At Stand 7A-603, Perstorp is launching Curalite™, its range of boosters for cationic UV-curing formulations that can increase reaction speeds up to 15 times. Cationic UV-curing technology is the perfect choice for printing on challenging surfaces such as plastic substrates or containers, where other technologies could fail.