Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Join Today
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • PCI News Now
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • JOIN!
Home » Topics » Breaking News » Company News

Company News
Company News RSS Feed RSS

Rockwood Holdings to Acquire Süd-Chemie's Rheological Additives

December 1, 2005
No Comments
Rockwood Holdings, Inc., has reached an agreement to acquire the rheological additives and carbonless developers businesses of Süd-Chemie AG, Munich, Germany.
Read More

DuPont Opens Automotive Paint Laboratory in Japan

December 1, 2005
No Comments
DuPont Automotive Systems opened a $10-million laboratory in Aichi Prefecture, Japan, to facilitate technical services and approvals for automotive coatings used by Japanese auto manufacturers worldwide, and to support their home-country assembly operations.
Read More

GE Acquires Witton's Silylated Polyurethane Resins

December 1, 2005
No Comments
Advanced Materials, Silicones acquired a group of high-quality silylated polyurethane resins from Witton Chemicals Ltd., a U.K.-based company, to complement the launch of GE's third generation of SPUR+ prepolymers
Read More

Air Products Sells SVS Distribution Activities

December 1, 2005
No Comments
Air Products has sold its sodium vinyl sulfonate (SVS) North American distribution activities to Proviron Fine Chemicals NV of Ostend, Belgium.
Read More

Solutia Appoints New Butvar Resins Distributor

December 1, 2005
No Comments
Solutia Inc. has appointed Dowd & Guild, Inc., as its newly authorized distributor for Butvar® polyvinyl butyral resins and waterborne dispersions in California, Nevada and Arizona.
Read More

Akzo Nobel Works With North American ITEC Dealerships

November 1, 2005
No Comments
Akzo Nobel Car Refinishes is currently working with International Truck and Engine Company (ITEC) to enable it to discover hidden opportunities within its North American operations.
Read More

Beacon Industrial Group Joins HunterLab Sales Team

November 1, 2005
No Comments
Hunter Associates Laboratory, Inc., has announced that Beacon Industrial Group has joined its sales team.
Read More

Michelman Unveils New Brand Identity

November 1, 2005
No Comments
Michelman, a leading manufacturer of water-based coatings for paperboard and performance-enhancing additives for industrial applications, is unveiling a new brand identity, corporate tagline and marketing campaign designed to raise the company's profile and communicate its value proposition to customers.
Read More

WACKER Commits to South America With New Technical Center

November 1, 2005
No Comments
WACKER has opened a new technical center, located in Jandira, Brazil, which is being situated on the premises of the existing sales office and production facility.
Read More

Arkema Awarded for Polymers Used in Antifoulant Paints

November 1, 2005
No Comments
Arkema Inc. announced that its Additives Business received an R&D 100 Award for two products that control the self-polishing behavior of marine antifoulant paints, preventing organism growth on the hulls of seagoing ships.
Read More
Previous 1 2 … 733 734 735 736 737 738 739 740 741 … 867 868 Next
Manage My Account
  • Join Paint & Coatings Industry
  • Manage My Preferences
  • Customer Service

More Videos

Popular Stories

industry news

Dozens Treated After Toledo Chemical Release

Mergers and aquisitions

Evonik Holds Off on BASF Takeover Talks

Lincoln Memorial Pool Coating

Inspection Report Finds at Least 85 Reflecting Pool Liner Failure Locations

Events

November 11, 2026

ChinaCoat

CHINACOAT2026 returns to Guangzhou this year. Welcome to exhibit, visit and join the annual industry gathering!

November 12, 2026

Premium Leveling, Broad Compatibility: A Cost-Effective Flow and Leveling Additive

This new workhorse additive is recommended in all types of coatings. This highly compatible, 100% active siloxane product prevents defects and maintains good defoamer synergy.

View All Submit An Event

Products

Powder Coatings - Foundation for the Novice Formulator (ebook)

Powder Coatings - Foundation for the Novice Formulator (ebook)

See More Products
PCI news now promo ad

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Manufacturing Division
  • JOIN TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing