Beckqua®Color is a next-generation waterborne basecoat for bumpers, mirror caps and door handles. By using an exclusive resins combination as well as matching the requirements on cost, solids, and leveling, Beckers’ new coating offers benefits that include a very high solid content, enhanced appearance through a smoother film surface, and a very good hiding power.
In the case of a white coating, this substantial improvement in solid content means that a coating line with a normal annual paint consumption of 60 tons can reduce this amount to 45 tons. This translates into 750 fewer pails of paint that need to be transported and kept in a climate-controlled warehouse.