Dunn-Edwards has made it much easier for architects, designers and contractors involved in green-building projects to navigate the complicated requirements for paint and coatings in order to be compliant with key green programs.
Micromeritics Analytical Services and MVA Scientific Consultants have joined forces to offer their clients additional analytical choices while improving customer service.
In May 2005, Degussa Corp. began operating a new plant for the manufacture of AEROSILĀ® fumed silica dispersions, which are known under the AERODISPĀ® trademark.
HALOX, a worldwide supplier of non-toxic corrosion and tannin stain inhibitors to the paint and coatings industry, is expanding its existing distribution agreement with the Dempsey Corp. to include all of Canada.
The Dow Chemical Company, Midland, Mich., has completed the acquisition of Pacific Epoxy Co., Ltd., a manufacturer of converted epoxy resins in Korea, from Saehan Industries, Inc.
The U.S. Environmental Protection Agency has awarded its Presidential Green Chemistry Challenge Award to BASF's Automotive Refinish Coatings business for the company's eco-efficient UV-curable primer.
Selected assets of the DSM SomosĀ® selective laser sintering business conducted by DSM Desotech Inc. and its DSM Somos subsidiary based in New Castle, Del., have been sold to The Valspar Corporation, Minneapolis.
Rohm and Haas Company celebrated the official groundbreaking of its new China Research and Development Center in Shanghai, with nearly 200 distinguished guests in attendance.
Philadelphia Mixing Solutions, Ltd. (PMSL), a leading industrial mechanical- and process-mixing optimization specialist, has announced availability of the world's largest mixing and process test lab for customers and contract facilities.