PERFORMALOC™ advanced productivity coatings are a new category of cross-linked coatings featuring a proprietary combination of low-VOC resins that cure fast and hard, thus eliminating the need for baking or force-drying of metal parts.
These coatings are designed for original equipment manufacturers (OEMs) that coat metal parts such as those used in agricultural equipment, locomotives and rail cars, outdoor furniture, light poles, exterior electrical cabinets and hardware, trailers, and shipping containers.