Ford Puts Engine Plant on a Fresh Footing with Flowcrete Products
ROMEO, MI — The Ford Motor Co. selected high-performance flooring solutions from Flowcrete Americas when it undertook a comprehensive renovation of its large-scale Romeo Engine Plant in Romeo, Michigan.
The facility has been a critical part of Ford’s industrial muscle since the early 70s, and it has recently embarked on a $150 million program of upgrades to enhance its capacity and prepare the plant for the future.