Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Join Today
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • PCI News Now
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • JOIN!
Home » Topics » New Products

New Products
New Products RSS Feed RSS

Mixer

August 1, 2010
No Comments
Designed for multiple mixing requirements, the Ross VersaMix (triple-shaft mixer) is now available with a solid/liquid injection manifold or S.L.I.M.™ system, which injects materials directly into the rotor/stator agitator.
Read More

Mini Tank

August 1, 2010
No Comments
The redesigned 110 cc mini tank allows customers to process batches as small as 20-30 cc of material.
Read More

Analyzer

August 1, 2010
No Comments
The Petrotest CLA 5 Cleveland open-cup flash-point and fire-point analyzer automatically tests both liquid and highly viscous liquid and solid samples.
Read More

Dust and Fume Collector

July 1, 2010
No Comments
The Zephyr® III pulse-cleaned dust and fume collector combines portable three-stage filtration with versatility and ease of use.
Read More

Ribbon Blender

July 1, 2010
No Comments
The model 42NSD ribbon blender features a discharge screw positioned across the entire bottom of the trough with very close tolerances between the screw and the trough.
Read More

Additive

July 1, 2010
No Comments
Michem Lube 190 is an anionic polyethylene wax emulsion additive that significantly improves the mar and scratch resistance, and water repellency, of architectural and decorative paints, stains, sealants and numerous other interior and exterior coatings.
Read More

Pigments

July 1, 2010
No Comments
The ED Pigments range has been expanded to simplify the pigment dispersion process for all paint systems by removing the need for a milling step.
Read More

Mixer Cartridges

July 1, 2010
No Comments
New B Series 50 mL cartridges provide an innovative interface for the mixer and a pre-assembled built-in piston retention feature for easier use.
Read More

Grinding Mill

July 1, 2010
No Comments
This ultrafine grinding mill is capable of processing materials at throughputs ranging from just a few kilograms to over 1000 kilograms per hour.
Read More

Adhesion Tape

July 1, 2010
No Comments
Elcometer 99 adhesion tape has been developed as a replacement for Permacel tape.
Read More
Previous 1 2 … 182 183 184 185 186 187 188 189 190 … 310 311 Next
Manage My Account
  • Join Paint & Coatings Industry
  • Manage My Preferences
  • Customer Service

More Videos

Popular Stories

Breaking News

H.B. Fuller to Close Seven Sites in Supply-Chain Overhaul

AkzoNobel Axalta

EU Clears $25B Akzo-Axalta Merger with One Big Condition

A robotic hand points at a glowing compliance concept surrounded by various icons representing laws, regulations, governance, and standards in a digital workspace

Powder Coater’s $1.64M OSHA Case Follows Earlier Citations

Events

December 2, 2026

Self-Activated Binder Technology: A New Path to Tin-Free Polyurethane Coatings

Through examples from protective and general industrial coating applications, attendees will learn how these innovative technologies can help maintain, and in some cases improve, coating performance while supporting safer, more sustainable formulations that align with evolving regulatory expectations

December 10, 2026

PC Academy: Waterborne Polymers and Film Formation

The trend towards waterborne polymers in the paint and coatings industry is clear; highlighting their environmentally friendly nature, regulatory considerations, growing market demand, and meeting sustainability goals.

View All Submit An Event

Products

Powder Coatings - Foundation for the Novice Formulator (ebook)

Powder Coatings - Foundation for the Novice Formulator (ebook)

See More Products
PCI news now promo ad

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Manufacturing Division
  • JOIN TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing