Designed to reliably and non-destructively measure the thickness of a range of coatings applied to metal substrates


Read More

Replica Tape Reader

DeFelsko Corp.
August 1, 2015
No Comments

The PosiTector RTR series measures and records surface profile parameters using Testex Press-OFilm Replica Tape.


Read More

Examining Interfacial Adhesion of Biomedical Coatings

Through Scratch Testing and Microanalysis
August 1, 2015
No Comments

It is concluded that for coating applications in medical devices, microcratch and nanoscratch are useful and quantitative approaches for examining coating-to-substrate adhesions.


Read More

New Research Will Improve Powder Processing Equipment Selection

July 5, 2015
No Comments

New collaborative research carried out by Freeman Technology, Tewkesbury, UK, and Gericke AG, Zurich, Switzerland, demonstrates how to achieve faster, more reliable equipment selection in the powder processing industries.


Read More

Brookfield Donates PFT Powder Flow Tester to Kansas State University

June 14, 2015
No Comments

Brookfield Engineering has donated a PFT Powder Flow Tester to the new Kansas State University (KSU) Bulk Solids Innovation Center.


Read More

NSL Analytical Builds Staff in New England

March 8, 2015
No Comments

NSL Analytical Services Inc. has appointed Jim Martin Business Development Leader in the New England states.


Read More
Previous 1 2 … 5 6 7 8 9 10 11 12 13 14 15 16 Next
Manage My Account
  • Join Paint & Coatings Industry
  • Manage My Preferences
  • Customer Service

More Videos

Popular Stories

industry news

Dozens Treated After Toledo Chemical Release

Mergers and aquisitions

Evonik Holds Off on BASF Takeover Talks

Lincoln Memorial Pool Coating

Inspection Report Finds at Least 85 Reflecting Pool Liner Failure Locations

Events

November 11, 2026

ChinaCoat

CHINACOAT2026 returns to Guangzhou this year. Welcome to exhibit, visit and join the annual industry gathering!

November 12, 2026

Premium Leveling, Broad Compatibility: A Cost-Effective Flow and Leveling Additive

This new workhorse additive is recommended in all types of coatings. This highly compatible, 100% active siloxane product prevents defects and maintains good defoamer synergy.

View All Submit An Event

Products

Powder Coatings - Foundation for the Novice Formulator (ebook)

Powder Coatings - Foundation for the Novice Formulator (ebook)

See More Products
PCI news now promo ad

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Manufacturing Division
  • JOIN TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing