Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • China Issue Archive
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • SIGN UP!
Home » Topics » New Products

New Products
New Products RSS Feed RSS

New Multi-functional Digital Thermo Hygrometer from Paul N. Gardner

New Multi-Functional Digital Thermo Hygrometer from Paul N. Gardner

January 24, 2023
No Comments

Paul N. Gardner USA's New Indoor/Outdoor Digital Thermo-Hygrometer is a multifunctional humidity thermometer that can display temperature, humidity, and time simultaneously.


Read More
image of hot plate and laboratory equipment

New Programmable Stirring Hot Plate from Torrey Pines

January 20, 2023
No Comments

Torrey Pines Scientific, Inc. offers its new EchoTherm™ Programmable Digital Stirring Hot Plate for use in chemical, pharmaceutical, environmental, biochemical, and other laboratories.


Read More
Image of Wet Film Thickness Gauges

New Custom Wet Film Thickness Gauge from Gardco

January 20, 2023
No Comments

The gauges are conveniently sized to fit in a wallet – like a calling card (2-1/4 " x 3-1/4" x .034") – and are made of solid aluminum stock.


Read More
New Plasma Nozzles from Plasmatreat

Plasma Nozzles from Plasmatreat

January 18, 2023
No Comments

Plasma technology can be used to modify the surface properties of a wide variety of materials in order to optimally prepare materials and material combinations for subsequent processes. This makes bonding, painting, printing, or gasketing easier or even possible in the first place.


Read More
New Adhesive for High-Performance ADAS Sensors from Henkel

New Adhesive for High-Performance ADAS Sensors from Henkel

January 13, 2023
No Comments

Henkel has developed a new adhesive – Loctite 3296 – a dual-cure adhesive for lens bonding in ADAS sensors. The new product provides a very high-cure depth after only a few seconds of exposure to UV-light, and is designed to bond particularly well to aluminum and FR4.


Read More
WoodCoatings-123946969.jpg

New Primer for Wood Substrates from AmCoat

December 29, 2022
No Comments

Formulated with a blend of resins and ceramic spheres, the elastomeric-acrylic coating was specifically developed as a primer coat for wood siding. SPC also offers protection on many other substrates including concrete, brick, masonry and stucco. In addition, SPC offers energy-saving insulation properties and soundproofing.


Read More
Fire Protection for Steel Structures from CIN

Fire Protection for Steel Structures from CIN

December 26, 2022
One Comment

CIN presents a certified system for corrosive environments for categories C3 with very high durability, C4 with high durability, and C5 with medium durability. The tests were approved by an accredited external laboratory that certified that the performance of the C-THERM® S100 intumescent remains unchanged even after aging tests under conditions specified in ISO 12944-6:2017.


Read More
New Dual Shaft Mixer from ROSS

New Dual Shaft Mixer from ROSS

December 22, 2022
No Comments

ROSS offers a line of dual shaft mixers that can be used to batch dispersions, suspensions, and emulsions with viscosities up to several hundred-thousand centipoise – like the custom-built ROSS FDA-3500. This multi-agitator system is equipped with independently controlled drives, and is efficient at producing good turnover and imparting shear to a viscous batch.


Read More
12.21New-Benchtop-Lift Mixers-from-INDCO.jpg

New Benchtop Lift Mixers from INDCO

December 21, 2022
No Comments

The five-gallon mixer is ideal for use in product development labs or production environments, across a wide range of applications, including viscous printing inks or dispersions, drywall mud, and lower viscosity materials like paint.


Read More
New Weatherability Tester from Applied Optix

New Weatherability Tester from Applied Optix

December 19, 2022
No Comments

The tester can be used in automotive materials, building and construction, paint and coatings, plastics and polymers, and composites applications. As a screening tool, the tester can generate five years of UV exposure in 10 days, which would both save money on R&D, and cut time to market for new products.


Read More
Previous 1 2 … 50 51 52 53 54 55 56 57 58 … 306 307 Next
Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

Popular Stories

Breaking News

Yenkin-Majestic Pleads Guilty in Fatal Resin Plant Explosion Case

Evonik Logo

Evonik to Close Two German Sites

Mergers-and-Company-Strategies.jpg

BASF Confirms Exploratory Talks on Potential Evonik Takeover

Webinar custom content box

Events

October 8, 2026

AI-Powered Reformulation: Finding PFAS-Free, Lower-VOC Formulations Faster

In this webinar, we will use case studies from industry to illustrate how AI can be used to identify PFAS-free formulations and select surfactant blends for water-based products.

January 1, 2030

Webinar Sponsorship Information

For webinar sponsorship information, visit www.bnpevents.com/webinars or email webinars@bnpmedia.com.

View All Submit An Event

Products

Advanced Coating Materials

Advanced Coating Materials

See More Products
Webinar custom content box

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing